Method For Producing Shaped Polyurethane Foam Wound Dressings
    1.
    发明申请
    Method For Producing Shaped Polyurethane Foam Wound Dressings 审中-公开
    生产聚氨酯泡沫伤口敷料的方法

    公开(公告)号:US20110201715A1

    公开(公告)日:2011-08-18

    申请号:US13060681

    申请日:2009-08-17

    IPC分类号: C08G18/10

    摘要: The invention relates to a process for producing shaped articles, where a foam layer which includes a polyurethane foam obtained by foaming a composition including an aqueous, anionically hydrophilicized polyurethane dispersion (I), and drying, is thermoformed where the thermoforming takes place at a temperature of from ≧100° C. to ≦200° C. and under a pressure of from ≧50 bar to ≦150 bar, and where additionally during the thermoforming the foam is compressed to ≧25% to ≦100% of its original volume. The foam can be stabilized using ethylene oxide/propylene oxide block copolymers. The invention further relates to shape articles obtainable in this way, and to the use thereof, preferably as wound dressings.

    摘要翻译: 本发明涉及一种生产成型制品的方法,其中包括通过使包含水性,阴离子亲水化的聚氨酯分散体(I)的组合物发泡得到的聚氨酯泡沫和干燥的泡沫层被热成型,其中热成型在温度 从≧100℃至< nlE; 200℃,压力≥50巴至< NlE; 150巴,并且另外在热成型期间,将泡沫压缩至≥25%至≤100;其100% 原卷。 泡沫可以使用环氧乙烷/环氧丙烷嵌段共聚物来稳定。 本发明还涉及以这种方式获得的形状制品及其用途,优选作为伤口敷料。

    METHOD FOR PRODUCING SHAPED POLYURETHANE FOAM WOUND DRESSINGS
    2.
    发明申请
    METHOD FOR PRODUCING SHAPED POLYURETHANE FOAM WOUND DRESSINGS 审中-公开
    用于生产形状的聚氨酯泡沫围巾的方法

    公开(公告)号:US20110160633A1

    公开(公告)日:2011-06-30

    申请号:US13060527

    申请日:2009-08-17

    IPC分类号: A61L15/22 B29C43/00 B32B7/02

    摘要: The present invention relates to a process for producing shaped articles comprising, acting on a foam layer in a first region with a pressure of from 0 to 150 bar at a temperature of from 0° C. to less than or equal to 200° C., whereby the foam layer is compressed in the first region to greater than 12.5% to 100% of its original volume; acting on the foam layer in a second region with a pressure of from 50 to 150 bar at a temperature of from 100° C. to 200° C., whereby the foam layer is compressed in the second region from greater than 0% to 12.5% of its original volume; and wherein the foam layer comprises in the first region and the second region a polyurethane foam which is obtained by foaming and drying a composition comprising an aqueous, anionically hydrophilicized polyurethane dispersion.

    摘要翻译: 本发明涉及一种生产成形制品的方法,其包括在0℃至小于或等于200℃的温度下,在0至150巴的压力下作用在第一区域的泡沫层上。 由此泡沫层在第一区域被压缩至其原始体积的12.5%至100%; 在100至200℃的温度下,在50至150巴的压力的第二区域中作用在泡沫层上,由此泡沫层在第二区域被压缩从大于0%至12.5 原始数量的百分比; 并且其中所述泡沫层在所述第一区域和所述第二区域中包含通过发泡和干燥包含水性阴离子亲水化聚氨酯分散体的组合物获得的聚氨酯泡沫。