公开(公告)号:US20230212708A1
公开(公告)日:2023-07-06
申请号:US17927975
申请日:2021-05-03
Applicant: SMS group GmbH
Inventor: Frank MASCHLER , Andreas BÖTTCHER , Pierre-Yves HALLEUX
IPC: C21D9/60 , C21D8/12 , C21D1/42 , C21D9/56 , C21D1/76 , C21D6/00 , F27B9/28 , F27D11/06 , F27B9/36 , F27B9/30
CPC classification number: C21D9/60 , C21D8/1272 , C21D1/42 , C21D8/1283 , C21D9/561 , C21D1/76 , C21D6/008 , F27B9/28 , F27D11/06 , F27B9/36 , F27B9/3005
Abstract: A method for the recrystallisation annealing of a non-grain-oriented electric strip (2) in a continuous annealing and coating line (1) is presented. Therein, the electric strip (2) is heated in an induction furnace (5) to a temperature of at least 680° C. at a heating rate of at least 80 K/s and then, in an optional second continuous furnace (8), to a temperature of at least 820° C. at a heating rate of at most 20 K/s. The electric strip (2) is initially heated before the induction furnace (5) via a first continuous furnace (3) to a temperature of at least 300° C. at a heating rate of at most 60 K/s.