公开(公告)号:US20230150171A1
公开(公告)日:2023-05-18
申请号:US17997341
申请日:2021-03-08
CPC分类号: B29B9/065 , B29C48/405 , B29C48/022 , C08G64/00 , C08K5/521 , C08L55/02 , B29K2069/00
摘要: A method for producing a polycarbonate resin composition pellet with a twin screw extruder, the polycarbonate resin composition pellet has 30 to 95 mass % of a resin pellet (A) containing more than 40 mass % of a polycarbonate resin in the pellet; not less than 5 mass % and less than 40 mass % of a phosphate ester flame retardant (B) that is a liquid at room temperature; 0 to 50 mass % of polycarbonate resin flake (C); 0 to 30 mass % of an ABS resin (D); and 0 to 15 mass % of an additive (E) other than component (B). The method includes feeding components (A), (C), (D) and (E) in a twin screw extruder and kneading with a first kneading zone; feeding component (B) to a downstream part in the first kneading zone and kneading with a second kneading zone; and decompressing a vent in the downstream part in the second kneading zone.
-
公开(公告)号:US20240076455A1
公开(公告)日:2024-03-07
申请号:US18262683
申请日:2022-01-13
发明人: Toshiyuki TAJIRI , Masaru TAKEHANA
CPC分类号: C08J3/203 , B29B7/48 , B29B7/90 , C08K7/14 , C08L67/02 , B29K2067/006 , C08J2367/02
摘要: A method for manufacturing a fiber-reinforced polybutylene terephthalate resin composition contain 40-90 mass % of a polybutylene terephthalate resin, 10-60 mass % of a reinforcing fiber, and 0-35 mass % of other polymer or additive by using a twin-screw extruder, the method includes using polybutylene terephthalate resin pellets (avg. weight of 16-29 mg) as a raw material for the resin by: (1) kneading the resin and the fiber with a first kneading part; (2) adding the fiber at a part downstream of the first kneading part and performing kneading with a second kneading part; and (3) reducing pressure of a vent at a part downstream of the second kneading part and performing devolatilization, where the first kneading part has a length of 5.0-9.0 D and a specific screw configuration, the second kneading part contains a specific screw configuration, and the production is carried out with a screw shaft torque density of 11.5-19 Nm/cm3.
-