1.
公开(公告)号:US09951406B2
公开(公告)日:2018-04-24
申请号:US14940199
申请日:2015-11-13
Applicant: NATIONAL INSTITUTE OF STANDARDS AND TECHNOLOGY , Tony Ying
Inventor: Eric A. Lass , Mark R. Stoudt , Carelyn Campbell , Tsineng Tony Ying
Abstract: A primary alloy includes: nickel; copper; zinc; an electrical conductivity from 5.2% International Annealed Copper Standard (IACS) to 5.6% IACS measured in accordance with ASTM E1004-09 (2009); and a disordered crystalline phase wherein atoms of the nickel, cooper, and zinc are randomly arranged in the disordered crystalline phase at room temperature in a post-annealed state. A process for making the primary alloy includes heating a secondary alloy to a first temperature that is greater than or equal to an annealing temperature to form an annealing alloy, the secondary alloy including a secondary phase; and quenching, by cooling the annealing alloy from the first temperature to a second temperature that is less than the annealing temperature, under a condition effective to form the primary alloy including the disordered crystalline phase, wherein the disordered crystalline phase is different than the secondary phase of the secondary alloy.