METHOD FOR PRODUCING CARBONITRIDED MEMBER
    1.
    发明申请
    METHOD FOR PRODUCING CARBONITRIDED MEMBER 有权
    生产碳化物的方法

    公开(公告)号:US20120211122A1

    公开(公告)日:2012-08-23

    申请号:US13415198

    申请日:2012-03-08

    IPC分类号: C23C8/32 C23C8/80

    摘要: A method for producing a carbonitrided member comprising the steps of carburizing a steel part having a composition of, by mass percent, C: 0.10 to 0.35%, Si: 0.15 to 1.0%, Mn: 0.30 to 1.0%, Cr: 0.40 to 2.0%, S: 0.05% or less with the balance being Fe and impurities in a carburizing atmosphere of 900 to 950° C. The carburized steel part is carbonitrided in a carbonitriding atmosphere with the temperature of 800 to 900° C. and the nitrogen potential of 0.2 to 0.6%. The carbonitrided steel part is qhenched and then shot peened. The shot peening treatment may be further performed while heating to a temperature not higher than 350° C. or immediately after heating to a temperature not higher than 350° C. After quenching, the shot peening treatment may be further performed after tempering in the temperature range exceeding 250° C. and not higher than 350° C.

    摘要翻译: 碳氮共渗构件的制造方法,其特征在于,将以质量%计含有C:0.10〜0.35%,Si:0.15〜1.0%,Mn:0.30〜1.0%,Cr:0.40〜2.0 %,S:0.05%以下,余量为渗碳气氛中的Fe和杂质为900〜950℃。渗碳钢部分在碳氮共渗气氛中碳氮共混,温度为800〜900℃,氮势 为0.2〜0.6%。 将碳氮共渗钢部分进行复层,然后喷丸硬化。 可以在加热至不高于350℃的温度或加热至不高于350℃的温度之后进一步进行喷丸硬化处理。淬火后,可以在温度回火之后进一步进行喷丸硬化处理 范围超过250℃,不高于350℃