发明人: Nobusato MORISHIGE , Kazumi MIZUKAMI , Ryutaro YAMAGATA , Takashi KATAOKA , Haruhiko ATSUMI , Daisuke ITABASHI , Junichi TAKAOBUSHI
IPC分类号: C21D9/46 , C21D8/12 , C22C38/60 , C22C38/06 , C22C38/04 , C22C38/02 , C22C38/00 , H01F1/147 , H01F41/00
CPC分类号: C21D9/46 , C21D8/1222 , C21D8/1233 , C21D8/1272 , C21D8/1283 , C21D8/1255 , C22C38/60 , C22C38/06 , C22C38/04 , C22C38/02 , C22C38/002 , C22C38/001 , C21D8/1261 , H01F1/14775 , H01F41/00 , C21D2201/05 , C22C2202/02
摘要: A new and improved method for producing grain-oriented electrical steel sheet enabling production of grain-oriented electrical steel sheet realizing high magnetic flux density and excellent in magnetic characteristics, that is, as one aspect, a method for producing grain-oriented electrical steel sheet comprising a hot rolling process, cold rolling process, primary recrystallization annealing process, finish annealing process, and flattening annealing process, wherein shot blasting treatment and/or leveling treatment and treatment for contact with a solution are performed, the solution contains Cu etc. in a predetermined amount, the pH is −1.5 or more and less than 7, a solution temperature is 15° C. or more and 100° C. or less, and the time during which the steel sheet is dipped in the solution is 5 seconds or more and 200 seconds or less.