摘要:
The present invention relates to formulations comprising at least one organic semiconductor and at least one organic solvent, characterized in that the formulation contains less than 10,000 particles per liter formulation having an average size in the range from 0.1 to 20 μm, to their use for the preparation of electronic devices, to methods for preparing electronic devices using the formulations of the present invention, and to electronic devices prepared from such methods and formulations.
摘要:
A light-emitting element includes an anode, a cathode, a hole transporting layer provided between the anode and cathode, a light-emitting layer provided in contact with the hole transporting layer between the anode and cathode, where the surface of the light-emitting layer side of the hole transporting layer is formed in a shape having a part in which the distance with the reference surface along the anode changes in a continuous or step-wise manner, and the surface of the opposite side to the hole transporting layer of the light-emitting layer is formed so as to have the same shape as the surface of the light-emitting layer of the hole transporting layer.
摘要:
An ink for forming a functional layer, which is used when any thin film layer among functional layers consisting of a plurality of thin film layers is formed, includes a functional layer forming material and a solvent for dissolving the functional layer forming material, and in which the number of particles of 0.5 μm or more is 7 or less in 10 ml of the ink for forming a functional layer.
摘要:
An ink for forming a functional layer, which is used when any thin film layer among functional layers consisting of a plurality of thin film layers is formed, includes a functional layer forming material and a solvent for dissolving the functional layer forming material, and in which the number of particles of 0.5 μm or more is 7 or less in 10 ml of the ink for forming a functional layer.
摘要:
An ink for forming a functional layer, which is used when any thin film layer among functional layers consisting of a plurality of thin film layers is formed, includes a functional layer forming material and a solvent for dissolving the functional layer forming material, and in which the number of particles of 0.5 μm or more is 7 or less in 10 ml of the ink for forming a functional layer.
摘要:
An organic EL element manufacturing method includes coating ink which contains a functional layer forming material in a coating region which is configured by a pixel electrode and a partition wall which surrounds a periphery of the pixel electrode, where, in the coating ink, the ink is coated so as to satisfy the following expressions (1) to (3) in a case where a contact angle of the ink with respect to the side surface of the partition wall is set to θbc and a contact angle with respect to a surface of the coating region where the ink is coated is set to θlc. θbc≦θlc (1) θbc≦5° (2) θlc≦20° (3)