摘要: A thermoelectric material and a method of making a thermoelectric material are provided. In certain embodiments, the thermoelectric material comprises at least 10 volume percent porosity. In some embodiments, the thermoelectric material has a zT greater than about 1.2 at a temperature of about 375 K. In some embodiments, the thermoelectric material comprises a topological thermoelectric material. In some embodiments, the thermoelectric material comprises a general composition of (Bi1-xSbx)u(Te1-ySey)w, wherein 0≦x≦1, 0≦y≦1, 1.8≦u≦2.2, 2.8≦w≦3.2. In further embodiments, the thermoelectric material includes a compound having at least one group IV element and at least one group VI element. In certain embodiments, the method includes providing a powder comprising a thermoelectric composition, pressing the powder, and sintering the powder to form the thermoelectric material.
摘要翻译: 提供热电材料和制造热电材料的方法。 在某些实施例中,热电材料包括至少10体积%的孔隙率。 在一些实施例中,热电材料在约375K的温度下具有大于约1.2的zT。在一些实施例中,热电材料包括拓扑热电材料。 在一些实施方案中,热电材料包括(Bi1-xSbx)u(Te1-ySey)w的一般组成,其中0和nlE; x和nlE; 1,0和nlE; y和nlE; 1.8,1.01; n和nlE; 2.2,2.8& 3.2。 在另外的实施方案中,热电材料包括具有至少一个IV族元素和至少一个VI族元素的化合物。 在某些实施方案中,该方法包括提供包含热电组合物的粉末,压制粉末,并烧结粉末以形成热电材料。
-
公开(公告)号:US20120248386A1
公开(公告)日:2012-10-04
申请号:US13436521
申请日:2012-03-30
CPC分类号: C04B35/547 , C04B38/0074 , C04B2235/40 , C04B2235/604 , C04B2235/6581 , C04B2235/77 , H01L35/16 , H01L35/34 , C04B38/0054 , C04B38/0061
摘要: A thermoelectric material and a method of making a thermoelectric material are provided. In certain embodiments, the thermoelectric material comprises at least 10 volume percent porosity. In some embodiments, the thermoelectric material has a zT greater than about 1.2 at a temperature of about 375 K. In some embodiments, the thermoelectric material comprises a topological thermoelectric material. In some embodiments, the thermoelectric material comprises a general composition of (Bi1-xSbx)u(Te1-ySey)w, wherein 0≦x≦1, 0≦y≦1, 1.8≦u≦2.2, 2.8≦w≦3.2. In further embodiments, the thermoelectric material includes a compound having at least one group IV element and at least one group VI element. In certain embodiments, the method includes providing a powder comprising a thermoelectric composition, pressing the powder, and sintering the powder to form the thermoelectric material.
摘要翻译: 提供热电材料和制造热电材料的方法。 在某些实施例中,热电材料包括至少10体积%的孔隙率。 在一些实施例中,热电材料在约375K的温度下具有大于约1.2的zT。在一些实施例中,热电材料包括拓扑热电材料。 在一些实施方案中,热电材料包括(Bi1-xSbx)u(Te1-ySey)w的一般组成,其中0和nlE; x和nlE; 1,0和nlE; y和nlE; 1.8,1.01; n和nlE; 2.2,2.8& 3.2。 在另外的实施方案中,热电材料包括具有至少一个IV族元素和至少一个VI族元素的化合物。 在某些实施方案中,该方法包括提供包含热电组合物的粉末,压制粉末,并烧结粉末以形成热电材料。
-