Austenitic stainless steel having increased yield ratio and manufacturing method thereof

    公开(公告)号:US12173392B2

    公开(公告)日:2024-12-24

    申请号:US17772324

    申请日:2020-07-08

    Applicant: POSCO

    Abstract: Disclosed is an austenitic stainless steel having an increased yield ratio. The disclosed austenitic stainless steel is characterized by comprising, in percent by weight (wt %), 0.1% or less (exclusive of 0) of C, 0.2% or less (exclusive of 0) of N, 1.5 to 2.5% of Si, 6.0 to 10.0% of Mn, 15.0 to 17.0% of Cr, 0.3% or less (exclusive of 0) of Ni, 2.0 to 3.0% of Cu, and the remainder of Fe and other inevitable impurities, and satisfying Expressions (1) and (2) below. 3.2≤5.53+1.4Ni−0.16Cr+17.1(C+N)+0.722Mn+1.4Cu−5.59Si≤7  Expression (1): 551−462(C+N)−9.2Si−8.1Mn−13.7Cr−29(Ni+Cu)≤110  Expression (2): wherein C, N, Si, Mn, Cr, Ni, and Cu indicate the content (wt %) of respective elements.

    AUSTENITIC STAINLESS STEEL HAVING INCREASED YIELD RATIO AND MANUFACTURING METHOD THEREOF

    公开(公告)号:US20220403491A1

    公开(公告)日:2022-12-22

    申请号:US17772324

    申请日:2020-07-08

    Applicant: POSCO

    Abstract: Disclosed is an austenitic stainless steel having an increased yield ratio. The disclosed austenitic stainless steel is characterized by comprising, in percent by weight (wt %), 0.1% or less (exclusive of 0) of C, 0.2% or less (exclusive of 0) of N, 1.5 to 2.5% of Si, 6.0 to 10.0% of Mn, 15.0 to 17.0% of Cr, 0.3% or less (exclusive of 0) of Ni, 2.0 to 3.0% of Cu, and the remainder of Fe and other inevitable impurities, and satisfying Expressions (1) and (2) below. 3.2≤5.53+1.4Ni−0.16Cr+17.1(C+N)+0.722Mn+1.4Cu−5.59Si≤7  Expression (1): 551-462(C+N)−9.2Si−8.1Mn−13.7Cr−29(Ni+Cu)≤110  Expression (2): wherein C, N, Si, Mn, Cr, Ni, and Cu indicate the content (wt %) of respective elements.

    FERRITIC STAINLESS STEEL HAVING IMPROVED MAGNETIC PROPERTIES AND MANUFACTURING METHOD THEREFOR

    公开(公告)号:US20240401174A1

    公开(公告)日:2024-12-05

    申请号:US18696200

    申请日:2022-10-19

    Applicant: POSCO CO., LTD

    Abstract: Disclosed herein are ferritic stainless steel and a manufacturing method wherein the ferritic stainless steel has magnetic properties improved by controlling alloy components and a manufacturing process in order to increase responsiveness to an externally applied magnetic field. The ferritic stainless steel having improved magnetic properties according to an embodiment of the present invention may comprise, by % by weight, C: 0% (exclusive) to 0.02% (inclusive), N: 0% (exclusive) to 0.02% (inclusive), Si: 0.5% to 2.0% (both inclusive), Mn: 0.1% to 0.3% (both inclusive), Cr: 16.0% to 20.1% (both inclusive), Mo: 1.0% (exclusive) to 2.0% (inclusive), Ti: 0.1% to 0.4% (both inclusive), and the balance of iron (Fe) and inevitable impurities.

    NON-MAGNETIC AUSTENITIC STAINLESS STEEL
    8.
    发明公开

    公开(公告)号:US20230151470A1

    公开(公告)日:2023-05-18

    申请号:US17624969

    申请日:2020-12-30

    Applicant: POSCO

    CPC classification number: C22C38/58 C22C38/44 C22C38/001 C22C38/02 C22C38/42

    Abstract: Provided is a non-magnetic austenitic stainless steel. According to an embodiment of the disclosed non-magnetic austenitic stainless steel, the non-magnetic austenitic stainless steel includes, in percent by weight (wt %), 0.01 to 0.1% of carbon (C), 1.5% or less (excluding 0) of silicon (Si), 0.5 to 3.5% of manganese (Mn), 16 to 22% of chromium (Cr), 7 to 15% of nickel (Ni), 3% or less of molybdenum (Mo), 0.01 to 0.3% of nitrogen (N), and the remainder of iron (Fe) and inevitable impurities, wherein a value of Expression (1) below is a negative value: (1) 3*(Cr+Mo)+5*Si−65*(C+N)−2*(Ni+Mn)−28, wherein in Expression (1), Cr, Mo, Si, C, N, Ni, and Mn denote contents (wt %) of the alloy elements, respectively.

    AUSTENITIC STAINLESS STEEL HAVING IMPROVED STRENGTH, AND METHOD FOR MANUFACTURING SAME

    公开(公告)号:US20220267875A1

    公开(公告)日:2022-08-25

    申请号:US17622474

    申请日:2020-06-10

    Applicant: POSCO

    Abstract: Provided is an austenitic stainless steel having improved strength. This austenitic stainless steel includes, in percent (%) by weight, 0.06 to 0.15% of carbon (C), 0.3% or less (excluding 0) of nitrogen (N), more than 1.0% and equal to or less than 2.0% of silicon (Si), 5.0 to 7.0% of manganese (Mn), 15.0 to 16.0% of chromium (Cr), 0.3% or less (excluding 0) of nickel (Ni), 2.5% or less (excluding 0) of copper (Cu), and the remainder of iron (Fe) and inevitable impurities, and satisfies Expressions (1), (2), and (3) below: 15≤0.2Mn+337C+1.2Cu−1.7Cr+3.3Ni+78N−3.5Si+3.0≤30   Expression (1): 2.3≤[Cr+1.5Si]/[Ni+0.31Mn+22C+1Cu+14.2N]≤3.0   Expression (2): 1.0≤((Cr+1.5Si+18)/(Ni+0.52Cu+30(C+N)+0.5Mn+36)+0.262)*161−161≤7.0   Expression (3): wherein C, N, Si, Mn, Cr, Ni, and Cu refer to contents of the elements, respectively.