公开(公告)号:US20110275505A1
公开(公告)日:2011-11-10
申请号:US13131651
申请日:2009-11-20
IPC分类号: C04B35/528 , C08L61/00
CPC分类号: C04B35/6263 , C01B32/05 , C04B35/6261 , C04B35/62655 , C04B35/62695 , C04B35/63416 , C04B35/63488 , C04B2235/528 , C04B2235/5436 , C04B2235/608 , C04B2235/61 , C04B2235/77 , C10C1/04 , Y10T428/2982
摘要: In a continuous method for production of a semicoke powder with high bulk density and flowability, a sinterable carbon powder (semicoke) is dispersed in water with addition of at least one binder and at least one liquefier, wherein the proportion of carbon in the dispersion is adjusted to at least 50 wt. %, relative to the mass of the dispersion, and the zeta potential of the dispersion is adjusted to less than −50 mV, the dispersion is submitted to homogenisation and stabilisation by continuous wet grinding with a residence time in the mill of less than 3 minutes and the homogeneous dispersion is spray-dried.
摘要翻译: 在生产具有高堆积密度和流动性的半焦粉末的连续方法中,将可烧结碳粉末(半焦)分散在水中,加入至少一种粘合剂和至少一种液化器,其中分散体中碳的比例为 调至至少50wt。 相对于分散体的质量,并且将分散体的ζ电位调节至小于-50mV,通过连续湿式研磨使分散体进行均化和稳定化,在研磨机中的停留时间小于3分钟 将均匀分散体喷雾干燥。
-
公开(公告)号:US08613801B2
公开(公告)日:2013-12-24
申请号:US13131651
申请日:2009-11-20
IPC分类号: C09C1/44
CPC分类号: C04B35/6263 , C01B32/05 , C04B35/6261 , C04B35/62655 , C04B35/62695 , C04B35/63416 , C04B35/63488 , C04B2235/528 , C04B2235/5436 , C04B2235/608 , C04B2235/61 , C04B2235/77 , C10C1/04 , Y10T428/2982
摘要: In a continuous method for production of a semicoke powder with high bulk density and flowability, a sinterable carbon powder (semicoke) is dispersed in water with addition of at least one binder and at least one liquefier, wherein the proportion of carbon in the dispersion is adjusted to at least 50 wt. %, relative to the mass of the dispersion, and the zeta potential of the dispersion is adjusted to less than −50 mV, the dispersion is submitted to homogenization and stabilization by continuous wet grinding with a residence time in the mill of less than 3 minutes and the homogeneous dispersion is spray-dried.
摘要翻译: 在生产具有高堆积密度和流动性的半焦粉末的连续方法中,将可烧结碳粉末(半焦)分散在水中,加入至少一种粘合剂和至少一种液化器,其中分散体中碳的比例为 调至至少50wt。 相对于分散体的质量,并且将分散体的ζ电位调节至小于-50mV,通过连续湿式研磨使分散体在磨机中停留时间小于3分钟进行均化和稳定化 将均匀分散体喷雾干燥。
-