摘要:
A process for the production of a lignocellulose-containing material, in which, based in each case on the lignocellulose-containing material: A) from 30 to 95% by weight of lignocellulose particles; B) from 1 to 25% by weight of expanded plastic particles having a bulk density in the range from 10 to 150 kg/m3; C) from 1 to 50% by weight of a binder selected from the group consisting of aminoplast resin, phenol-formaldehyde resin and organic isocyanate having at least two isocyanate groups, and optionally D) additives are mixed and are then pressed at elevated temperature and under elevated pressure, wherein the component B) comprises a curing agent for the component C).
摘要翻译:一种用于生产含木素纤维素的材料的方法,其中基于含木素纤维素的材料:A)30至95重量%的木质纤维素颗粒; B)1至25重量%的堆积密度在10至150kg / m 3范围内的发泡塑料颗粒; C)1至50重量%的选自氨基塑料树脂,酚醛树脂和具有至少两个异氰酸酯基团的有机异氰酸酯和任选的D)添加剂的粘合剂混合,然后在升高的温度下压制, 在高压下,其中组分B)包含组分C)的固化剂。
摘要:
A process for the production of a lignocellulose-containing material, in which, based in each case on the lignocellulose-containing material: A) from 30 to 95% by weight of lignocellulose particles; B) from 1 to 25% by weight of expanded plastic particles having a bulk density in the range from 10 to 150 kg/m3; C) from 1 to 50% by weight of a binder selected from the group consisting of aminoplast resin, phenol-formaldehyde resin and organic isocyanate having at least two isocyanate groups, and optionally D) additives are mixed and are then pressed at elevated temperature and under elevated pressure, wherein the component B) comprises a formaldehyde scavenger.
摘要翻译:一种用于生产含木素纤维素的材料的方法,其中基于含木素纤维素的材料:A)30至95重量%的木质纤维素颗粒; B)1至25重量%的堆积密度在10至150kg / m 3范围内的发泡塑料颗粒; C)1至50重量%的选自氨基塑料树脂,酚醛树脂和具有至少两个异氰酸酯基团的有机异氰酸酯和任选的D)添加剂的粘合剂混合,然后在升高的温度下压制, 在高压下,其中组分B)包含甲醛清除剂。
摘要:
A process for the production of a lignocellulose-containing material, in which, based in each case on the lignocellulose-containing material: A) from 30 to 95% by weight of lignocellulose particles; B) from 1 to 25% by weight of expanded plastic particles having a bulk density in the range from 10 to 150 kg/m3; C) from 1 to 50% by weight of a binder selected from the group consisting of aminoplast resin, phenol-formaldehyde resin and organic isocyanate having at least two isocyanate groups, and optionally D) additives are mixed and are then pressed at elevated temperature and under elevated pressure, wherein the component B) comprises a formaldehyde scavenger.
摘要翻译:一种用于生产含木素纤维素的材料的方法,其中基于含木素纤维素的材料:A)30至95重量%的木质纤维素颗粒; B)1至25重量%的堆积密度在10至150kg / m 3范围内的发泡塑料颗粒; C)1至50重量%的选自氨基塑料树脂,酚醛树脂和具有至少两个异氰酸酯基团的有机异氰酸酯和任选的D)添加剂的粘合剂混合,然后在升高的温度下压制, 在高压下,其中组分B)包含甲醛清除剂。
摘要:
A light wood-containing material having an average density in the range from 200 to 600 kg/m3, comprising, based in each case on the wood-containing material: A) from 30 to 95% by weight of wood particles; B) from 1 to 25% by weight of a filler having a bulk density in the range from 10 to 150 kg/m3, selected from the group consisting of foamable plastic particles and already foamed plastic particles; C) from 0.1 to 50% by weight of a binder and, if appropriate, D) additives, the following relationship being true for the d′ values according to Rosin-Rammler-Sperling-Bennet of the wood particles A) and of the particles of the filler B): d′ of the particles A) ≦2.5×d′ of the particles B).
摘要翻译:平均密度为200至600kg / m 3的含轻木材的材料包括基于木材的材料:A)30至95重量%的木材颗粒; B)1至25重量%的堆积密度在10至150kg / m 3范围内的填料,其选自可发泡塑料颗粒和已发泡塑料颗粒; C)0.1至50重量%的粘合剂,并且如果合适,D)添加剂,根据木材颗粒A)和木颗粒A)的松香 - 拉姆勒 - 斯珀林 - 班奈特 的填料B):d'颗粒A)≦̸ 2.5×d'的颗粒B)。
摘要:
A light wood-containing material having an average density in the range from 200 to 600 kg/m3, comprising, based in each case on the wood-containing material: A) from 30 to 95% by weight of wood particles; B) from 1 to 25% by weight of a filler having a bulk density in the range from 10 to 150 kg/m3, selected from the group consisting of foamable plastic particles and already foamed plastic particles; C) from 0.1 to 50% by weight of a binder and, if appropriate, D) additives, the following relationship being true for the d′ values according to Rosin-Rammler-Sperling-Bennet of the wood particles A) and of the particles of the filler B): d′ of the particles A)≦2.5×d′ of the particles B).
摘要翻译:平均密度为200至600kg / m 3的含轻木材的材料包括基于木材的材料:A)30至95重量%的木材颗粒; B)1至25重量%的堆积密度在10至150kg / m 3范围内的填料,其选自可发泡塑料颗粒和已发泡塑料颗粒; C)0.1至50重量%的粘合剂,并且如果合适,D)添加剂,根据木材颗粒A)和木颗粒A)的松香 - 拉姆勒 - 斯珀林 - 班奈特 的填料B):d'颗粒A)≦̸ 2.5×d'的颗粒B)。
摘要:
A process for the production of a lignocellulose-containing material, in which, based in each case on the lignocellulose-containing material: A) from 30 to 95% by weight of lignocellulose particles; B) from 1 to 25% by weight of expanded plastic particles having a bulk density in the range from 10 to 150 kg/m3; C) from 1 to 50% by weight of a binder selected from the group consisting of aminoplast resin, phenol-formaldehyde resin and organic isocyanate having at least two isocyanate groups, and optionally D) additives are mixed and are then pressed at elevated temperature and under elevated pressure, wherein the component B) comprises a curing agent for the component C).
摘要翻译:一种用于生产含木素纤维素的材料的方法,其中基于含木素纤维素的材料:A)30至95重量%的木质纤维素颗粒; B)1至25重量%的堆积密度在10至150kg / m 3范围内的发泡塑料颗粒; C)1至50重量%的选自氨基塑料树脂,酚醛树脂和具有至少两个异氰酸酯基团的有机异氰酸酯和任选的D)添加剂的粘合剂混合,然后在升高的温度下压制, 在高压下,其中组分B)包含组分C)的固化剂。
摘要:
A process for the production of a lignocellulose-containing substance having an average density in the range from more than 600 to 900 kg/m3, in which, in each case based on the lignocellulose-containing substance: A) from 30 to 95% by weight of lignocellulose particles; B) from 1 to 25% by weight of expanded plastics particles having a bulk density in the range from 10 to 100 kg/m3; C) from 3 to 50% by weight of a binder selected from the group consisting of aminoplast resin, phenol-formaldehyde resin and organic isocyanate having at least two isocyanate groups and, if appropriate D) additives, are mixed and then pressed at elevated temperature and under elevated pressure.
摘要翻译:一种生产含木素纤维素的物质的方法,其平均密度为600-900kg / m3以上,其中,基于含木素纤维素的物质,A)为30〜95% 木质纤维素颗粒重量; B)1至25重量%的堆积密度在10至100kg / m 3范围内的发泡塑料颗粒; C)3至50重量%的选自氨基塑料树脂,酚醛树脂和具有至少两个异氰酸酯基团的有机异氰酸酯和如果合适的D)添加剂的粘合剂混合,然后在高温下压制 并在高压下。
摘要:
The present invention relates to light wood-base materials comprising from 30 to 92.5% by weight, based on the wood-base material, of wood particles, the wood particles having a mean density of from 0.4 to 0.85 g/cm3, from 2.5 to 20% by weight, based on the wood-base material, of polystyrene and/or of styrene copolymer as a filler, the filler having a bulk density of from 10 to 100 kg/m3, and from 5 to 50% by weight, based on the wood-base material, of a binder, the mean density of the light wood-base material being less than or equal to 600 kg/m3.
摘要翻译:本发明涉及轻木基材料,其包含基于木质材料的木质颗粒的30至92.5重量%,木材颗粒的平均密度为0.4至0.85g / cm 3,2.5至 基于木质材料的20重量%的聚苯乙烯和/或作为填料的苯乙烯共聚物,填料的堆积密度为10至100kg / m 3,和5至50重量%,基于 在木基材料上的粘合剂中,轻木基材料的平均密度小于或等于600kg / m 3。
摘要:
The present invention relates to light wood-base materials comprising from 30 to 92.5% by weight, based on the wood-base material, of wood particles, the wood particles having a mean density of from 0.4 to 0.85 g/cm3, from 2.5 to 20% by weight, based on the wood-base material, of polystyrene and/or of styrene copolymer as a filler, the filler having a bulk density of from 10 to 100 kg/m3, and from 5 to 50% by weight, based on the wood-base material, of a binder, the mean density of the light wood-base material being less than or equal to 600 kg/m3.
摘要翻译:本发明涉及轻木基材料,其包含基于木质材料的木质颗粒的30至92.5重量%,木材颗粒的平均密度为0.4至0.85g / cm 3,2.5至 基于木质材料的20重量%的聚苯乙烯和/或作为填料的苯乙烯共聚物,填料的堆积密度为10至100kg / m 3,和5至50重量%,基于 在木基材料上的粘合剂中,轻木基材料的平均密度小于或等于600kg / m 3。
摘要:
A light wood-containing material having an average density in the range from 200 to 600 kg/m3, comprising, based in each case on the wood-containing material: A) from 30 to 95% by weight of wood particles; B) from 1 to 15% by weight of a filler having a bulk density in the range from 10 to 100 kg/m3, selected from the group consisting of foamable plastic particles and already foamed plastic particles; C) from 3 to 50% by weight of a binder comprising an aminoplast resin and an organic isocyanate having at least two isocyanate groups and, if appropriate, D) additives.
摘要翻译:平均密度为200至600kg / m 3的含轻木材的材料包括基于木材的材料:A)30至95重量%的木材颗粒; B)1至15重量%的堆积密度在10至100kg / m 3范围内的填料,其选自可发泡塑料颗粒和已发泡塑料颗粒; C)3至50重量%的包含氨基塑料树脂和具有至少两个异氰酸酯基团的有机异氰酸酯和如果合适的话,D)添加剂的粘合剂。