摘要: A catheter balloon and method involves extruded tubing with multiple layers of different durometer values, selected such that the blow up ratio (BUR) at the balloon's inner surface is increased. In one method a two stage blow mold process uses a small radius initial stage where radial growth is limited, followed by a second stage to a final dimension. A single stage blow mold process is also disclosed where the materials and processing are selected to approach the elongation to failure limit of the material. The single stage approach is preferably followed by a modified post-expansion heat set treatment to promote greater axial strength, leading to a preferred failure mode in the axial rather than radial direction.
摘要翻译: 导管球囊和方法包括具有多层不同硬度值的挤出管,其选择为使得球囊内表面处的吹胀比(BUR)增加。 在一种方法中,两级吹塑工艺使用径向生长受限的小半径初始阶段,随后是第二阶段到最终尺寸。 还公开了单级吹塑工艺,其中选择材料和加工以接近材料的伸长率到破坏极限。 单阶段方法优选地是经过改进的后膨胀热定形处理以促进更大的轴向强度,导致在轴向而不是径向方向上优选的破坏模式。
-
公开(公告)号:US08703260B2
公开(公告)日:2014-04-22
申请号:US12881733
申请日:2010-09-14
IPC分类号: B32B1/00 , B32B1/08 , A61M29/00 , A61M31/00 , B29C71/00 , B29C49/00 , B29C47/00 , B29C45/14 , B29C35/02
CPC分类号: A61M25/1029 , A61F2/958 , A61L29/04 , A61L29/06 , A61L29/14 , A61L2420/08 , A61M25/0009 , A61M25/10 , A61M25/1027 , A61M25/104 , A61M2025/1075 , B29C49/04 , B29C49/185 , B29C49/22 , B29L2031/7543 , Y10T428/1334 , Y10T428/1352 , Y10T428/1386 , Y10T428/1393
摘要: A catheter balloon and method involves extruded tubing with multiple layers of different durometer values, selected such that the blow up ratio (BUR) at the balloon's inner surface is increased. In one method a two stage blow mold process uses a small radius initial stage where radial growth is limited, followed by a second stage to a final dimension. A single stage blow mold process is also disclosed where the materials and processing are selected to approach the elongation to failure limit of the material. The single stage approach is preferably followed by a modified post-expansion heat set treatment to promote greater axial strength, leading to a preferred failure mode in the axial rather than radial direction.
摘要翻译: 导管球囊和方法包括具有多层不同硬度值的挤出管,其选择为使得球囊内表面处的吹胀比(BUR)增加。 在一种方法中,两级吹塑工艺使用径向生长受限的小半径初始阶段,随后是第二阶段到最终尺寸。 还公开了单级吹塑工艺,其中选择材料和加工以接近材料的伸长率到破坏极限。 单阶段方法优选地是经过改进的后膨胀热定形处理以促进更大的轴向强度,导致在轴向而不是径向方向上优选的破坏模式。
-
公开(公告)号:US08140686B2
公开(公告)日:2012-03-20
申请号:US12478058
申请日:2009-06-04
CPC分类号: H04L63/102
摘要: A client device interrogates an access point on a network to request an initial connection to the network. Without using a browser, the client device determines if the connection failed due to a lack of authorization for the client device to connect to the network.
摘要翻译: 客户机设备询问网络上的接入点以请求与网络的初始连接。 不使用浏览器,由于客户端设备没有授权连接到网络,客户端设备确定连接是否失败。
-
-