Method of modifying molecular sieves by means of solid state ion exchange
    1.
    发明授权
    Method of modifying molecular sieves by means of solid state ion exchange 失效
    通过固态离子交换法改性分子筛的方法

    公开(公告)号:US5434114A

    公开(公告)日:1995-07-18

    申请号:US197481

    申请日:1994-02-16

    CPC分类号: B01J37/30 B01J29/74

    摘要: Molecular sieves are modified by an ion exchange process where metal cations are introduced into the molecular sieves by means of solid state ion exchange. The solid state ion exchange can be carried out as follows: a weighed amount of calcined and activated zeolite is intimately mixed with a precalculated amount of PtCl.sub.2, PdCl.sub.2, RhCl.sub.3, CuCl.sub.2, V.sub.2 O.sub.5 or another compound of the noble metals (e.g., corresponding halides or oxides), the solids mixture is then heated in a current of inert gas (e.g., a current of helium gas or of nitrogen) to temperatures of 400.degree. to 600.degree. C., then cooled down to room temperature and subsequently reduced in a current of hydrogen for 10 to 14 hours at 280.degree. to 350.degree. C. in order to produce small metal clusters from the cationically introduced metal.

    摘要翻译: 分子筛通过离子交换方法进行改性,其中通过固态离子交换将金属阳离子引入分子筛中。 固态离子交换可以如下进行:称重量的煅烧和活化的沸石与预先计算量的PtCl 2,PdCl 2,RhCl 3,CuCl 2,V 2 O 5或贵金属的另一种化合物(例如,相应的卤化物或 氧化物),然后将固体混合物在惰性气体(例如,氦气或氮气流)中加热至400至600℃的温度,然后冷却至室温,随后减少电流 的氢气在280〜350℃下进行10〜14小时,以从阳离子导入的金属产生小的金属簇。

    Modified molecular sieves by means of solid ion exchange
    2.
    发明授权
    Modified molecular sieves by means of solid ion exchange 失效
    通过固体离子交换改性分子筛

    公开(公告)号:US5529964A

    公开(公告)日:1996-06-25

    申请号:US388832

    申请日:1995-02-15

    CPC分类号: B01J37/30 B01J29/74

    摘要: Molecular sieves are modified by an ion exchange process where metal cations are introduced into the molecular sieves by means of solid state ion exchange. The solid state ion exchange can be carried out as follows: a weighed amount of calcined and activated zeolite is intimately mixed with a precalculated amount of PtCl.sub.2, PdCl.sub.2, RhCl.sub.3, CuCl.sub.2, V.sub.2 O.sub.5 or another compound of the noble metals (e.g., corresponding halides or oxides), the solids mixture is then heated in a current of inert gas (e.g., a current of helium gas or of nitrogen) to temperatures of 400.degree. to 600.degree. C., then cooled down to room temperature and subsequently reduced in a current of hydrogen for 10 to 14 hours at 280.degree. to 350.degree. C. in order to produce small metal clusters from the cationically introduced metal.

    摘要翻译: 分子筛通过离子交换方法进行改性,其中通过固态离子交换将金属阳离子引入分子筛中。 固态离子交换可以如下进行:称重量的煅烧和活化的沸石与预先计算量的PtCl 2,PdCl 2,RhCl 3,CuCl 2,V 2 O 5或贵金属的另一种化合物(例如,相应的卤化物或 氧化物),然后将固体混合物在惰性气体(例如,氦气或氮气流)中加热至400至600℃的温度,然后冷却至室温,随后减少电流 的氢气在280〜350℃下进行10〜14小时,以从阳离子导入的金属产生小的金属簇。

    Method of modifying molecular sieves by means of solid state ion
exchange, and a method for hydrogenating olefinic compounds
    3.
    发明授权
    Method of modifying molecular sieves by means of solid state ion exchange, and a method for hydrogenating olefinic compounds 失效
    通过固态离子交换法改性分子筛的方法,以及烯烃化合物的氢化方法

    公开(公告)号:US5545784A

    公开(公告)日:1996-08-13

    申请号:US419896

    申请日:1995-04-11

    CPC分类号: B01J37/30 B01J29/74

    摘要: Molecular sieves are modified by an ion exchange process where metal cations are introduced into the molecular sieves by means of solid state ion exchange. The solid state ion exchange can be carried out as follows: a weighed amount of calcined and activated zeolite is intimately mixed with a precalculated amount of PtCl.sub.2, PdCl.sub.2, RhCl.sub.3, CuCl.sub.2, V.sub.2 O.sub.5 or another compound of the noble metals (e.g., corresponding halides or oxides), the solids mixture is then heated in a current of inert gas (e.g., a current of helium gas or of nitrogen) to temperatures of 400.degree. to 600.degree. C., then cooled down to room temperature and subsequently reduced in a current of hydrogen for 10 to 14 hours at 280.degree. to 350.degree. C. in order to produce small metal clusters from the cationically introduced metal.

    摘要翻译: 分子筛通过离子交换方法进行改性,其中通过固态离子交换将金属阳离子引入分子筛中。 固态离子交换可以如下进行:称重量的煅烧和活化的沸石与预先计算量的PtCl 2,PdCl 2,RhCl 3,CuCl 2,V 2 O 5或贵金属的另一种化合物(例如,相应的卤化物或 氧化物),然后将固体混合物在惰性气体(例如,氦气或氮气流)中加热至400至600℃的温度,然后冷却至室温,随后减少电流 的氢气在280〜350℃下进行10〜14小时,以从阳离子导入的金属产生小的金属簇。