Abstract:
Provided is a carbon material having a large specific surface area and good filling properties. The carbon material has a circularity of more than 0.83 and a specific surface area of not less than 400 m2/g. The carbon material is produced by a production method includes: providing a suspension containing first carbon particles having a specific surface area of not less than 50 m2/g, a water-soluble binder, and water; obtaining granular bodies from the suspension; and subjecting the granular bodies to heat treatment to obtain second carbon particles.
Abstract:
A positive electrode active material for non-aqueous secondary battery includes core particles containing a lithium transition metal composite oxide, and a covering layer covering, that covers a surface of the core particle. The covering layer contains niobium and carbonate ions, and the carbonate ions are present at a concentration of from 0.2 weight % to 0.4 weight %. The positive electrode active material for non-aqueous secondary battery exhibits infrared absorption peaks at a wavenumber range of from 1320 cm−1 to 1370 cm−1, and at a wavenumber range of from 1640 cm−1 to 1710 cm−1.
Abstract:
Provided is a positive electrode composition with which a lithium sulfur battery may achieve a high cycle capacity retention. The positive electrode composition for lithium sulfur batteries includes a sulfur-carbon composite including a carbon material having void spaces and an elemental sulfur containing material disposed in the void spaces of the carbon material, and a lithium transition metal composite oxide.
Abstract:
A method for producing a nickel cobalt complex hydroxide includes first crystallization of supplying a solution containing Ni, Co and Mn, a complex ion forming agent and a basic solution separately and simultaneously to one reaction vessel to obtain nickel cobalt complex hydroxide particles, and a second crystallization of, after the first crystallization, further supplying a solution containing nickel, cobalt, and manganese, a solution of a complex ion forming agent, a basic solution, and a solution containing said element M separately and simultaneously to the reaction vessel to crystallize a complex hydroxide particles containing nickel, cobalt, manganese and said element M on the nickel cobalt complex hydroxide particles crystallizing a complex hydroxide particles comprising Ni, Co, Mn and the element M on the nickel cobalt complex hydroxide particles.
Abstract:
A method of manufacturing hexagonal boron nitride fibers includes: providing amorphous fibrous boron nitride; performing heat treatment on the amorphous fibrous boron nitride at a first temperature of 500° C. or greater and less than 900° C. in an oxygen-containing atmosphere to obtain a first heat-treated product; and performing heat treatment on the first heat-treated product at a second temperature in a range of 1000° C. to 1800° C. in a nitrogen-containing atmosphere to obtain a second heat-treated product containing hexagonal boron nitride.
Abstract:
A method of producing a nickel-cobalt composite hydroxide includes: preparing a first solution containing nickel ions and cobalt ions; preparing a second solution containing tungsten ions and having a pH of 10 or more; preparing a third solution containing a complex ion-forming factor; preparing a liquid medium having a pH in a range of 10 to 13.5; supplying the first solution, the second solution, and the third solution separately and simultaneously to the liquid medium to obtain a reacted solution having a pH in a range of 10 to 13.5; and obtaining the nickel-cobalt composite hydroxide containing nickel, cobalt, and tungsten from the reacted solution.
Abstract:
A positive electrode active material for non-aqueous secondary battery includes core particles containing a lithium transition metal composite oxide, and a covering layer covering, that covers a surface of the core particle. The covering layer contains niobium and carbonate ions, and the carbonate ions are present at a concentration of from 0.2 weight % to 0.4 weight %. The positive electrode active material for non-aqueous secondary battery exhibits infrared absorption peaks at a wavenumber range of from 1320 cm−1 to 1370 cm−1, and at a wavenumber range of from 1640 cm−1 to 1710 cm−1.
Abstract:
A method for producing a nickel cobalt complex hydroxide includes first crystallization of supplying a solution containing Ni, Co and Mn, a complex ion forming agent and a basic solution separately and simultaneously to one reaction vessel to obtain nickel cobalt complex hydroxide particles, and a second crystallization of, after the first crystallization, further supplying a solution containing nickel, cobalt, and manganese, a solution of a complex ion forming agent, a basic solution, and a solution containing said element M separately and simultaneously to the reaction vessel to crystallize a complex hydroxide particles containing nickel, cobalt, manganese and said element M on the nickel cobalt complex hydroxide particles crystallizing a complex hydroxide particles comprising Ni, Co, Mn and the element M on the nickel cobalt complex hydroxide particles.