Nickel-metal hydride storage battery
    6.
    发明申请
    Nickel-metal hydride storage battery 审中-公开
    镍氢蓄电池

    公开(公告)号:US20060078794A1

    公开(公告)日:2006-04-13

    申请号:US11244034

    申请日:2005-10-06

    IPC分类号: H01M4/58 H01M4/62

    摘要: Middle point voltage of discharge is increased and at the same time cycle life improved in a nickel-metal hydride storage battery having a negative electrode utilizing a rare earth-nickel hydrogen-absorbing alloy containing Mg and the like and having a crystal structure other than a CaCu5 structure. A nickel-metal hydride storage battery contains a positive electrode (1), a negative electrode (2) including a hydrogen-absorbing alloy, and an alkaline electrolyte solution. The hydrogen-absorbing alloy contains at least a rare-earth element, magnesium, nickel, and aluminum, and has an intensity ratio IA/IB of 0.1 or greater as determined by X-ray diffraction analysis using Cu-Kα radiation as an X-ray source, where IA is the strongest peak intensity that appears in the range of 20=30° to 34°, and IB is the strongest peak intensity that appears in the range of 2θ=40° to 44°. The negative electrode contains a cobalt compound.

    摘要翻译: 使用含有Mg等的稀土 - 镍氢吸收合金的具有负极的镍金属氢化物蓄电池中,放电的中点电压增加,同时循环寿命得到改善,并具有不同于 CaCu 5< 5>结构。 镍氢蓄电池包含正极(1),含有吸氢合金的负极(2)和碱性电解质溶液。 吸氢合金至少含有稀土元素镁,镍和铝,并且其强度比为0.1或更大,为0.1或更大,为 通过使用Cu-Kalpha辐射的X射线衍射分析确定为X射线源,其中I A是在20 = 30°至34°的范围内出现的最强峰强度,I B 是在2θ= 40°至44°的范围内出现的最强峰值强度。 负极含有钴化合物。

    NEGATIVE ELECTRODE FOR ALKALINE STORAGE BATTERY AND ALKALINE STORAGE BATTERY
    7.
    发明申请
    NEGATIVE ELECTRODE FOR ALKALINE STORAGE BATTERY AND ALKALINE STORAGE BATTERY 审中-公开
    碱性电池和碱性电池的负极电极

    公开(公告)号:US20110052983A1

    公开(公告)日:2011-03-03

    申请号:US12872601

    申请日:2010-08-31

    IPC分类号: H01M4/62 H01M4/525

    摘要: An alkaline storage battery having a positive electrode (1), a negative electrode (2), and an alkaline electrolyte solution, and the negative electrode having fluorinated oil being present on the surface thereof. The negative electrode includes a hydrogen-absorbing alloy represented by the general formula Ln1-xMgxNiy-a-bAlaMb, where Ln is at least one element selected from Zr, Ti, and a rare-earth element including Y; M is at least one element selected from the group consisting of V, Nb, Ta, Cr, Mo, Mn, Fe, Co, Ga, Zn, Sn, In, Cu, Si, P, and B; 0.05≦x≦0.30; 0.05≦a≦0.30; 0≦b≦0.50; and 2.8≦y≦3.9.

    摘要翻译: 具有正极(1),负极(2)和碱性电解液的碱性蓄电池,其表面上存在氟化油的负极。 负极包括由通式Ln1-xMgxNiy-a-bAlaMb表示的吸氢合金,其中Ln是选自Zr,Ti和包含Y的稀土元素中的至少一种元素; M是选自V,Nb,Ta,Cr,Mo,Mn,Fe,Co,Ga,Zn,Sn,In,Cu,Si,P和B中的至少一种元素; 0.05≦̸ x≦̸ 0.30; 0.05≦̸ a≦̸ 0.30; 0≦̸ b≦̸ 0.50; 和2.8≦̸ y≦̸ 3.9。

    Hydrogen-absorbing alloy electrode and alkaline storage battery
    8.
    发明申请
    Hydrogen-absorbing alloy electrode and alkaline storage battery 有权
    吸氢合金电极和碱性蓄电池

    公开(公告)号:US20060046141A1

    公开(公告)日:2006-03-02

    申请号:US11169901

    申请日:2005-06-30

    IPC分类号: H01M4/58

    摘要: A hydrogen-absorbing alloy for a negative electrode in an alkaline storage battery includes a first hydrogen-absorbing alloy and a second first hydrogen-absorbing alloy. The first hydrogen-absorbing alloy contains at least a rare-earth element, Mg, Ni, and Al, and has an intensity ratio IA/IB of 0.1 or greater in X-ray diffraction analysis using Cu—Kα radiation as an X-ray source, where IA is the strongest peak intensity that appears in the range of 2θ=31° to 33°, and IB is the strongest peak intensity that appears in the range of 2θ=40° to 44°. The second hydrogen-absorbing alloy has a Co content greater than that of the first hydrogen-absorbing alloy.

    摘要翻译: 碱性蓄电池中的负极吸氢合金包括第一吸氢合金和第二第一吸氢合金。 第一吸氢合金含有至少一种稀土元素Mg,Ni和Al,并且其强度比为0.1或更大的强度比I SUB / I B B 在使用Cu-Kalpha辐射作为X射线源的X射线衍射分析中,其中I A是在2θ= 31°至33°的范围内出现的最强峰强度,I < SUB> B 是出现在2θ= 40°至44°范围内的最强峰值强度。 第二吸氢合金的Co含量大于第一吸氢合金的Co含量。

    Nickel metal hydride storage battery
    9.
    发明申请
    Nickel metal hydride storage battery 审中-公开
    镍氢蓄电池

    公开(公告)号:US20050100789A1

    公开(公告)日:2005-05-12

    申请号:US10964741

    申请日:2004-10-15

    摘要: A nickel metal hydride storage battery including a positive electrode, a negative electrode including a hydrogen absorbing alloy, and an alkaline electrolyte, the hydrogen absorbing alloy containing at least a rare-earth element, magnesium, nickel and aluminum, and having an intensity ratio (IA/IB) of not smaller than 0.1 (where IA represents an intensity of the highest peak in a range of 2θ=30°˜34° in an X-ray diffraction pattern using CuKα-radiation as the X-ray source and IB represents the intensity of the highest peak in a range of 2θ=40°˜44° in an X-ray diffraction pattern using CuKα-radiation as the X-ray source), and the battery containing manganese in an amount of not greater than 1.0 wt % relative to the hydrogen absorbing alloy.

    摘要翻译: 一种镍金属氢化物蓄电池,包括正极,含有吸氢合金的负极和碱性电解质,所述吸氢合金至少含有稀土元素,镁,镍和铝,并且具有强度比( 不小于0.1(其中I A表示在2θ= 30的范围内的最高峰的强度) 在使用CuKαα-辐射作为X射线源的X射线衍射图中,I〜34°,I B 表示在 2θ= 40°〜44°的X射线衍射图,使用CuKα-α射线作为X射线源),含锰量相对不大于1.0wt% 到吸氢合金。