公开(公告)号:US20220033941A1
公开(公告)日:2022-02-03
申请号:US17312119
申请日:2019-08-23
Applicant: POSCO
Inventor: Jong Jin Jeon , Mi-Nam Park , Sang Seok Kim
Abstract: A stainless steel with a yield strength of 2,200 MPa or more is disclosed through the generation of the strain-induced martensite phase and the increase of the martensite phase strength. A high strength stainless steel according to an embodiment of present disclosure includes, in percent (%) by weight of the entire composition, C: 0.14 to 0.20%, Si: 0.8 to 1.0%, Mn: more than 0 and 0.5% or less, Cr: 15.0 to 17.0%, Ni: 4.0 to 5.0%, Mo: 0.6 to 0.8%, Cu: 0.5% or less, N: 0.05 to 0.11%, the remainder of iron (Fe) and other inevitable impurities, and C+N: 0.25% or more and Md30 value satisfies 40° C. or more.
-
公开(公告)号:US11952649B2
公开(公告)日:2024-04-09
申请号:US17312119
申请日:2019-08-23
Applicant: POSCO
Inventor: Jong Jin Jeon , Mi-Nam Park , Sang Seok Kim
CPC classification number: C22C38/44 , C21D6/004 , C21D6/005 , C21D6/008 , C21D8/0205 , C21D8/0226 , C21D8/0263 , C21D9/46 , C22C38/001 , C22C38/02 , C22C38/04 , C22C38/42 , C21D2211/001 , C21D2211/005 , C21D2211/008
Abstract: A stainless steel with a yield strength of 2,200 MPa or more is disclosed through the generation of the strain-induced martensite phase and the increase of the martensite phase strength. A high strength stainless steel according to an embodiment of present disclosure includes, in percent (%) by weight of the entire composition, C: 0.14 to 0.20%, Si: 0.8 to 1.0%, Mn: more than 0 and 0.5% or less, Cr: 15.0 to 17.0%, Ni: 4.0 to 5.0%, Mo: 0.6 to 0.8%, Cu: 0.5% or less, N: 0.05 to 0.11%, the remainder of iron (Fe) and other inevitable impurities, and C+N: 0.25% or more and Md30 value satisfies 40° C. or more.
-
公开(公告)号:US20220018006A1
公开(公告)日:2022-01-20
申请号:US17293274
申请日:2019-10-31
Applicant: POSCO
Inventor: Kyung-Hun Kim , Hak Kim , Man Jin Ha , Ji Soo Kim , Jong Jin Jeon
Abstract: Disclosed are austenitic stainless steel that can exhibit high strength while having non-magnetic properties, and a manufacturing method thereof.
The high strength non-magnetic austenitic stainless steel according to an embodiment of present disclosure includes, in percent (%) by weight of the entire composition, C: 0.02 to 0.12%, Si: 1.2% or less, Mn: 0.5 to 2.0%, Cr: 17.0 to 22.0%, Ni: 11.0 to 15.0%, Mo: 3.0% or less, N: 0.25% or less, the remainder of iron (Fe) and other inevitable impurities, satisfies C+N: 0.25% or more, and satisfies following Formulas (1) and (2). [{Cr+Mo+1.5*Si+18}/{Ni+30*(C+N)+0.5*Mn+36}+0.262]*161−161−log(cooling rate)
-
-