公开(公告)号:US20210404099A1
公开(公告)日:2021-12-30
申请号:US17290926
申请日:2019-11-06
Applicant: IDEMITSU KOSAN CO.,LTD.
Inventor: Mari YABE , Takumi SUGIUCHI , Masaki OKANO , Yutaka MINAMI
Abstract: The present invention relates to a nonwoven fabric including a conjugated fiber containing 40% by mass or more and 80% by mass or less of a propylene homopolymer (A) having a melting point (Tm-D) measured by a differential scanning calorimeter (DSC) of higher than 120° C., 4% by mass or more and 40% by mass or less of a polypropylene-based resin (B) having a melting point (Tm-D) measured by a differential scanning calorimeter (DSC) of 120° C. or lower, and 10% by mass or more and 55% by mass or less of a polyethylene-based resin (C), wherein the nonwoven fabric has a texture uniformity of 2.1 or more and 3.0 or less and a bulkiness of 450 μm or more.
-
2.
公开(公告)号:US20180215878A1
公开(公告)日:2018-08-02
申请号:US15762996
申请日:2016-09-23
Applicant: IDEMITSU KOSAN CO., LTD.
Inventor: Masaki OKANO , Yoshihito KOYAMA , Shinobu YAMAO
CPC classification number: C08H6/00 , C08G8/20 , C08H8/00 , C08L97/005 , C08L101/00
Abstract: Provided is a method of producing a purified lignin, including: treating a plant biomass in a first solvent mixture formed of water and a first organic solvent under specific conditions; subjecting a solid fraction insoluble in a first solution mixture and the first solution mixture to solid-liquid separation after the treatment; mixing the first solution mixture from which the insoluble solid fraction has been separated, and a second organic solvent excluding the first organic solvent and having a dipole moment of 0.25 d or less to provide a second solution mixture; and subjecting a solid fraction insoluble in the second solution mixture to solid-liquid separation to extract the purified lignin in a liquid phase of the second solution mixture.
-
公开(公告)号:US20230303813A1
公开(公告)日:2023-09-28
申请号:US18041231
申请日:2021-08-25
Applicant: IDEMITSU KOSAN CO.,LTD.
Inventor: Nozomu FUJII , Masaki OKANO , Asami KOGA
IPC: C08L23/12 , C09J123/12
CPC classification number: C08L23/12 , C09J123/12 , C08L2205/025
Abstract: A propylene resin composition containing a propylene homopolymer that satisfies conditions (1) to (3) described below, and having a semicrystallization time (t1/2) of 60 seconds or more:
(1) having a melting point (Tm-D) of 120° C. or lower;
(2) having a molecular weight distribution (Mw/Mn) less than 3.0;
(3) having a melt viscosity at 190° C. of 30,000 mPa·s or less.-
4.
公开(公告)号:US20190211207A1
公开(公告)日:2019-07-11
申请号:US16330842
申请日:2017-09-04
Applicant: IDEMITSU KOSAN CO., LTD.
Inventor: Yoshihito KOYAMA , Shinobu YAMAO , Masaki OKANO
CPC classification number: C08L97/005 , C08H6/00 , C08J5/00 , C08L61/06 , C08L97/00 , C08L101/00
Abstract: The method for producing a resin composition of the present invention includes a step of obtaining a lignin-containing solution that contains a solubilized lignin prepared through a treatment of separating lignin in a lignin-containing solution and a solvent, and a step of adding a resin to the lignin-containing solution to thereby obtain a lignin/resin-containing solution. Also, the method for producing a resin composition of the present invention includes a step of mixing the lignin/resin-containing solution with at least one solvent selected from water and a hydrocarbon having a dipole moment of 0.25 d or less. The lignin-containing resin molded article of the present invention uses the resin composition obtained according to the production method of the present invention.
-
-
-