Thermoplastic elastomers of good dyeability and high strength and elasticity as well as impact-resistant polymer blends produced therefrom
    2.
    发明授权
    Thermoplastic elastomers of good dyeability and high strength and elasticity as well as impact-resistant polymer blends produced therefrom 失效
    具有良好的可染性和高强度和弹性的热塑性弹性体以及由其制备的耐冲击聚合物共混物

    公开(公告)号:US06310140B1

    公开(公告)日:2001-10-30

    申请号:US09229416

    申请日:1999-04-19

    IPC分类号: C08F800

    摘要: Thermoplastic elastomers of good dyeability and high strength and elasticity, the incorporated elastomeric particles of which have and average particle diameter of 0.05 to 5 &mgr;m. The thermoplastic elastomers are formed according to a method in which mixtures of propylene homopolymers and/or propylene copolymers, elastomeric C4 C12 olefin copolymers and/or terpolymers and C8 to C14 diacrylates, C7 to C16 diallyl compounds, C9 to C15 dimethacrylates, C7 to C10 divinyl compounds, C12 to C17 acrylate esters of polyalcohols, C15 to C21 methacrylate esters of polyalcohols and/or C9 C12 triallyl compounds are added to a melt. The thermoplastic elastomers, as well as mixtures of the thermoplastic elastomers with conventional polyolefins, are suitable for use in the vehicle industry, in the domestic appliances industry, in the construction industry and in medical technology.

    摘要翻译: 具有良好的染色性和高强度和弹性的热塑性弹性体,其结合的弹性体颗粒具有0.05至5μm的平均粒径。 热塑性弹性体是根据丙烯均聚物和/或丙烯共聚物,弹性体C 4 C 12烯烃共聚物和/或三元共聚物和C 8至C 14二丙烯酸酯,C 7至C 16二烯丙基化合物,C 9至C 15二甲基丙烯酸酯,C 7至C 10 二乙烯基化合物,多元醇的C12〜C17丙烯酸酯,多元醇的C15〜C21甲基丙烯酸酯和/或C9 C12三烯丙基化合物加入到熔体中。 热塑性弹性体以及热塑性弹性体与常规聚烯烃的混合物适用于汽车工业,家用电器工业,建筑业和医疗技术领域。