METHOD FOR MANUFACTURING HIGH STRENGTH STEEL PLATE
    1.
    发明申请
    METHOD FOR MANUFACTURING HIGH STRENGTH STEEL PLATE 有权
    制造高强度钢板的方法

    公开(公告)号:US20110168304A1

    公开(公告)日:2011-07-14

    申请号:US13053879

    申请日:2011-03-22

    IPC分类号: C21D8/02

    摘要: A high strength steel plate containing 0.02 to 0.08% C, by mass, and has substantially a two phase microstructure of ferrite and bainite. The ferrite contains precipitates having a particle size of 30 nm or smaller grain size. The steel plate has a yield strength of 448 MPa or higher. A method for manufacturing the high strength steel plate which comprises hot rolling, accelerated cooling and reheating. The accelerated cooling is conducted down to a temperature of 300 to 600° C. at a cooling rate of 5° C./s or higher. The reheating is conducted up to a temperature of 550 to 700° C. at a heating rate of 0.5° C./s or higher.

    摘要翻译: 含有0.02〜0.08%C质量%的高强度钢板,并具有铁素体和贝氏体的两相显微组织。 铁素体含有粒径为30nm以下的析出物。 钢板的屈服强度为448MPa以上。 一种制造高强度钢板的方法,其包括热轧,加速冷却和再加热。 加速冷却以5℃/ s以上的冷却速度进行到300〜600℃的温度。 以0.5℃/ s以上的加热速度将再加热进行到550〜700℃的温度。