摘要:
Methods of improving the corrosion resistance and hot working productivity of AA7000 series aluminum alloys include, in one mode, the steps of treating a stock material to form a globular microstructure, preferably by a thermal conversion treatment, and subsequently hot working the treated stock material, quenching it and aging it. The globular microstructure permits increasing the hot working rate to attain T6 properties using only a T5 temper practice and without adverse effect on the surface of the hot worked product as a result of the increased hot working rate. Consequently, an acceptable product is made at a significantly lower cost due to the increased hot working rates and fewer processing steps. The method also improves the corrosion resistance, particularly exfoliation corrosion resistance, of the product such that corrosion resistance generally attainable using only a T7 temper practice is achieved using only a T5 temper practice.
摘要:
New 6xxx aluminum alloy bodies and methods of producing the same are disclosed. The new 6xxx aluminum alloy bodies may be produced by preparing the aluminum alloy body for post-solutionizing cold work, cold working by at least 25%, and then thermally treating. The new 6xxx aluminum alloy bodies may realize improved strength and other properties.
摘要:
A method for producing a heat treated aluminum alloy product in a shortened period of time, the method comprising: (a) providing a heat treatable aluminum alloy; (b) working the heat treatable aluminum alloy at a solutionizing temperature to form a product; (c) first stage cooling the product to a critical temperature at which precipitation of second phase particles of the heat treatable aluminum alloy is negligible, wherein the first stage cooling comprises a first stage cooling rate from about 15° F. per second to about 100° F. per second; (d) second stage cooling the product to ambient temperature; (e) heating the product to an artificial aging temperature; and (f) artificially aging the product at the artificial aging temperature for a predetermined artificial aging time to form the heat treated aluminum alloy product.
摘要:
A method of producing aluminum alloy sheet product includes casting a slab, homogenizing the cast slab, and hot rolling the homogenized slab to provide an intermediate gauge product. The temperature and other operating parameters of the hot rolling process are controlled so that the temperature of the intermediate gauge product exiting the hot rolling step is between about 500.degree. F. and 650.degree. F. Preferably, the temperature does not exceed 575.degree. F. The intermediate gauge product is then subjected to a cold reduction of 45% to 70%, annealed, and cold rolled to final gauge. The combination of controlling the hot rolling to provide a desired exit temperature of the intermediate gauge product and annealing prior to cold rolling to final gauge minimizes or eliminates the appearance of ridging or roping line defects in the aluminum sheet product when subjected to further straining in a forming or stamping operation. An improved aluminum alloy sheet product is produced having a superior surface finish for use in automotive components such as hoods or deck lids.
摘要:
New 6xxx aluminum alloy bodies and methods of producing the same are disclosed. The new 6xxx aluminum alloy bodies may be produced by preparing the aluminum alloy body for post-solutionizing cold work, cold working by at least 25%, and then thermally treating. The new 6xxx aluminum alloy bodies may realize improved strength and other properties.
摘要:
New 2xxx aluminum alloy bodies and methods of producing the same are disclosed. The new 2xxx aluminum alloy bodies may be produced by preparing the aluminum alloy body for post-solutionizing cold work, cold working by at least 25%, and then thermally treating. The new 2xxx aluminum alloy bodies may realize improved strength and other properties.
摘要:
New 6xxx aluminum alloy bodies and methods of producing the same are disclosed. The new 6xxx aluminum alloy bodies may be produced by preparing the aluminum alloy body for post-solutionizing cold work, cold working by at least 25%, and then thermally treating. The new 6xxx aluminum alloy bodies may realize improved strength and other properties.
摘要:
Multi-alloy composite sheets and methods of producing the composite sheets for use in automotive applications are disclosed. The automotive application may include an automotive panel having a bi-layer or a tri-layer composite sheet with 3xxx and 6xxx aluminum alloys. The composite sheets may be produced by roll bonding or multi-alloy casting, among other techniques. Each of the composite sheets may demonstrate good flat hem rating and mechanical properties, long shelf life, and high dent resistance, among other properties.
摘要:
New 6xxx aluminum alloy bodies and methods of producing the same are disclosed. The new 6xxx aluminum alloy bodies may be produced by preparing the aluminum alloy body for post-solutionizing cold work, cold working by at least 25%, and then thermally treating. The new 6xxx aluminum alloy bodies may realize improved strength and other properties.
摘要:
New 2xxx aluminum alloy bodies and methods of producing the same are disclosed. The new 2xxx aluminum alloy bodies may be produced by preparing the aluminum alloy body for post-solutionizing cold work, cold working by at least 25%, and then thermally treating. The new 2xxx aluminum alloy bodies may realize improved strength and other properties.