1.
公开(公告)号:US20180034010A1
公开(公告)日:2018-02-01
申请号:US15655980
申请日:2017-07-21
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao LIAO , Ying-Te HUANG , Chao-Hsien LIN , Teng-Ko MA , Ching-Yao YUAN , Chen-Ho LAI
IPC: H01M2/02
Abstract: An aluminum plastic film packaging material for lithium batteries to prolong service life, at least comprising an inner layer and an aluminum foil layer, is performed an anti-corrosion treatment between the inner layer and the aluminum foil layer by one of the following ways: 1) a chromium-containing anti-corrosion layer is formed from an aqueous modified resin containing trivalent chromium; and 2) an adhesive layer with non-chromium material is formed from an aqueous modified resin, an epoxy curing agent, a silane coupling agent and a nano-sized metal oxide particle.
-
2.
公开(公告)号:US20150104698A1
公开(公告)日:2015-04-16
申请号:US14505713
申请日:2014-10-03
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Dein-Run FUNG , Ying-Te HUANG , Chao-Hsien LIN , Ching-Yao YUAN , Teng-Ko MA
IPC: H01M2/02
CPC classification number: H01M2/0287 , H01M2/0277 , H01M2/0285 , H01M10/052
Abstract: A method for lithium aluminum film packaging materials, with water, high temperature and corrosion resistance, the substrate layer, and then layer, aluminum foil layer, anti-corrosion layer, adhesive layer and the inner layer together constitute from the outermost to innermost layer laminate structure in which one side of the aluminum foil layer, or both side surface of the conductive coating material to said coating and curing anticorrosive layer, and the use of fluorine-containing polyurethane resin constituting the laminated rubber layer and the inner layer of corrosion between the adhesive layer, used lithium batteries as plastic film packaging applications, it can promote lithium battery with Merit water resistance, high temperature resistance and corrosion resistance, and enhance the use of lithium batteries in years.
Abstract translation: 一种锂铝薄膜包装材料的方法,具有耐水,耐高温和耐腐蚀的能力,基材层,然后层,铝箔层,防腐层,粘合剂层和内层共同构成从最外层到最内层层压 铝箔层的一面或导电性涂料的两面与所述涂层和固化防腐层的结构以及构成层压橡胶层的含氟聚氨酯树脂的使用和内层的腐蚀之间的结构 粘合剂层,使用锂电池作为塑料薄膜包装应用,可以促进锂电池具有优良的耐水性,耐高温和耐腐蚀性,并且可以在数年内增强锂电池的使用。
-
3.
公开(公告)号:US20180056637A1
公开(公告)日:2018-03-01
申请号:US15682612
申请日:2017-08-22
Applicant: NAN YA PLASTICS CORPORATION
Inventor: Te-Chao LIAO , Ying-Te HUANG , Chen-Ho LAI , Chao-Hsien LIN , Ching-Yao YUAN , Teng-Ko MA
CPC classification number: B32B27/304 , C01D17/00 , C01D17/003 , C01G41/006 , C08F14/06 , C08J5/18 , C08J2327/06 , C08K3/11 , C08K5/0016 , C08K5/005 , C08K5/098 , C08K5/12 , C08K5/1515 , C08L27/06
Abstract: A heat-insulating transparent PVC sheet is formed from a PVC substrate having a thickness of 0.02-2.0 mm and contains heat-insulation pastes evenly distributed over the PVC substrate, since the heat-insulation paste contains an essential component of wolfram cesium powder (WCs) with a chemical formula of CsXNYWO3-ZClC and having a particle size of 0.005-2 μm, the heat-insulating transparent PVC sheet has an excellent weatherability, and particularly before and after tested in 300-hour service life in line with ASTM G-154 specification, has a physical property of weatherability decay rate (%) small than 4%.
-
-