Elliptically polarizing plate, liquid crystal panel, liquid crystal display device, and image display device
    1.
    发明申请
    Elliptically polarizing plate, liquid crystal panel, liquid crystal display device, and image display device 审中-公开
    椭圆偏光板,液晶面板,液晶显示装置和图像显示装置

    公开(公告)号:US20070020407A1

    公开(公告)日:2007-01-25

    申请号:US11455107

    申请日:2006-06-19

    IPC分类号: C09K19/00

    摘要: An elliptically polarizing plate comprising a retardation film having a film comprising a polymer which has, as its main chain, a polyol skeleton having a side chain substituted with at least one chemical group selected from the group consisting of an aromatic carbonyl group, an aryl-substituted lower alkylcarbonyl group, and an unsaturated aliphatic carbonyl group, the chemical group being bonded to an oxygen atom in the polyol skeleton side chain, and a polarizer stacked over the retardation film, wherein the polarizer is made of a coating film obtained by applying a dichromatic colorant. As the dichromatic colorant, an organic colorant represented by (chromogen)(SO3M)n wherein M represents a cation is used. The elliptically polarizing plate has a good visibility in the range of visible rays and can be made thin and light.

    摘要翻译: 一种椭圆偏振片,包括具有膜的延迟膜,所述延迟膜包含聚合物,所述聚合物以其主链作为被具有至少一个选自芳族羰基,芳基羰基, 取代的低级烷基羰基和不饱和脂肪族羰基,所述化学基团与所述多元醇骨架侧链中的氧原子键合,以及叠层在所述延迟膜上的偏振片,其中所述偏振片由涂布膜 二色染料。 作为二色性着色剂,使用由(着色剂)(SO 3 M)N N表示的有机着色剂,其中M表示阳离子。 椭圆偏振板在可见光范围内具有良好的可视性,并且可以变得薄而轻。

    Retardation film, use of said retardation film, and novel modified polymer
    2.
    发明授权
    Retardation film, use of said retardation film, and novel modified polymer 有权
    延迟膜,使用所述延迟膜和新型改性聚合物

    公开(公告)号:US07722935B2

    公开(公告)日:2010-05-25

    申请号:US11579921

    申请日:2005-06-14

    IPC分类号: G02F1/13363

    摘要: A modified polymer which can serve as a raw material of novel reverse dispersion retardation films is provided, the modified polymer having no need to select a plurality of monomers or polymers in order to realize a reverse dispersion and having no problems concerning glass transition temperature or the like in drawing treatment. A polymer having a polyol skeleton as its main chain is caused to react with a compound for modification such as an aromatic carboxylic acid hydride. Through this reaction, a modified polymer in which a chemical group such as an aromatic carbonyl group is bonded to an oxygen atom in a side chain of the polyol skeleton is prepared. For example, polyvinyl alcohols and benzoyl chloride can be used as the polymer and the compound for modification, respectively. The chemical group may be a benzoyl group. When this modified polymer is formed into a film and then subjected to drawing treatment, a retardation film which exhibits a reverse wavelength dispersion characteristic can be obtained.

    摘要翻译: 可以提供可用作新型反分散延迟膜的原料的改性聚合物,为了实现反向分散而不需要选择多种单体或聚合物,改性聚合物不需要玻璃化转变温度或 像画画处理。 使以多元醇骨架为主链的聚合物与芳香族羧酸氢化物等改性化合物反应。 通过该反应,制备其中诸如芳族羰基的化学基团与多元醇骨架的侧链中的氧原子结合的改性聚合物。 例如,聚乙烯醇和苯甲酰氯可以分别用作聚合物和用于改性的化合物。 化学基团可以是苯甲酰基。 当将该改性聚合物形成膜然后进行拉伸处理时,可以获得呈现反向波长色散特性的延迟膜。

    Retardation Film, Use of Said Retardation Film, and Novel Modified Polymer
    3.
    发明申请
    Retardation Film, Use of Said Retardation Film, and Novel Modified Polymer 有权
    延迟膜,所述延迟膜的用途和新型改性聚合物

    公开(公告)号:US20070243340A1

    公开(公告)日:2007-10-18

    申请号:US11579921

    申请日:2005-06-14

    IPC分类号: C09K19/00 G02F1/1335

    摘要: A modified polymer which can serve as a raw material of novel reverse dispersion retardation films is provided, the modified polymer having no need to select a plurality of monomers or polymers in order to realize a reverse dispersion and having no problems concerning glass transition temperature or the like in drawing treatment. A polymer having a polyol skeleton as its main chain is caused to react with a compound for modification such as an aromatic carboxylic acid hydride. Through this reaction, a modified polymer in which a chemical group such as an aromatic carbonyl group is bonded to an oxygen atom in a side chain of the polyol skeleton is prepared. For example, polyvinyl alcohols and benzoyl chloride can be used as the polymer and the compound for modification, respectively. The chemical group may be a benzoyl group. When this modified polymer is formed into a film and then subjected to drawing treatment, a retardation film which exhibits a reverse wavelength dispersion characteristic can be obtained.

    摘要翻译: 可以提供可用作新型反分散延迟膜的原料的改性聚合物,为了实现反向分散而不需要选择多种单体或聚合物,改性聚合物不需要玻璃化转变温度或 像画画处理。 使以多元醇骨架为主链的聚合物与芳香族羧酸氢化物等改性化合物反应。 通过该反应,制备其中诸如芳族羰基的化学基团与多元醇骨架的侧链中的氧原子结合的改性聚合物。 例如,聚乙烯醇和苯甲酰氯可以分别用作聚合物和用于改性的化合物。 化学基团可以是苯甲酰基。 当将该改性聚合物形成膜然后进行拉伸处理时,可以获得呈现反向波长色散特性的延迟膜。

    LIQUID CRYSTAL PANEL, LIQUID CRYSTAL DISPLAY APPARATUS USING THE PANEL, AND METHOD OF PRODUCING A LIQUID CRYSTAL PANEL
    4.
    发明申请
    LIQUID CRYSTAL PANEL, LIQUID CRYSTAL DISPLAY APPARATUS USING THE PANEL, AND METHOD OF PRODUCING A LIQUID CRYSTAL PANEL 审中-公开
    液晶板,使用面板的液晶显示装置,以及液晶面板的制造方法

    公开(公告)号:US20100134737A1

    公开(公告)日:2010-06-03

    申请号:US12067467

    申请日:2007-01-26

    IPC分类号: G02F1/13363 H01J9/20

    摘要: Provided are a liquid crystal panel and a liquid crystal display apparatus each of which: contributes to a reduction in thickness; and is excellent in optical characteristics, and a method of producing the liquid crystal panel with extremely high production efficiency. A liquid crystal panel of the present invention has a first polarizer, a first protective layer, a first optical compensation layer, a first negative C plate, a liquid crystal cell, a second negative C plate, a second optical compensation layer, a second protective layer, and a second polarizer in the stated order. The first optical compensation layer is arranged between the first protective layer and the first negative C plate to be in close contact with the first protective layer without using any adhesive. The second optical compensation layer is arranged between the second negative C plate and the second protective layer to be in close contact with the second protective layer without using any adhesive. The first and second optical compensation layers are each a coating layer functioning as a λ/4 plate, and each have a thickness of 0.3 to 3 μm. The first and second negative C plates are each a coating layer, and each have a thickness of 0.5 to 10 μm.

    摘要翻译: 本发明提供一种液晶显示装置和液晶显示装置,它们均有助于减小厚度; 光学特性优异,生产效率极高的液晶面板的制造方法。 本发明的液晶面板具有第一偏振片,第一保护层,第一光学补偿层,第一负C板,液晶单元,第二负C板,第二光学补偿层,第二保护层 层和第二偏振器。 第一光学补偿层布置在第一保护层和第一负C板之间,以不使用任何粘合剂与第一保护层紧密接触。 第二光学补偿层布置在第二负C板和第二保护层之间,以与第二保护层紧密接触,而不使用任何粘合剂。 第一和第二光学补偿层各自是用作λ/ 4板的涂层,并且各自具有0.3至3μm的厚度。 第一和第二负C板各自是涂层,并且各自具有0.5至10μm的厚度。

    METHOD FOR PRODUCING OPTICAL FILM
    5.
    发明申请
    METHOD FOR PRODUCING OPTICAL FILM 审中-公开
    生产光膜的方法

    公开(公告)号:US20090017203A1

    公开(公告)日:2009-01-15

    申请号:US11814744

    申请日:2006-01-24

    IPC分类号: B05D3/12 B05D5/00

    摘要: This invention provides a method for producing an optical film, the method comprising a rubbing treatment step of rubbing the surface of a lengthy plastic film F with a rubbing roll 4 obtained by winding a raised fabric 4a, an application step of applying a liquid crystalline molecule to the surface of the plastic film processed through said rubbing treatment step and a fixing step of fixing said applied liquid crystalline molecule. In the rubbing treatment step, the lengthy plastic film is supported and conveyed by a conveyer belt 3 having a metal surface, and plural backup rolls 5 which support the underside of the conveyer belt supporting the plastic film are disposed opposite to said rubbing roll, to set a rubbing strength RS defined by the following equation (1) to 2600 mm or more (more preferably 3400 mm or more).

    摘要翻译: 本发明提供一种光学薄膜的制造方法,其特征在于,该方法包括:摩擦处理步骤,其通过卷绕凸起的织物4a而获得的摩擦辊4摩擦长的塑料薄膜F的表面;施加液晶分子 通过所述摩擦处理步骤处理的塑料膜的表面和固定所施加的液晶分子的定影步骤。 在摩擦处理步骤中,通过具有金属表面的输送带3支撑并输送长时间的塑料膜,并且支撑支撑塑料膜的输送带的下侧的多个支承辊5设置在与所述摩擦辊相对的位置, 将由下式(1)定义的摩擦强度RS设定为2600mm以上(更优选为3400mm以上)。

    Method of producing elliptically polarizing plate and image display using the elliptically polarizing plate
    6.
    发明申请
    Method of producing elliptically polarizing plate and image display using the elliptically polarizing plate 审中-公开
    使用椭圆偏光板制造椭圆偏光板的方法和图像显示

    公开(公告)号:US20070139773A1

    公开(公告)日:2007-06-21

    申请号:US11655249

    申请日:2007-01-19

    IPC分类号: G02B5/30 G02B27/28

    CPC分类号: G02B5/3016

    摘要: The present invention provides: a method of producing a broadband and wide viewing angle elliptically polarizing plate having excellent characteristics in an oblique direction as well; and an image display using the elliptically polarizing plate obtained through the method. The method of producing an elliptically polarizing plate according to the present invention includes the steps of: subjecting a surface of a transparent protective film to alignment treatment; forming a first birefringent layer by applying a liquid crystal composition onto the surface of the transparent protective film subjected to the alignment treatment; laminating a polarizer on a surface of the transparent protective film opposite to the surface subjected to the alignment treatment; and forming a second birefringent layer by laminating a polymer film on a surface of the first birefringent layer, in which the elliptically polarizing plate has a relationship represented by the following expression (1) 2α+40°

    摘要翻译: 本发明提供一种在倾斜方向上具有优异特性的宽带宽视角椭圆偏光板的制造方法。 以及使用通过该方法获得的椭圆偏光板的图像显示。 根据本发明的椭圆偏光板的制造方法包括以下步骤:对透明保护膜的表面进行取向处理; 通过将液晶组合物施加到经过取向处理的透明保护膜的表面上来形成第一双折射层; 在与所述取向处理的表面相对的所述透明保护膜的表面上层叠偏振片; 并且通过在第一双折射层的表面上层叠聚合物膜来形成第二双折射层,其中椭圆偏振片具有由以下表达式(1)表示的关系<?in-line-formula description =“In-line 公式“end =”lead“?> 2alpha + 40° )中,α表示偏振片的吸收轴与透明保护膜的取向方向之间的角度,β表示偏振片的吸收轴与第二双折射层的慢轴之间的角度。

    METHOD OF PRODUCING A LIQUID CRYSTAL PANEL, LIQUID CRYSTAL PANEL, AND IMAGE DISPLAY APPARATUS
    7.
    发明申请
    METHOD OF PRODUCING A LIQUID CRYSTAL PANEL, LIQUID CRYSTAL PANEL, AND IMAGE DISPLAY APPARATUS 审中-公开
    液晶板,液晶板和图像显示装置的制造方法

    公开(公告)号:US20090040443A1

    公开(公告)日:2009-02-12

    申请号:US11573594

    申请日:2006-08-02

    IPC分类号: G02F1/13363

    摘要: To provide a method of producing a liquid crystal panel capable of easily realizing stable high contrast of the liquid crystal panel to be obtained at low cost, a liquid crystal panel, and an image display apparatus. There is provided a method of producing a liquid crystal panel including a first optical compensation layer having refractive index profile of nx>ny=nz and a polarizer on each side of a liquid crystal cell in the order given, in which an angle formed between an absorption axis of the polarizer (A) and a slow axis of the first optical compensation layer (B) on one side of the liquid crystal cell is +α°, an angle formed between an absorption axis of the polarizer (A′) and a slow axis of the first compensation layer (B′) on another side of the liquid crystal cell is −α°, and 0

    摘要翻译: 为了提供一种能够容易地实现低成本获得的液晶面板的稳定的高对比度的液晶面板的制造方法,液晶面板和图像显示装置。 提供了一种制造液晶面板的方法,该液晶面板包括具有nx> ny = nz的折射率分布的第一光学补偿层和液晶单元的每一侧上的偏振器,其中形成在 偏振器(A)的吸收轴和液晶单元一侧的第一光学补偿层(B)的慢轴为+α°,在偏振器(A')的吸收轴和 在液晶单元的另一侧的第一补偿层(B')的慢轴为α°,0 <α<90,该方法包括使由单一原始片形成的衬底经受+α °和相对于基底的纵向方向以α°的取向处理; 以及在经受+α°取向处理的表面上形成第一光学补偿层(B)并在经受α°取向处理的表面上形成第一光学补偿层(B')的步骤。

    Method of producing elliptically polarizing plate and image display apparatus using the elliptically polarizing plate
    8.
    发明申请
    Method of producing elliptically polarizing plate and image display apparatus using the elliptically polarizing plate 审中-公开
    椭圆偏光板的制造方法以及使用该椭圆偏光板的图像显示装置

    公开(公告)号:US20090040434A1

    公开(公告)日:2009-02-12

    申请号:US10581724

    申请日:2005-12-08

    IPC分类号: G02F1/13363 B29D11/00

    摘要: To provide a method of producing a broadband and wide viewing angle elliptically polarizing plate having excellent properties in an oblique direction, the elliptically polarizing plate, and an image display apparatus.The method of producing an elliptically polarizing plate of the present invention includes the steps of: forming a first birefringent layer on a surface of a transparent protective film; laminating a polarizer on a surface of the transparent protective film; and forming a second birefringent layer on a surface of the first birefringent layer, in which: the first birefringent layer and the polarizer are arranged on opposite sides of the transparent protective film; the step of forming a first birefringent layer includes the steps of: applying a liquid crystal material to an alignment substrate; forming a first birefringent layer on the substrate from the liquid crystal material; and transferring the first birefringent layer to a surface of the transparent protective film; and angles α and β satisfy a predetermined relationship (where, α represents an angle formed between a slow axis of the polarizer and a slow axis of the first birefringent layer, and β represents an angle formed between the absorption axis of the polarizer and a slow axis of the second birefringent layer).

    摘要翻译: 提供一种在倾斜方向上具有优异特性的宽视角和宽视角椭圆偏振板的制造方法,椭圆偏光板和图像显示装置。 本发明的椭圆偏光板的制造方法包括以下步骤:在透明保护膜的表面上形成第一双折射层; 在透明保护膜的表面上层叠偏振片; 以及在所述第一双折射层的表面上形成第二双折射层,其中:所述第一双折射层和所述偏振片布置在所述透明保护膜的相对侧上; 形成第一双折射层的步骤包括以下步骤:将液晶材料施加到取向基板; 从液晶材料在基板上形成第一双折射层; 并将所述第一双折射层转印到所述透明保护膜的表面上; 角度α和β满足预定的关系(其中,α表示在偏振片的慢轴与第一双折射层的慢轴之间形成的角度,β表示在偏振片的吸收轴之间形成的角度, 第二双折射层的轴)。

    Method of producing elliptically polarizing plate and image display using the elliptically polarizing plate
    9.
    发明申请
    Method of producing elliptically polarizing plate and image display using the elliptically polarizing plate 审中-公开
    使用椭圆偏光板制造椭圆偏光板的方法和图像显示

    公开(公告)号:US20060001799A1

    公开(公告)日:2006-01-05

    申请号:US11169964

    申请日:2005-06-30

    IPC分类号: G02F1/1335

    CPC分类号: G02B5/3016

    摘要: The present invention provides: a method of producing a broadband and wide viewing angle elliptically polarizing plate having excellent characteristics in an oblique direction as well; and an image display using the elliptically polarizing plate obtained through the method. The method of producing an elliptically polarizing plate according to the present invention includes the steps of: subjecting a surface of a transparent protective film to alignment treatment; forming a first birefringent layer by applying a liquid crystal composition onto the surface of the transparent protective film subjected to the alignment treatment; laminating a polarizer on a surface of the transparent protective film opposite to the surface subjected to the alignment treatment; and forming a second birefringent layer by laminating a polymer film on a surface of the first birefringent layer, in which the elliptically polarizing plate has a relationship represented by the following expression (1) 2α+40°

    摘要翻译: 本发明提供一种在倾斜方向上具有优异特性的宽带宽视角椭圆偏光板的制造方法。 以及使用通过该方法获得的椭圆偏光板的图像显示。 根据本发明的椭圆偏光板的制造方法包括以下步骤:对透明保护膜的表面进行取向处理; 通过将液晶组合物施加到经过取向处理的透明保护膜的表面上来形成第一双折射层; 在与所述取向处理的表面相对的所述透明保护膜的表面上层叠偏振片; 并且通过在第一双折射层的表面上层叠聚合物膜来形成第二双折射层,其中椭圆偏振片具有由以下表达式(1)表示的关系<?in-line-formula description =“In-line 公式“end =”lead“?> 2alpha + 40° )中,α表示偏振片的吸收轴与透明保护膜的取向方向之间的角度,β表示偏振片的吸收轴与第二双折射层的慢轴之间的角度。

    LIQUID CRYSTAL PANEL AND LIQUID CRYSTAL DISPLAY APPARATUS USING THE PANEL
    10.
    发明申请
    LIQUID CRYSTAL PANEL AND LIQUID CRYSTAL DISPLAY APPARATUS USING THE PANEL 审中-公开
    液晶面板和液晶显示装置使用面板

    公开(公告)号:US20100225854A1

    公开(公告)日:2010-09-09

    申请号:US12279865

    申请日:2007-01-26

    IPC分类号: G02F1/1335

    摘要: Provided are a liquid crystal panel which contributes to reduction in thickness and is excellent in optical properties and a liquid crystal display apparatus. The liquid crystal panel of the present invention includes a liquid crystal cell, a first polarizer disposed on one side of the liquid crystal cell, a second polarizer disposed on another side of the liquid crystal cell, a first optical compensation layer and a first negative C plate disposed between the first polarizer and the liquid crystal cell, and a second negative C plate and a second optical compensation layer disposed between the liquid crystal cell and the second polarizer, in which the first optical compensation layer is disposed between the first polarizer and the first negative C plate, the second optical compensation layer is disposed between the second negative C plate and the second polarizer, the first and second optical compensation layers each include a coating layer functioning as a λ/4 plate, and each have a thickness of 0.3 to 3 μm, and the first and second negative C plates each include a coating layer, and each have a thickness of 0.5 to 10 μm.

    摘要翻译: 提供有助于减小厚度并且具有优异的光学性质的液晶面板和液晶显示装置。 本发明的液晶面板包括液晶单元,配置在液晶单元的一侧的第一偏振器,配置在液晶单元的另一侧的第二偏振片,第一光学补偿层和第一负极C 设置在第一偏振器和液晶单元之间的板,以及设置在液晶单元和第二偏振器之间的第二负C板和第二光学补偿层,其中第一光学补偿层设置在第一偏振器和第二偏振器之间 第一负C板,第二光学补偿层设置在第二负C板和第二偏光板之间,第一和第二光学补偿层各自包括用作λ/ 4板的涂层,并且各自具有0.3的厚度 至3μm,并且第一和第二负C板各自包括涂层,并且各自具有0.5至10μm的厚度。