Biodegradable polyester resin composition
    1.
    发明授权
    Biodegradable polyester resin composition 有权
    可生物降解聚酯树脂组合物

    公开(公告)号:US09371445B2

    公开(公告)日:2016-06-21

    申请号:US14388954

    申请日:2013-03-29

    Abstract: This invention aims at improving the tear strength of a film and a sheet molded from a resin composition containing microorganism-produced aliphatic polyester. This invention relates to a biodegradable polyester resin composition containing polybutylene adipate terephthalate (PBAT) in the proportion of 60 to 400 parts by weight and modified-glycerin in the proportion of 10 to 50 parts by weight based on 100 parts by weight of aliphatic polyester (P3HA) having a repeating unit represented by Formula (1): [—CHR—CH2—CO—O—] (wherein R is an alkyl group represented by CnH2n+1 and n is an integer of 1 or more and 15 or lower) and a film or a sheet obtained by molding the biodegradable polyester resin composition in which the maximum major axis of phases containing the aliphatic polyester (P3HA) measured by a transmission electron microscopy analysis-image analysis method (TEM method) is 18 μm or lower and the average value is 8 μm or lower.

    Abstract translation: 本发明的目的在于提高膜和由含有微生物生产的脂肪族聚酯的树脂组合物成型的片材的撕裂强度。 本发明涉及以聚对苯二甲酸丁二醇酯(PBAT)为60〜400重量份的生物降解性聚酯树脂组合物,相对于100重量份的脂肪族聚酯为10〜50重量份的改性甘油 具有由式(1)表示的重复单元的化合物(其中R是由C n H 2n + 1表示的烷基,n是1以上且15以下的整数) 以及通过透射电子显微镜分析图像分析方法(TEM法)测定的含有脂肪族聚酯(P3HA)的相的最大长轴的生物降解性聚酯树脂组合物成型为18μm以下, 平均值为8μm以下。

    Method for producing injection-molded body

    公开(公告)号:US12134217B2

    公开(公告)日:2024-11-05

    申请号:US17627428

    申请日:2020-06-08

    Abstract: A method for producing an injection-molded body from a molding material containing a poly(3-hydroxybutyrate) resin includes: melting the molding material by heating the molding material to a temperature between a melting point peak temperature and a melting point peak end temperature in differential scanning calorimetry analysis of the molding material, wherein the difference between the melting point peak temperature and the melting point peak end temperature of the molding material is from 10 to 70° C.; injecting the molten molding material into a mold having a temperature of 30 to 80° C.; and cooling the molding material in the mold to crystallize and solidify the molding material.

    Polyester resin composition and molded article containing this resin composition
    3.
    发明授权
    Polyester resin composition and molded article containing this resin composition 有权
    聚酯树脂组合物和含有该树脂组合物的模制品

    公开(公告)号:US09475934B2

    公开(公告)日:2016-10-25

    申请号:US14419414

    申请日:2013-07-11

    CPC classification number: C08L67/04 C08G63/06 C08G63/08 C08K5/053

    Abstract: An object is to increase crystallization speed, which is a drawback of polyhydroxyalkanoate, to improve processability in processing such as injection molding or blow molding and increase the speed of processing and is, in addition, to refine the crystal of polyhydroxyalkanoate to suppress a change of mechanical properties with passage of time of a resulting molded article. Disclosed herein is a polyester resin composition containing polyhydroxyalkanoate and pentaerythritol.

    Abstract translation: 目的是提高结晶速度,这是聚羟基链烷酸酯的缺点,以提高加工中的加工性能,例如注射成型或吹塑成型,并提高加工速度,此外,为了改善聚羟基链烷酸酯的结晶以抑制 机械性能随着所得模塑制品的时间流逝。 本文公开了含有聚羟基链烷酸酯和季戊四醇的聚酯树脂组合物。

    POLYESTER RESIN COMPOSITION AND MOLDED ARTICLE CONTAINING THIS RESIN COMPOSITION
    4.
    发明申请
    POLYESTER RESIN COMPOSITION AND MOLDED ARTICLE CONTAINING THIS RESIN COMPOSITION 有权
    聚酯树脂组合物和含有该树脂组合物的模塑制品

    公开(公告)号:US20150210801A1

    公开(公告)日:2015-07-30

    申请号:US14419414

    申请日:2013-07-11

    CPC classification number: C08L67/04 C08G63/06 C08G63/08 C08K5/053

    Abstract: An object is to increase crystallization speed, which is a drawback of polyhydroxyalkanoate, to improve processability in processing such as injection molding or blow molding and increase the speed of processing and is, in addition, to refine the crystal of polyhydroxyalkanoate to suppress a change of mechanical properties with passage of time of a resulting molded article. Disclosed herein is a polyester resin composition containing polyhydroxyalkanoate and pentaerythritol.

    Abstract translation: 目的是提高结晶速度,这是聚羟基链烷酸酯的缺点,以提高加工中的加工性能,例如注射成型或吹塑成型,并提高加工速度,此外,为了改善聚羟基链烷酸酯的结晶以抑制 机械性能随着所得模塑制品的时间流逝。 本文公开了含有聚羟基链烷酸酯和季戊四醇的聚酯树脂组合物。

    BIODEGRADABLE POLYESTER RESIN COMPOSITION
    5.
    发明申请
    BIODEGRADABLE POLYESTER RESIN COMPOSITION 有权
    生物可降解聚酯树脂组合物

    公开(公告)号:US20150073079A1

    公开(公告)日:2015-03-12

    申请号:US14388954

    申请日:2013-03-29

    Abstract: This invention aims at improving the tear strength of a film and a sheet molded from a resin composition containing microorganism-produced aliphatic polyester. This invention relates to a biodegradable polyester resin composition containing polybutylene adipate terephthalate (PBAT) in the proportion of 60 to 400 parts by weight and modified-glycerin in the proportion of 10 to 50 parts by weight based on 100 parts by weight of aliphatic polyester (P3HA) having a repeating unit represented by Formula (1): [—CHR—CH2—CO—O—] (wherein R is an alkyl group represented by CnH2n+1 and n is an integer of 1 or more and 15 or lower) and a film or a sheet obtained by molding the biodegradable polyester resin composition in which the maximum major axis of phases containing the aliphatic polyester (P3HA) measured by a transmission electron microscopy analysis-image analysis method (TEM method) is 18 μm or lower and the average value is 8 μm or lower.

    Abstract translation: 本发明的目的在于提高膜和由含有微生物生产的脂肪族聚酯的树脂组合物成型的片材的撕裂强度。 本发明涉及以聚对苯二甲酸丁二醇酯(PBAT)为60〜400重量份的生物降解性聚酯树脂组合物,相对于100重量份的脂肪族聚酯为10〜50重量份的改性甘油 具有由式(1)表示的重复单元的化合物(其中R是由C n H 2n + 1表示的烷基,n是1以上且15以下的整数) 以及通过透射电子显微镜分析图像分析方法(TEM法)测定的含有脂肪族聚酯(P3HA)的相的最大长轴的生物降解性聚酯树脂组合物成型为18μm以下, 平均值为8μm以下。