Accelerated furanic aggregate binders from bio-derived components
    1.
    发明申请
    Accelerated furanic aggregate binders from bio-derived components 审中-公开
    来自生物衍生组分的加速的呋喃聚集体粘合剂

    公开(公告)号:US20080125517A1

    公开(公告)日:2008-05-29

    申请号:US11904723

    申请日:2007-09-28

    IPC分类号: B22C1/22 B22C1/20

    CPC分类号: B22C1/224

    摘要: Broadly, the invention provides for newly available bio-derived formaldehyde-free furanic materials for aggregate binding. A specific example is aggregate binding for forms used in the metal casting process. The inventive binder formulations involve the use of 2,5-furan dimethanol and other “filler” components for high productivity and fast tensile development without formaldehyde, urea, urea-formaldehyde or formaldehyde containing compositions.

    摘要翻译: 广泛地,本发明提供了用于聚集结合的新近可用的生物衍生的无甲醛呋喃材料。 一个具体的例子是在金属铸造过程中使用的形式的聚合结合。 本发明的粘合剂制剂涉及使用2,5-呋喃二甲醇和其它“填料”组分,用于高生产率和快速拉伸显影,而不含甲醛,尿素,脲醛或含甲醛的组合物。

    Furanic resin aggregate binders and method
    3.
    发明申请
    Furanic resin aggregate binders and method 审中-公开
    呋喃树脂骨料和方法

    公开(公告)号:US20080207796A1

    公开(公告)日:2008-08-28

    申请号:US11865404

    申请日:2007-10-01

    IPC分类号: B22C1/22

    摘要: Broadly, the invention provides for newly available bio-derived formaldehyde free furanic materials for aggregate binding. The specific example case is aggregate binding for forms used in the metal casting process. The new materials make possible higher productivity and lower phenol, formaldehyde, urea, and/or furfuryl alcohol content in the metal casting form-making process. It is expected that the formulations will work well in other aggregate binding situations as well.

    摘要翻译: 广泛地,本发明提供了用于聚集结合的新近可用的生物衍生的不含甲醛的呋喃形物质。 具体的示例情况是用于金属铸造工艺中的形式的聚合结合。 新型材料可以提高生产率,并降低金属铸造成型工艺中的苯酚,甲醛,尿素和/或糠醇含量。 预期配方在其他聚合物结合情况下也能很好地起作用。

    Use of bisphenol a tar in furan no-bake foundry binders
    10.
    发明授权
    Use of bisphenol a tar in furan no-bake foundry binders 失效
    在呋喃无烘烤铸造粘合剂中使用双酚焦油

    公开(公告)号:US5856375A

    公开(公告)日:1999-01-05

    申请号:US583178

    申请日:1996-01-04

    IPC分类号: B22C1/22

    CPC分类号: B22C1/224

    摘要: Broadly, the present invention relates to furan no-bake foundry binders where bisphenol A tar (BPAT) is used to replace a portion of the furfuryl alcohol and any conventional filler optionally included in for binder formulation. Reduction in the amount of furfuryl alcohol in the foundry binder formulation may lead to a reduction in the cost and an improvement in early strength of these formulations. Accordingly, in a furan no-bake foundry binder of a resin derived from a major proportion of furfuryl alcohol and optionally fillers, the improvement which comprises at least a fraction of said furfuryl alcohol being bisphenol A tar. Bisphenol A tar also can replace at least a fraction of any filler included in the binder formulation.

    摘要翻译: 广义上,本发明涉及呋喃无烘烤铸造粘合剂,其中使用双酚A焦油(BPAT)来代替一部分糠醇,以及任选地包括在粘合剂制剂中的任何常规填料。 铸造粘合剂制剂中糠醇的量的减少可导致成本的降低和这些制剂的早期强度的改善。 因此,在主要比例的糠醇和任选的填料的呋喃无烘烤铸造粘结剂中,至少包含一部分所述糠醇为双酚A焦油的改进。 双酚A焦油还可以替代粘合剂制剂中包含的任何填料的至少一部分。