Process for activation of catalysts with a nitrogenous compound and excess thionic compound the catalysts that is obtained and it use in hydroconversion
    2.
    发明授权
    Process for activation of catalysts with a nitrogenous compound and excess thionic compound the catalysts that is obtained and it use in hydroconversion 有权
    用含氮化合物和过量的硫辛酸化合物活化催化剂的方法,所得催化剂及其在加氢转化中的应用

    公开(公告)号:US06187708B1

    公开(公告)日:2001-02-13

    申请号:US09305285

    申请日:1999-05-05

    IPC分类号: B01J3720

    CPC分类号: B01J37/20 C10G47/12

    摘要: The invention relates to a process for the sulfurization of hydroconversion catalysts, whereby said catalyst contains at least one element of group VIII of the periodic table and optionally an element of group VI, whereby said metal is present in the oxide state. Said process comprises at least one stage that is carried out in a hydrotreatment zone in the presence of at least one thionic compound and at least one nitrogenous compound. This process is carried out in such a way that before the final sulfurization temperature is reached, at least 130% of the stoichiometric amount of sulfur that is necessary for complete sulfurization of the catalyst is injected in said catalyst.

    摘要翻译: 本发明涉及一种加氢转化催化剂硫化方法,其中所述催化剂含有至少一种元素周期表第Ⅷ族元素和任选的第Ⅵ族元素,其中所述金属以氧化态存在。 所述方法包括在至少一种硫辛酸化合物和至少一种含氮化合物的存在下在加氢处理区中进行的至少一个阶段。 该方法是在达到最终硫化温度之前进行的,在催化剂中注入催化剂完全硫化所需的化学计量量的至少130%的硫。

    Process for the hydrogenation of aromatic compounds comprising chlorine
injection, using catalysts based on a noble metal
    4.
    发明授权
    Process for the hydrogenation of aromatic compounds comprising chlorine injection, using catalysts based on a noble metal 失效
    使用基于贵金属的催化剂对包含氯注入的芳族化合物进行氢化的方法

    公开(公告)号:US5986154A

    公开(公告)日:1999-11-16

    申请号:US105002

    申请日:1998-06-26

    CPC分类号: C10G45/52

    摘要: The invention concerns a process for the hydrogenation of aromatic compounds contained in feeds with an initial boiling point of more than 100.degree. C. and which contain at least 10% by weight of aromatic compounds. It consists of introducing chlorine in a concentration of 0.5-500 ppm by weight with respect to the feed at a temperature of between 200.degree. C. and 450.degree. C., a pressure in the range 1 MPa to 25 MPa, an HSV of between 0.1 h.sup.-1 and 10 h.sup.-1 and a volume ratio of hydrogen to feed of 100-2000. The catalyst used is a noble metal type and contains less than 1% of at least one halogen. Preferably, the catalyst is fluorinated or chlorinated.

    摘要翻译: 本发明涉及一种氢化初始沸点高于100℃并含有至少10重量%芳族化合物的饲料中的芳族化合物的方法。 它包括在200至450℃之间的温度下引入浓度为0.5-500ppm重量的氯,压力在1MPa至25MPa的范围内,HSV介于 0.1h-1和10h-1,氢与进料的体积比为100-2000。 所使用的催化剂是贵金属型,并含有少于1%的至少一种卤素。 优选地,催化剂是氟化的或氯化的。

    Process for activation of a catalyst in the presence of thionic and nitrogenous compounds
    6.
    发明授权
    Process for activation of a catalyst in the presence of thionic and nitrogenous compounds 有权
    在存在硫酸和含氮化合物的情况下活化催化剂的方法

    公开(公告)号:US06329314B1

    公开(公告)日:2001-12-11

    申请号:US09305287

    申请日:1999-05-05

    IPC分类号: B01J27049

    摘要: A process for activation of a hydroconversion catalyst, whereby said catalyst contains at least one metal or element of group VIII, at least one acid element and optionally at least one metal or element of group VI according to which a light petroleum fraction, at least one thionic compound and at least one nitrogenous compound are injected in said catalyst. This process is carried out such that the QS sulfur amount that is injected before the temperature of the catalyst reaches 250° C. is at least equal to half the QSO sulfur amount that is necessary for complete sulfurization of the catalyst.

    摘要翻译: 一种用于活化加氢转化催化剂的方法,其中所述催化剂含有至少一种第VIII族金属或元素,至少一种酸元素和任选的至少一种第VI族金属或元素,根据该催化剂,轻质石油馏分,至少一种 将硫辛酸化合物和至少一种含氮化合物注入所述催化剂中。 进行该过程,使得在催化剂的温度达到250℃之前注入的QS硫量至少等于催化剂完全硫化所需的QSO硫量的一半。