摘要:
An optical fiber preform manufacturing method includes: supporting a drilling jig in a radial direction of a preform that is cylinder-shaped; moving the drilling jig in a longitudinal direction of the preform; and forming a plurality of slits each extending in the longitudinal direction and each directed from an outer side of the preform toward a center the preform, and a plurality of holes each extending in the longitudinal direction and each connecting with an end of one of the plurality of slits in a depth direction of the one of the plurality of slits.
摘要:
An optical fiber preform manufacturing method includes: supporting a drilling jig in a radial direction of a preform that is cylinder-shaped; moving the drilling jig in a longitudinal direction of the preform; and forming a plurality of slits each extending in the longitudinal direction and each directed from an outer side of the preform toward a center the preform, and a plurality of holes each extending in the longitudinal direction and each connecting with an end of one of the plurality of slits in a depth direction of the one of the plurality of slits.
摘要:
Optical fibers to form an optical transmission line suitable for WDM transmission in a wide-spreading wavelength band, having the following characteristics and parameters: a dispersion in absolute value of 0.5 ps/nm/km to 9 ps/nm/km in a wavelength band of 1430 nm to 1625 nm, a dispersion slope in absolute value of 0.04 ps/nm2/km or less at a wavelength of 1550 nm, a mode field diameter of 7 μm or less at a wavelength of 1550 nm and a cable cutoff wavelength of less than 1430 nm; core 11 surrounded by cladding 7, core 11 being at least two-layered (first layer 1 at the center and second layer 2 surrounding the first layer; relative refractive index of glass layer Δ1 with reference to the cladding being adjusted to not less than 0.6 but not more than 1.6%, relative refractive index of second layer Δ2 with reference to the cladding being adjusted to a negative value.
摘要:
Optical fibers to form an optical transmission line suitable for WDM transmission in a wide-spreading wavelength band, having the following characteristics and parameters: a dispersion in absolute value of 0.5 ps/nm/km to 9 ps/nm/km in a wavelength band of 1430 nm to 1625 nm, a dispersion slope in absolute value of 0.04 ps/nm2/km or less at a wavelength of 1550 nm, a mode field diameter of 7 μm or less at a wavelength of 1550 nm and a cable cutoff wavelength of less than 1430 nm; core 11 surrounded by cladding 7, core 11 being at least two-layered (first layer 1 at the center and second layer 2 surrounding the first layer; relative refractive index of glass layer Δ1 with reference to the cladding being adjusted to not less than 0.6 but not more than 1.6%, relative refractive index of second layer Δ2 with reference to the cladding being adjusted to a negative value.
摘要:
Optical fibers to form an optical transmission line suitable for WDM transmission in a wide-spreading wavelength band, having the following characteristics and parameters: a dispersion in absolute value of 0.5 ps/nm/km to 9 ps/nm/km in a wavelength band of 1430 nm to 1625 nm, a dispersion slope in absolute value of 0.04 ps/nm2/km or less at a wavelength of 1550 nm, a mode field diameter of 7 μm or less at a wavelength of 1550 nm and a cable cutoff wavelength of less than 1430nm; core 11 surrounded by cladding 7, core 11 being at least two-layered (first layer 1 at the center and second layer 2 surrounding the first layer; relative refractive index of glass layer Δ1 with reference to the cladding being adjusted to not less than 0.6 but not more than 1.6%, relative refractive index of second layer Δ2 with reference to the cladding being adjusted to a negative value.
摘要:
The present invention provides an optical fiber of a high nonlinear characteristic which has low dispersion values in a wide wavelength region in the vicinity of a wavelength of 1550 nm. An excellent optical signal processing apparatus is realized by using this optical fiber, such as an optical wavelength converter and a pulse compressor. The optical fiber has characteristics; a dispersion slope at the wavelength of 1550 nm of −0.01 to 0.01 ps/nm2/km, an absolute value of dispersion at the wavelength of 1550 nm of 10 ps/nm/km or less, and a nonlinear constant at the wavelength of 1550 nm of 30×10−10/W or more. A polarization retaining maintaining members are uniquely applied.
摘要:
Disclosed is a nonlinear dispersion-shifted optical fiber, wherein a charomatic dispersion at a wavelength of 1550 nm is equal to a set value required for optical signal processing utilizing a nonlinear phenomenon, a dispersion slope at a wavelength of 1550 nm falls within a range of 0.001 to 0.1 ps/nm2/km, a margin of fluctuation of the charomatic dispersion in a longitudinal direction of the optical fiber at a wavelength of 1550 nm falls within a range of 0.01 to 3 ps/nm/km, and a nonlinear constant n2/Aeff at a wavelength of 1550 nm is not smaller than 15×10−10/W.
摘要:
An inner core has a first refractive index. An outer core having a second refractive index lower than the first refractive index is formed on outer circumference of the inner core. A cladding having a refractive index that is higher than the second refractive index and lower than the first refractive index is formed on outer circumference of the outer core. A diameter of the inner core is enlarged, the second refractive index is decreased, and a center core having a refractive index lower than the first refractive index is formed at a center of the inner core, to increase an effective core area while maintaining wavelength dispersion and bending loss.
摘要:
An inner core has a first refractive index. An outer core having a second refractive index lower than the first refractive index is formed on outer circumference of the inner core. A cladding having a refractive index that is higher than the second refractive index and lower than the first refractive index is formed on outer circumference of the outer core. A diameter of the inner core is enlarged, the second refractive index is decreased, and a center core having a refractive index lower than the first refractive index is formed at a center of the inner core, to increase an effective core area while maintaining wavelength dispersion and bending loss.
摘要:
The present invention provides an optical fiber of a high nonlinear characteristic which has low dispersion values in a wide wavelength region in the vicinity of a wavelength of 1550 nm. An excellent optical signal processing apparatus is realized by using this optical fiber, such as an optical wavelength converter and a pulse compressor. The optical fiber has characteristics; a dispersion slope at the wavelength of 1550 nm of −0.01 to 0.01 ps/nm2/km, an absolute value of dispersion at the wavelength of 1550 nm of 10 ps/nm/km or less, and a nonlinear constant at the wavelength of 1550 nm of 30×10−10/W or more. A polarization retaining maintaining members are uniquely applied.