    摘要: The present invention is a golf club (30) having a club head main body (34) with a hollow interior (49), a support layer 41 defining a depth of a recess (38), a polymer insert (40) in the recess (38), an isolation layer (52) and a weight body (50). The polymer insert (40) is composed of a thermosetting polyurethane material having a Shore D hardness in the range of 42 to 55, and a Bayshore rebound in the range of 51 to 60. The preferred thermosetting polyurethane material is formed from a p-phenylene diisocyanate prepolymer and a curing agent. The golf club (30) is preferably a putter, however, it may be a wood or an iron. The particular thermosetting polyurethane provides a soft striking face for feel and a good rebound for distance. The weight body (50) is preferably composed of a tungsten alloy, and the isolation layer (52) is preferably composed of a thermoplastic polyurethane.

    摘要翻译: 本发明是一种具有球杆头主体(34)的高尔夫球杆(30),其具有中空的内部(49),限定凹部(38)的深度的支撑层41,凹部中的聚合物插入件(40) (38),隔离层(52)和重量体(50)。 聚合物插入物(40)由肖氏D硬度在42至55范围内的热固性聚氨酯材料和51至60范围内的贝氏反弹组成。优选的热固性聚氨酯材料由对亚苯基 二异氰酸酯预聚物和固化剂。 高尔夫球杆(30)优选为推杆,但是也可以是木头或铁杆。 特定的热固性聚氨酯提供了柔软的触感面以及远距离的良好反弹。 重量体(50)优选由钨合金构成,隔离层(52)优选由热塑性聚氨酯构成。

    Cross-linked thermoplastic polyurethane/polyurea and method of making same
    10.
    发明授权
    Cross-linked thermoplastic polyurethane/polyurea and method of making same 有权
    交联热塑性聚氨酯/聚脲及其制造方法

    公开(公告)号:US07417094B2

    公开(公告)日:2008-08-26

    申请号:US10992907

    申请日:2004-11-18

    IPC分类号: C08G18/08

    摘要: A cross-linked thermoplastic polyurea is formed by heating a mixture containing a thermoplastic urethane base material, a monomeric and/or polymeric di-isocyanate comprising between 1 to 10% of the total weight of the mixture, and a diamine comprising between 1 to 10% of the total weight of the mixture. A thermoplastic polyurethane may be formed by substituting hydroquinone for the diamine. The mixture is heated to a temperature within the range of 250° F. to 550° F. The heated mixture, which is flowable, is then injected into at least one injection molding device. The mixture is then cured at a temperature between 150° F. to 250° F. for a period of time between 2 and 36 hours. The cross-linked thermoplastic polyurethane/polyurea retains the excellent flowability characteristics of a thermoplastic urethane while the same time exhibits good abrasion, tensile strength, rebound, and compression set characteristics which are similar to those found in thermoset urethanes.

    摘要翻译: 交联的热塑性聚脲通过加热含有热塑性氨基甲酸酯基材料,包含混合物总重量的1至10%的单体和/或聚合二异氰酸酯的混合物和包含1至10个 混合物总重量的百分比。 可以通过用氢醌代替二胺来形成热塑性聚氨酯。 将混合物加热到250°F至550°F范围内的温度。然后将可流动的加热混合物注入至少一个注射成型装置中。 然后将混合物在150°F至250°F的温度下固化2至36小时之间的时间。 交联的热塑性聚氨酯/聚脲保留了热塑性聚氨酯的优异的流动性特征,同时表现出与热固性聚氨酯中发现的相似的良好的耐磨性,拉伸强度,回弹和压缩变形特性。