公开(公告)号:US20180079903A1
公开(公告)日:2018-03-22
申请号:US15561177
申请日:2016-03-25
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Robert Russell Gallucci , Hao Zhou , Edward Venema
CPC classification number: C08L81/02 , C08K7/14 , C08L79/08 , C08L83/10 , C08L2666/20
Abstract: Disclosed herein is a composition comprising a poly(arylene sulfide); a polysiloxane/polyimide block copolymer; glass fiber and an optional platy filler. The polysiloxane/polyimide block copolymer has greater than or equal to 10 weight percent siloxane content, based on the total weight of the polysiloxane/polyimide block copolymer. The composition retains greater than or equal to 60% of the initial viscosity after being retained at 320° C. for 30 minutes and the composition has an OSU peak heat release less than 45 kW/m2 when measured using the method of FAR F25.4 and according to FAR 25.853 (d). Articles comprising the composition are also described.
-
公开(公告)号:US10457808B2
公开(公告)日:2019-10-29
申请号:US15561177
申请日:2016-03-25
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Robert Russell Gallucci , Hao Zhou , Edward Venema
Abstract: Disclosed herein is a composition comprising a poly(arylene sulfide); a polysiloxane/polyimide block copolymer; glass fiber and an optional platy filler. The polysiloxane/polyimide block copolymer has greater than or equal to 10 weight percent siloxane content, based on the total weight of the polysiloxane/polyimide block copolymer. The composition retains greater than or equal to 60% of the initial viscosity after being retained at 320° C. for 30 minutes and the composition has an OSU peak heat release less than 45 kW/m2 when measured using the method of FAR F25.4 and according to FAR 25.853 (d). Articles comprising the composition are also described.
-
公开(公告)号:US11292879B2
公开(公告)日:2022-04-05
申请号:US16469568
申请日:2017-12-21
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Carmen Rocio Misiego Arpa , Edward Venema , Bernabe Quevedo Sanchez , Javier Nieves Remacha , Juan J. Rodriguez Ordonez
IPC: C08G73/10
Abstract: A method of manufacturing an isolated polyetherimide composition includes combining an as-synthesized polyetherimide comprising units of the formula (I) and a melt-stabilizing amount of a tri(C8-30 acyl) glyceride, an anhydride of the formula (II), or a combination comprising at least one of the foregoing, to provide a mixture; and isolating a polyetherimide composition from the mixture to provide the isolated polyetherimide composition having a change in complex viscosity measured over 30 minutes at 390° C., at a shear rate of 6.28 rad/seconds, strain=5%, and under nitrogen, from +15 to −20%, preferably from +10 to −20%, more preferably from +5 to −20%.
-
公开(公告)号:US20180215897A1
公开(公告)日:2018-08-02
申请号:US15747600
申请日:2016-07-28
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Edward Venema , Laura Maria Unica Romero , Carmen Rocío Misiego Arpa , Antonius Leonardus Sacharias , Peter Catsman
CPC classification number: C08K5/11 , C08G73/1003 , C08G73/1071 , C08K5/103 , C08K2201/019 , C08L71/00 , C08L79/08
Abstract: Disclosed herein is a composition comprising a polyetherimide comprising halogen-containing end groups, nitro-containing end groups, or a combination comprising halogen-containing end groups and nitro-containing end groups; and a tri(C8-20 acyl) glyceride. Also disclosed is a method of making the composition.
-
-
-