1.
公开(公告)号:US10759708B2
公开(公告)日:2020-09-01
申请号:US16289369
申请日:2019-02-28
Inventor: Aimin Yang , Xuekui Mo , Xibin Song
IPC: C04B35/488 , C04B35/26 , C04B35/64 , C04B35/632 , C01G25/02 , C04B35/634 , C04B35/626 , C04B35/486 , C04B35/636 , A61K6/61 , A61K6/818
Abstract: Provided is a high-light transmittance zirconia sintered body, prepared by processing and forming a material for the high-light transmittance zirconia sintered body, and then performing high-temperature sintering in the atmosphere under normal pressure. The material for a high-light transmittance zirconia sintered body is prepared from zirconia powder and α-aluminum oxide as raw materials, wherein the molar percentage of yttrium oxide in the zirconia powder is 4-6%. The high-light transmittance zirconia sintered body can be used for preparing a fixed dental prosthesis. The zirconia sintered body has a grain size of 0.1-0.7 μm, and due to the dispersion and toughening by aluminum oxide, the zirconia sintered body has a higher strength and toughness. Pores in the zirconia powder can be eliminated by adding aluminum oxide. The zirconia sintered body has a higher light transmittance, and the prepared dentures are good in texture, good in jade-like appearance, and closer to the human teeth.
-
公开(公告)号:US10737983B2
公开(公告)日:2020-08-11
申请号:US16329519
申请日:2017-08-03
Inventor: Aimin Yang , Xuekui Mo , Xibin Song
IPC: C04B35/486 , C04B35/626 , C04B35/64
Abstract: A black zirconia sintered body is obtained by processing and forming a powder for the black zirconia sintered body, and then sintering the same at a high temperature and normal pressure in the atmosphere. The powder for the black zirconia sintered body is prepared by a hydrothermal synthesis method using a soluble zirconium salt, a soluble yttrium salt and a color former as raw materials, wherein the molar ratio of the soluble zirconium salt, the soluble yttrium salt and the color former is 90-95:1-5:1-9. The black zirconia sintered body can be used in ceramic processes.
-
公开(公告)号:US20190194076A1
公开(公告)日:2019-06-27
申请号:US16329519
申请日:2017-08-03
Inventor: Aimin Yang , Xuekui Mo , Xibin Song
IPC: C04B35/486 , C04B35/626
CPC classification number: C04B35/486 , C04B35/62645 , C04B35/62675 , C04B35/6268 , C04B35/62695 , C04B35/64 , C04B2235/3217 , C04B2235/3224 , C04B2235/3225 , C04B2235/3232 , C04B2235/3241 , C04B2235/3246 , C04B2235/3262 , C04B2235/3272 , C04B2235/3275 , C04B2235/3279 , C04B2235/3281 , C04B2235/3284 , C04B2235/3418 , C04B2235/443 , C04B2235/5409 , C04B2235/5445 , C04B2235/6022 , C04B2235/61 , C04B2235/658 , C04B2235/77 , C04B2235/96 , C04B2235/9661
Abstract: A black zirconia sintered body is obtained by processing and forming a powder for the black zirconia sintered body, and then sintering the same at a high temperature and normal pressure in the atmosphere. The powder for the black zirconia sintered body is prepared by a hydrothermal synthesis method using a soluble zirconium salt, a soluble yttrium salt and a color former as raw materials, wherein the molar ratio of the soluble zirconium salt, the soluble yttrium salt and the color former is 90-95:1-5:1-9. The black zirconia sintered body can be used in ceramic processes.
-
-