Starting pitch for carbon fibers
    1.
    发明授权
    Starting pitch for carbon fibers 失效
    碳纤维起始间距

    公开(公告)号:US4579645A

    公开(公告)日:1986-04-01

    申请号:US484155

    申请日:1983-04-12

    摘要: Provided is a starting pitch for producing carbon fiber by heat-treating the starting pitch to obtain a precursor pitch, melt-spinning the precursor pitch, then rendering the resultant pitch fiber infusible, followed by carbonization, and further followed by graphitization if required, the starting pitch comprising a mixture of (a) 100 parts by weight of a pitch and (b) 5 to 500 parts by weight of a methanol-insoluble and benzene-soluble component contained in a heavy oil obtained in a fluid catalytic cracking of petroleum, the heavy oil having a boiling range not lower than 200.degree. C.