公开(公告)号:US4179275A
公开(公告)日:1979-12-18
申请号:US906110
申请日:1978-05-15
申请人: Paul Metz , Robert Schockmel , Roland Mersch
发明人: Paul Metz , Robert Schockmel , Roland Mersch
CPC分类号: C03B7/16 , C03B19/108 , C03B19/1085 , C21B3/06 , C21B3/08 , Y02P40/52 , Y02W30/543
摘要: Molten metallurgical slags are expanded by contact with water in a liquid or vapor state by passing the molten slag along a prefoaming or expanding trough by delivering the slag to this trough via an intermediate trough which is shiftable along the prefoaming trough in order to vary the location at which the slag contacts the prefoaming trough and the expanding-agent film thereon in accordance with physical characteristics of the molten slag, especially its temperature and viscosity. From the pre-expanding or prefoaming trough, the partially expanded slag may be subjected to expansion by conventional means, e.g. a rotating drum which disperses the slag particles through the air so that they can be collected in a completely expanded, dry and solidified state.
摘要翻译: 熔融冶金炉渣通过与液体或蒸汽状态的水接触而膨胀,通过使熔融炉渣沿着预发泡或膨胀槽通过将渣通过沿预发泡槽移动的中间槽输送到该槽来改变位置 渣根据熔渣的物理特性,尤其是其温度和粘度,与预发泡槽及其上的膨胀剂膜接触。 从预膨胀或预发泡槽中,部分膨胀的炉渣可以通过常规方法进行膨胀,例如, 一个旋转的鼓,其将渣粒分散通过空气,使得它们可以以完全膨胀,干燥和固化的状态收集。
-
公开(公告)号:US4352764A
公开(公告)日:1982-10-05
申请号:US162361
申请日:1980-06-24
申请人: Paul Metz , Robert Schockmel , Roland Mersch
发明人: Paul Metz , Robert Schockmel , Roland Mersch
CPC分类号: C03B19/1015 , C03B37/05 , C03B37/055 , C21B3/08
摘要: Slag sand and slag wool are formed by a method wherein molten slag is poured at a temperature above 1300.degree. C. in a thin flowing stream onto a vaned drum rotating at a peripheral speed of at least 25 m/sec. This drum, which may have forwardly directed nozzles for mixing the falling slag stream with a cooling medium such as water, breaks the slag up into droplets and projects these droplets through the air so they cool and form filaments and granules. The granules are collected separately from the filaments so that the installation simultaneously produces slag sand and slag wool.
摘要翻译: 炉渣砂和矿渣棉是通过一种方法形成的,其中将熔渣在1300℃以上的温度下以薄的流动流倒入以至少25m /秒的圆周速度旋转的叶片滚筒上。 该鼓可以具有用于将下落的炉渣流与诸如水的冷却介质混合的前向喷嘴将炉渣向上分散成液滴并将这些液滴突出通过空气,从而冷却并形成细丝和颗粒。 颗粒与细丝分开收集,使得安装同时产生渣砂和矿渣棉。
-
公开(公告)号:US4123247A
公开(公告)日:1978-10-31
申请号:US851636
申请日:1977-11-15
申请人: Paul Metz , Robert Schockmel , Roland Mersch
发明人: Paul Metz , Robert Schockmel , Roland Mersch
CPC分类号: C03B19/1085 , C03B19/108 , C03B7/16 , C21B3/06 , Y02P40/52 , Y02P40/57 , Y02W30/543
摘要: Molten metallurgical slags are expanded by contact with water in a liquid or vapor state by passing the molten slag along a prefoaming or expanding trough by delivering the slag to this trough via an intermediate trough which is shiftable along the prefoaming trough in order to vary the location at which the slag contacts the prefoaming trough and the expanding-agent film thereon in accordance with physical characteristics of the molten slag, especially its temperature and viscosity. From the pre-expanding or prefoaming trough, the partially expanded slag may be subjected to expansion by conventional means, e.g. a rotating drum which disperses the slag particles through the air so that they can be collected in a completely expanded, dry and solidified state.
摘要翻译: 熔融冶金炉渣通过与液体或蒸汽状态的水接触而膨胀,通过使熔融炉渣沿着预发泡或膨胀槽通过将渣通过沿预发泡槽移动的中间槽输送到该槽来改变位置 渣根据熔渣的物理特性,尤其是其温度和粘度,与预发泡槽及其上的膨胀剂膜接触。 从预膨胀或预发泡槽中,部分膨胀的炉渣可以通过常规方法进行膨胀,例如, 一个旋转的鼓,其将渣粒分散通过空气,使得它们可以以完全膨胀,干燥和固化的状态收集。
-
-