摘要:
Li2O—Al2O3—SiO2 crystallized glass is provided which has clarity and glass characteristics equivalent to or superior to a conventional crystallized glass, even when the content of As2O3 is decreased. The Li2O—Al2O3—SiO2 crystallized glass contains, by weight, 0.05 to 4% Sb2O3, in which the content of &bgr;-OH is 0.3 to 4/mm.
摘要翻译:提供Li2O-Al2O3-SiO2结晶玻璃,其具有与常规结晶玻璃相当或优于常规结晶玻璃的透明度和玻璃特性,即使As2O3含量降低。 Li 2 O-Al 2 O 3 -SiO 2结晶玻璃含有0.05〜4重量%的Sb 2 O 3,其中β-OH的含量为0.3〜4 / mm。
摘要:
Li2O—Al2O3—SiO2 crystallized glass is provided which has clarity and glass characteristics equivalent to or superior to a conventional crystallized glass, even when the content of As2O3 is decreased. The Li2O—Al2O3—SiO2 crystallized glass consists essentially of, by weight, 60 to 75% SiO2, 17 to 27% Al2O3, 3 to 5% Li2O, 0 to 0.9% MgO, 0 to 0.9% ZnO, 0.3 to 5% BaO, 0 to 3% Na2O, 0 to 3% K2O, 0 to 4% TiO2, 1 to 4% ZrO2, 0 to 4% P2O5, 0.05 to 2% Sb2O3, 0 to 0.9% MgO+ZnO, and 0 to 4% Na2O+K2O.
摘要翻译:提供Li2O-Al2O3-SiO2结晶玻璃,其具有与常规结晶玻璃相当或优于常规结晶玻璃的透明度和玻璃特性,即使As2O3含量降低。 Li 2 O-Al 2 O 3 -SiO 2结晶玻璃基本上由以重量计组成的60至75%的SiO 2,17至27%的Al 2 O 3,3至5%的Li 2 O,0至0.9%的MgO,0至0.9%的ZnO,0.3至5%的BaO ,0〜3%的Na 2 O,0〜3%的K 2 O,0〜4%的TiO 2,1〜4%的ZrO 2,0〜4的P 2 O 5,0.05〜2的Sb 2 O 3,0〜0.9的MgO + ZnO,0〜4质量% Na2O + K2O。
摘要:
A top plate (3) of a low-expansion crystallized glass of deep color, with a first enamel coating coated on a heating portion (5, 7, 9, 11) of the plate and a second enamel coating coated on a non-heating portion (13) around and other than the heating portion. The first enamel coating consists essentially, by weight, of 40 to 98% glass content, 5 to 55% at least one of ZrSiO.sub.4 and ZrO.sub.2 crystals, and 0 to 54% coloring pigment. The second enamel coating consists essentially, by weight, of 30 to 94% glass content, 5 to 69% TiO.sub.2 crystals, 0 to 34% coloring pigment.
摘要:
In order to provide an enamel frit composition capable of preventing a hue of a low-expansion crystallized glass plate of a dark color from being seen through an enamel coating without increasing the thickness of the enamel coating and the mixing ratio of a coloring pigment as well as to provide an enamel-coated low-expansion crystallized glass plate using the above-mentioned composition, the enamel frit composition for a low-expansion crystallized glass essentially consists, by weight, of 30-94 wt % glass powder, 5-69 wt % TiO.sub.2 powder, and 0.05-34 wt % coloring pigment.
摘要:
In an Li2O—Al2O3—SiO2 transparent crystallized glass, &bgr;-quartz solid solution is produced as main crystals, an average coefficient of linear thermal expansion within a range between 30 and 380° C. is −10˜10×10−7/°C., and &bgr;-OH in an amount of 0.28/mm or more is contained. Preferably, the content of each component of Li2O, SiO2, and Al2O3 satisfies, by weight ratio, the relationship given by 0.058≧{Li2O/(SiO2+Al2O3)}≧0.031.
摘要翻译:在Li 2 O-Al 2 O 3 -SiO 2透明结晶玻璃中,生成作为主晶体的β-石英固溶体,在30〜380℃的范围内的平均线性热膨胀系数为-10〜10×10-7 /℃。 ,含有0.28 / mm以上的β-OH。 优选地,Li 2 O,SiO 2和Al 2 O 3的各成分的含量以重量比满足0.058≤{Li 2 O /(SiO 2 + Al 2 O 3)}> = 0.031的关系。
摘要:
A laminated glass (10) has a structure in which seven sheet glasses (20) and six PVB resin layers (30) are laminated alternately. A laminated region from a transparent surface (10a) on one side to 4.0 mm comprises two 0.7 mm-thick glass layers formed of two sheet glasses (20), one 0.8 mm-thick glass layer formed of the portion (20c) of one 1.5 mm-thick sheet glass (20) positioned in the laminated region, and two adhesion layers (30) with thicknesses of 1.3 mm and 0.5 mm. Each of the adhesion layers is interposed between the glass layers and is adhered to the glass layers. The laminated region with a depth of 4.0 mm from a transparent surface (10b) on the other side also has the same laminated structure as that in the above laminated region.
摘要:
A laminated glass for windows has a multilayer structure, wherein plural sheets of glass are laminated through a resin layer. The sheet glasses are made of an alkali-free borosilicate glass. Each sheet glass has a thickness of 1 mm or less, and the total thickness of the sheet glasses is 2 to 10 mm.
摘要:
In a window member (10) to be used as a window of a combustion apparatus, adjusting means is bonded to a substrate (11) made of glass. The adjusting means adjusts an average transmittance of the window member so that the average transmittance at a thickness of 4 mm for an electromagnetic wave having a wavelength of 0.4–0.8 μm falls within a range between 10 and 50%. The adjusting means may comprise a film member (12) bonded to a principal surface (11a) of the substrate.
摘要:
A substrate is made of a crystallized glass having translucency and an average linear thermal expansion coefficient of −5×10−7/° C. at 30 to 500° C. The substrate has a first surface (working surface) of a smooth surface having a surface roughness Rmax of less than 0.5 μm, and a second surface (non-working surface) of a rough surface having a surface roughness Rmax of 4 μm. A light shielding layer consisting of a light shielding film and an antioxidant film is formed on the second surface of the substrate through sputtering.
摘要:
A laminated glass which is constituted of seven glass layers each formed of a 0.7 mm thick glass sheet and resin layers interposed between the glass layers respectively which resin layers are made of polyvinyl butyral (PVB) resin and have each a thickness of 0.5 mm with the total number of the glass layers and the resin layers being 13. Between a glass layer and a resin layer which are adjacent to each other, the thickness ratio of the resin layer to the glass layer (11) (the ratio of the thickness of the resin layer and the thickness of the glass layer) is 0.71. A base material resin constituting the resin layers may be ethylene/vinyl acetate copolymer (EVA) or methacrylic resin (PMA) as well as polyvinyl butyral (PVB) resin.