Method for processing aluminium in a rotary or a reverberating furnace
    1.
    发明授权
    Method for processing aluminium in a rotary or a reverberating furnace 有权
    在旋转或混响炉中加工铝的方法

    公开(公告)号:US07655067B2

    公开(公告)日:2010-02-02

    申请号:US10589935

    申请日:2005-02-07

    IPC分类号: C22B21/00

    摘要: The invention relates to a method for processing aluminum in a furnace consisting in introducing an aluminum-containing material and possibly one or several types of salt into the furnace, melting said material by heating with the aid of at least one burner supplied with a combustive material and fuel in such a way that a molten aluminum possibly covered with a slag containing, in particular alumina and at least one salt is produced and in measuring a carbon monoxide and/or hydrogen concentration in the furnace atmosphere or in a smoke at the exit of the furnace. Oxygen content in the combustive material supplying at least one burner is greater than 10% by volume, preferably greater than 21% by volume. The inventive method also involves a final phase of reduction of the molten aluminum oxydation during which the fuel flow rate is substantially constant while the injected combustive flow rate is controlled at a value ranging from 3 to 15% by volume which is greater than a CO concentration in the furnace and/or in the smoke without control.

    摘要翻译: 本发明涉及一种用于在炉中加工铝的方法,该方法包括将含铝材料和可能的一种或几种盐引入炉中,借助至少一种燃烧器供应燃料来加热熔化所述材料, 和燃料,使得可能产生含有特别是氧化铝和至少一种盐的炉渣的熔融铝,并且测量炉气氛中的烟气中的一氧化碳和/或氢浓度 炉子。 供应至少一个燃烧器的燃烧材料中的氧含量大于10体积%,优选大于21体积%。 本发明的方法还涉及熔融铝氧化降低的最终阶段,在该阶段期间燃料流速基本上恒定,同时将注入的燃烧流量控制在3至15体积%的值,其大于CO浓度 在炉中和/或烟雾中无控制。

    Method for processing aluminium in a rotary or a reverberating furnace
    2.
    发明申请
    Method for processing aluminium in a rotary or a reverberating furnace 有权
    在旋转或混响炉中加工铝的方法

    公开(公告)号:US20070171954A1

    公开(公告)日:2007-07-26

    申请号:US10589935

    申请日:2005-02-07

    IPC分类号: H05B6/22

    摘要: The invention relates to a method for processing aluminum in a furnace consisting in introducing an aluminum-containing material and possibly one or several types of salt into the furnace, melting said material by heating with the aid of at least one burner supplied with a combustive material and fuel in such a way that a molten aluminum possibly covered with a slag containing, in particular alumina and at least one salt is produced and in measuring a carbon monoxide and/or hydrogen concentration in the furnace atmosphere or in a smoke at the exit of the furnace. Oxygen content in the combustive material supplying at least one burner is greater than 10% by volume, preferably greater than 21% by volume. The inventive method also involves a final phase of reduction of the molten aluminum oxydation during which the fuel flow rate is substantially constant while the injected combustive flow rate is controlled at a value ranging from 3 to 15% by volume which is greater than a CO concentration in the furnace and/or in the smoke without control.

    摘要翻译: 本发明涉及一种用于在炉中加工铝的方法,该方法包括将含铝材料和可能的一种或几种盐引入炉中,借助至少一种燃烧器供应燃料来加热熔化所述材料, 和燃料,使得可能产生含有特别是氧化铝和至少一种盐的炉渣的熔融铝,并且测量炉气氛中的烟气中的一氧化碳和/或氢浓度 炉子。 供应至少一个燃烧器的燃烧材料中的氧含量大于10体积%,优选大于21体积%。 本发明的方法还涉及熔融铝氧化降低的最终阶段,在该阶段期间燃料流速基本上恒定,同时注入的燃烧流量控制在3至15体积%的范围内,其大于CO浓度 在炉中和/或烟雾中无控制。