摘要:
The present invention provides a negative active material for a secondary battery with an improved expansion rate, which is formed by a formula below, and in which an expansion rate of the negative active material after 50 cycles is 70 to 150%, and an amorphization degree on a matrix within an alloy has a range of 25% or more, and Si has a range of 60 to 70%, Ti has a range of 9 to 14%, Fe has a range of 9 to 14%, and Al has a range larger than 1% and less than 20%. Formula: SixTiyFezAlu (x, y, z, and u are at %, x: 1−(y+z+u)).
摘要:
The present invention provides a negative active material for a secondary battery with an improved expansion rate, which is formed by a formula below, and in which an expansion rate of the negative active material after 50 cycles is 70 to 150%, and an amorphization degree on a matrix within an alloy has a range of 25% or more, and Si has a range of 60 to 70%, Ti has a range of 9 to 14%, Fe has a range of 9 to 14%, and Al has a range larger than 1% and less than 20%. Formula: SixTiyFezAlu (x, y, z, and u are at %, x: 1−(y+z+u))
摘要翻译:本发明提供一种具有改善的膨胀率的二次电池用负极活性物质,其由下式形成,其中负极活性物质在50个循环后的膨胀率为70〜150%,非晶化度 在合金中的基体上具有25%以上的范围,Si的范围为60〜70%,Ti为9〜14%的范围,Fe为9〜14%的范围,Al为 范围大于1%且小于20%。 公式:SixTiyFezAlu(x,y,z和u在%,x:1-(y + z + u))