Method for producing composition for melt processing

    公开(公告)号:US12240955B2

    公开(公告)日:2025-03-04

    申请号:US17627356

    申请日:2020-07-10

    Abstract: A method for producing a poly(3-hydroxybutyrate) resin-containing composition for melt processing includes: heating a material containing a poly(3-hydroxybutyrate) resin to a temperature equal to or higher than a melting point peak temperature in differential scanning calorimetry analysis of the poly(3-hydroxybutyrate) resin and equal to or lower than a melting point peak end temperature in the differential scanning calorimetry analysis of the poly(3-hydroxybutyrate) resin, wherein the difference between the melting point peak temperature and the melting point peak end temperature of the poly(3-hydroxybutyrate) resin is 10° C. or more; and extruding the heated material to obtain a composition for melt processing that has a new crystallization peak at a temperature higher than the melting point peak temperature.

    POLYESTER RESIN COMPOSITION AND METHOD FOR PRODUCING SAME
    2.
    发明申请
    POLYESTER RESIN COMPOSITION AND METHOD FOR PRODUCING SAME 有权
    聚酯树脂组合物及其生产方法

    公开(公告)号:US20150232660A1

    公开(公告)日:2015-08-20

    申请号:US14433504

    申请日:2013-10-01

    Abstract: Provided is a resin composition that is suitable for use in producing a film or sheet having high tear strength and is excellent in processability, mechanical properties, and biodegradability. The resin composition is a biodegradable polyester resin composition containing an aliphatic polyester (P3HA) having a repeating unit represented by the following general formula (1) [—CHR—CH2—CO—O—]  (1) (wherein R is an alkyl group represented by CnH2n+1 and n is an integer of 1 or more and 15 or less), polybutylene adipate terephthalate (PBAT), and hydrophilic silica (A), wherein a weight ratio of the aliphatic polyester (P3HA) to the polybutylene adipate terephthalate (PBAT) is 90/10 to 10/90, and an amount of the hydrophilic silica (A) contained is 2 to 30 parts by weight with respect to 100 parts by weight of a total amount of the aliphatic polyester (P3HA) and the polybutylene adipate terephthalate (PBAT) contained.

    Abstract translation: 本发明提供一种适用于制造撕裂强度高,加工性,机械特性,生物降解性优异的膜或片的树脂组合物。 树脂组合物是含有具有下述通式(1)表示的重复单元的脂肪族聚酯(P3HA)[-CHR-CH2-CO-O-](1)(式中,R为烷基)的生物降解性聚酯树脂组合物 由CnH2n + 1表示,n为1以上且15以下的整数),聚对苯二甲酸丁二醇酯(PBAT)和亲水性二氧化硅(A),其中脂肪族聚酯(P3HA)与聚己二酸丁二醇酯 (PBAT)为90/10〜10/90,亲水性二氧化硅(A)的含量相对于脂肪族聚酯(P3HA)的总量100重量份为2〜30重量份, 聚对苯二甲酸丁二醇酯(PBAT)。

    Poly(3-hydroxybutyrate) resin tube and method for producing same

    公开(公告)号:US12221538B2

    公开(公告)日:2025-02-11

    申请号:US17266676

    申请日:2019-08-19

    Inventor: Tetsuo Okura

    Abstract: Provided is a poly(3-hydroxybutyrate) resin tube including a poly(3-hydroxybutyrate) resin, the tube having a wall thickness of 0.1 to 0.6 mm. The difference between the melting point peak temperature and the melting point peak end temperature in differential scanning calorimetry analysis of the poly(3-hydroxybutyrate) resin is preferably 10° C. or higher. Preferably, production of the tube includes the step of melting a poly(3-hydroxybutyrate) resin in an extruder, then extruding the resin from an annular die, and introducing the resin into water, the annular die temperature being set to a temperature between the melting point peak temperature and the melting point peak end temperature in differential scanning calorimetry analysis of the poly(3-hydroxybutyrate) resin.

    Polyester resin composition and method for producing same

    公开(公告)号:US09850376B2

    公开(公告)日:2017-12-26

    申请号:US14433504

    申请日:2013-10-01

    Abstract: A resin composition for producing a film or sheet having high tear strength that is excellent in processability, mechanical properties, and biodegradability. The resin composition is a biodegradable polyester resin composition containing: (i) an aliphatic polyester (P3HA) having a repeating unit of formula (1): [—CHR—CH2—CO—O—] (1), wherein R is an alkyl group represented by CnH2n+1, where n is an integer of 1 or more and 15 or less; (ii) polybutylene adipate terephthalate (PBAT); and hydrophilic silica (A), wherein a weight ratio of the aliphatic polyester (P3HA) to the polybutylene adipate terephthalate (PBAT) is 90/10 to 10/90, and an amount of the hydrophilic silica (A) is 2 to 30 parts by weight with respect to 100 parts by weight of a total amount of the aliphatic polyester (P3HA) and the polybutylene adipate terephthalate (PBAT) combined.

Patent Agency Ranking