公开(公告)号:US20190319305A1
公开(公告)日:2019-10-17
申请号:US16461235
申请日:2017-08-08
Applicant: IDEMITSU KOSAN CO., LTD.
Inventor: Futoshi UTSUNO , Akiko NAKATA , Kota TERAI , Masaru NAKAGAWA
IPC: H01M10/0562 , H01M10/0525
Abstract: Provided is a sulfide solid electrolyte containing lithium, phosphorus, sulfur and chlorine, in which a molar ratio of the chlorine to the phosphorus, c (Cl/P), is greater than 1.0 and 1.9 or less, the sulfide solid electrolyte includes an argyrodite-type crystal structure, and a lattice constant of the argyrodite-type crystal structure is 9.820 Å or less.
-
公开(公告)号:US20220367907A1
公开(公告)日:2022-11-17
申请号:US17814374
申请日:2022-07-22
Applicant: IDEMITSU KOSAN CO.,LTD.
Inventor: Futoshi UTSUNO , Akiko NAKATA , Kota TERAI , Masaru NAKAGAWA
IPC: H01M10/0562 , H01M10/0525
Abstract: Provided is a sulfide solid electrolyte containing lithium, phosphorus, sulfur and chlorine, in which a molar ratio of the chlorine to the phosphorus, c (Cl/P), is greater than 1.0 and 1.9 or less, the sulfide solid electrolyte includes an argyrodite-type crystal structure, and a lattice constant of the argyrodite-type crystal structure is 9.820 Å or less.
-
公开(公告)号:US20210075056A1
公开(公告)日:2021-03-11
申请号:US16619682
申请日:2018-05-24
Applicant: Idemitsu Kosan Co.,Ltd.
Inventor: Akiko NAKATA , Junpei MARUYAMA , Miki MONOI , Ryohei HASHIMOTO
IPC: H01M10/0562 , H01M10/0525 , C01B25/14
Abstract: A method for producing a sulfide solid electrolyte comprising an argyrodite-type crystal structure, wherein phosphorus sulfide having a phosphorus content of 28.3 mass % or less and containing free sulfur is used as the raw material.
-
公开(公告)号:US20180016185A1
公开(公告)日:2018-01-18
申请号:US15522580
申请日:2015-10-30
Applicant: IDEMITSU KOSAN CO., LTD.
Inventor: Akiko NAKATA , Junpei MARUYAMA
IPC: C03C3/32 , C03C4/14 , C03C1/02 , H01M10/0525 , H01M10/0562
CPC classification number: C03C3/32 , C03C1/02 , C03C3/321 , C03C4/14 , H01B1/06 , H01B1/10 , H01B13/00 , H01M4/587 , H01M4/62 , H01M10/052 , H01M10/0525 , H01M10/0562 , H01M2300/008
Abstract: A method for producing sulfide glass wherein phosphorus sulfide satisfying the following formula (1) is used as a raw material: 100×A/B≧37 (1) wherein in the formula, A is peak areas of peaks that appear at peak positions in a range of 57.2 ppm or more and 58.3 ppm or less, and 63.0 ppm or more and 64.5 ppm or less in 31PNMR spectroscopy, and B is the total of peak areas of all peaks measured in 31PNMR spectroscopy.
-
-
-