Abstract:
An object of the present invention is to provide, as a simple method, a surface nitriding treatment method of a titanium material, forming a hardened nitrided layer excellent in abrasion resistance on the surface of a titanium material in a shorter time. In order to achieve the object, the present invention adopts a surface nitriding treatment method of a titanium material, wherein a hardened nitrided layer is formed on the surface of the titanium material, by blowing nitrogen gas at a flow rate of 10 L/min or more to the surface of the titanium material while the titanium material is being heated to 800° C. to 1000° C. in an inert gas atmosphere.
Abstract:
An induction heating coil (3) has a primary coil (4) to which electric power is supplied and a ring-shaped secondary coil (5) forming a closed circuit. The primary coil (4) has a base-side portion that covers an outer periphery of the secondary coil (5) and a distal-side portion extending from the base-side portion in the center axis direction of the secondary coil (5) in a state in which the base-side portion covers the secondary coil (5). The opening width of the base-side portion is greater than the opening width of the distal-side portion. The secondary coil (5) is provided such that it can be inserted into and removed from the inside of the primary coil (4) from the base-side portion of the primary coil (4).