摘要:
The present invention provides a conductive member in which it is possible to control a variation in resistance due to physical stress from a contact member, and an uneven density in a halftone image can be prevented.The conductive member is a development roller which includes a conductive shaft core, a conductive elastic layer, and a conductive surface layer. The conductive elastic layer contains silicone rubber and a basic carbon black dispersed in the silicone rubber. The surface layer contains a urethane resin having a carboxyl group in its molecule and an acidic carbon black dispersed in the urethane resin.
摘要:
The present invention provides a conductive member in which it is possible to control a variation in resistance due to physical stress from a contact member, and an uneven density in a halftone image can be prevented.The conductive member is a development roller which includes a conductive shaft core, a conductive elastic layer, and a conductive surface layer. The conductive elastic layer contains silicone rubber and a basic carbon black dispersed in the silicone rubber. The surface layer contains a urethane resin having a carboxyl group in its molecule and an acidic carbon black dispersed in the urethane resin.
摘要:
A developing roller having a surface layer which contains a urethane resin composed of a reaction product of an isocyanate with a group of specific alcohols and has a surface having a contact angle to ethylene glycol of from 60.0 degrees or more to 90.0 degrees or less and a contact angle to diiodomethane of from 30.0 degrees or more to 38.0 degrees or less. The developing roller is highly reliable as having controlled banding which is an image difficulty caused at the part of contact between the developing roller and a developer feed roller.
摘要:
The invention relates to a developing roller capable of suppressing scattering of toner during a developing process and providing a further higher-quality electrophotographic image. The developing roller has a mandrel, an elastic layer provided on the circumference of the mandrel, and a surface layer provided on the circumference of the elastic layer. The surface layer contains a urethane resin serving as a binder and urethane resin particles dispersed in the binder, for forming convex portions on the surface of the surface layer. The surface of the urethane resin particle is partly covered with fine inorganic particles containing at least one element selected from silicon, titanium and aluminum and the urethane resin particles are in direct contact with the binder at the surface onto which the fine inorganic particles are not attached.
摘要:
A developing roller suppresses scattering of toner during a developing process and provides a further higher-quality electrophotographic image. The developing roller has a mandrel, an elastic layer provided on the circumference of the mandrel, and a surface layer provided on the circumference of the elastic layer. The surface layer contains a urethane resin serving as a binder and urethane resin particles dispersed in the binder, for forming convex portions on the surface of the surface layer. The surface of the urethane resin particles is partly covered with fine inorganic particles containing at least one element selected from silicon, titanium and aluminum and the urethane resin particles are in direct contact with the binder at the surface onto which the fine inorganic particles are not attached.
摘要:
The present invention intends to provide a method of producing a developing roller capable of providing high-quality electrophotographic images under a variety of environments. The method of producing a developing roller according to the present invention is a method of producing a developing roller having a mandrel, a resin layer on the outer periphery of the mandrel, and a surface layer on the outer periphery of the resin layer, the method including the step of curing a mixture containing a carbon black, a specific diol, and a specific isocyanate compound to form the surface layer.
摘要:
The present invention intends to provide a method of producing a developing roller capable of providing high-quality electrophotographic images under a variety of environments. The method of producing a developing roller according to the present invention is a method of producing a developing roller having a mandrel, a resin layer on the outer periphery of the mandrel, and a surface layer on the outer periphery of the resin layer, the method including the step of curing a mixture containing a carbon black, a specific diol, and a specific isocyanate compound to form the surface layer.
摘要:
A regenerated elastic rollers manufacturing process is provided. The process includes the step of removing an agglutinated stain of toner adhered to the surface of an elastic roller including a mandrel and an elastic layer. The step further includes the steps of: (1) pressing a pressing roller against the surface of the elastic roller so as to crack the agglutinated stain on the surface of the elastic roller; and (2) removing the agglutinated stain cracked in the step (1) from the surface of the elastic roller by means of an adhesive roller.
摘要:
A regenerated elastic rollers manufacturing process is provided. The process includes the step of removing an agglutinated stain of toner adhered to the surface of an elastic roller including a mandrel and an elastic layer. The step further includes the steps of: (1) pressing a pressing roller against the surface of the elastic roller so as to crack the agglutinated stain on the surface of the elastic roller; and (2) removing the agglutinated stain cracked in the step (1) from the surface of the elastic roller by means of an adhesive roller.
摘要:
A regenerated elastic rollers manufacturing process is provided. The process includes the step of removing an agglutinated stain of toner adhered to the surface of an elastic roller including a mandrel and an elastic layer. The step further includes the steps of: (1) pressing a pressing roller against the surface of the elastic roller so as to crack the agglutinated stain on the surface of the elastic roller; and (2) removing the agglutinated stain cracked in the step (1) from the surface of the elastic roller by means of an adhesive roller.