POSITIVE ELECTRODE ACTIVE MATERIAL, PREPARATION METHOD THEREOF, AND LITHIUM BATTERY INCLUDING THE SAME
    1.
    发明申请
    POSITIVE ELECTRODE ACTIVE MATERIAL, PREPARATION METHOD THEREOF, AND LITHIUM BATTERY INCLUDING THE SAME 有权
    正极活性物质,其制备方法和包括其的锂电池

    公开(公告)号:US20150111106A1

    公开(公告)日:2015-04-23

    申请号:US14321195

    申请日:2014-07-01

    Abstract: A positive electrode active material including: a lithium complex oxide represented by Formula 1; and a carbon coating layer disposed on the lithium complex oxide, wherein, in a C1s XPS spectrum of the positive electrode active material, a peak intensity of a first peak at a binding energy from about 288 eV to about 293 eV is greater than a peak intensity of a second peak at a binding energy from about 283 eV to about 287 eV, and in an O1s X-ray photoelectron spectrum of the positive electrode active material, a peak intensity of a third peak at a binding energy from about 530.5 eV to about 535 eV is greater than a peak intensity of a fourth peak at a binding energy from about 527.5 electron volts to about 530 electron volts, LiaMbM′cM″dOe.  Formula 1

    Abstract translation: 1.一种正极活性物质,其包含:式1表示的锂复合氧化物; 以及设置在所述锂复合氧化物上的碳涂层,其中在所述正极活性物质的C1s XPS光谱中,约288eV至约293eV的结合能的第一峰的峰强度大于峰值 在约283eV至约287eV的结合能量处的第二峰的强度,以及在正极活性物质的O1s X射线光电子光谱中,在约530.5eV的结合能下的第三峰的峰强度为约530.5eV至 约535eV大于在约527.5电子伏特至约530电子伏特,LiaMbM'cM“dee的结合能力处的第四峰的峰值强度。 公式1

Patent Agency Ranking