公开(公告)号:US07799167B2
公开(公告)日:2010-09-21
申请号:US11447119
申请日:2006-06-06
申请人: Shinji Suzuki , Yukio Hayashi , Noriyasu Ike , Hiromu Matsumoto , Eri Tamura , Yasunori Endo , Jun Morisawa , Maya Sasaki , Kenji Taniguchi
发明人: Shinji Suzuki , Yukio Hayashi , Noriyasu Ike , Hiromu Matsumoto , Eri Tamura , Yasunori Endo , Jun Morisawa , Maya Sasaki , Kenji Taniguchi
CPC分类号: B31F1/07 , B31F1/122 , B31F1/36 , B31F2201/0756 , B31F2201/0761 , B31F2201/0784 , Y10T156/1023 , Y10T156/1039 , Y10T428/1303 , Y10T428/24455 , Y10T428/24463 , Y10T428/24479 , Y10T428/24612 , Y10T428/24628 , Y10T428/27
摘要: An object of the present invention is to provide an embossed crepe paper which can clearly be formed into fine embossed shapes, and is excellent in the fluffy feel and therefore excellent in such as absorbency for fats. As a means of achieving this object, the method for manufacturing an embossed crepe paper, according to the present invention, is a method for manufacturing an embossed crepe paper comprising a step of embossing a raw crepe paper, wherein: a raw paper having a basis weight of 6 to 28 g/m2 is used as the raw crepe paper; and the embossing step includes the steps of: (a) supplying the raw crepe paper with water in an amount of 0.1 to 100 weight % based on the basis weight to thereby put the raw crepe paper in a wet condition; (b) embossing the wet-conditioned raw crepe paper; and (c) drying the embossed wet-conditioned raw crepe paper.
摘要翻译: 本发明的目的是提供一种压花皱纹纸,其可以明显地形成为细小的浮雕形状,并且蓬松感觉优异,因此对于脂肪的吸收性优异。 作为实现该目的的手段,根据本发明的压纹皱纹纸的制造方法是一种压纹皱纹纸的制造方法,其特征在于,包括对原料绉纸进行压花的工序,其中, 重量为6〜28g / m2用作生绉纸; 并且压花步骤包括以下步骤:(a)以原料重量为基准,以0.1至100重量%的量向原料起皱纸供应水,从而使生皱纹纸处于潮湿状态; (b)将湿绉原料绉纹纸压花; 和(c)干燥压花的湿条纹生绉纸。
-
公开(公告)号:US20060278357A1
公开(公告)日:2006-12-14
申请号:US11447119
申请日:2006-06-06
申请人: Shinji Suzuki , Yukio Hayashi , Noriyasu Ike , Hiromu Matsumoto , Eri Tamura , Yasunori Endo , Jun Morisawa , Maya Sasaki , Kenji Taniguchi
发明人: Shinji Suzuki , Yukio Hayashi , Noriyasu Ike , Hiromu Matsumoto , Eri Tamura , Yasunori Endo , Jun Morisawa , Maya Sasaki , Kenji Taniguchi
CPC分类号: B31F1/07 , B31F1/122 , B31F1/36 , B31F2201/0756 , B31F2201/0761 , B31F2201/0784 , Y10T156/1023 , Y10T156/1039 , Y10T428/1303 , Y10T428/24455 , Y10T428/24463 , Y10T428/24479 , Y10T428/24612 , Y10T428/24628 , Y10T428/27
摘要: An object of the present invention is to provide an embossed crepe paper which can clearly be formed into fine embossed shapes, and is excellent in the fluffy feel and therefore excellent in such as absorbency for fats. As a means of achieving this object, the method for manufacturing an embossed crepe paper, according to the present invention, is a method for manufacturing an embossed crepe paper comprising a step of embossing a raw crepe paper, wherein: a raw paper having a basis weight of 6 to 28 g/m2 is used as the raw crepe paper; and the embossing step includes the steps of: (a) supplying the raw crepe paper with water in an amount of 0.1 to 100 weight % based on the basis weight to thereby put the raw crepe paper in a wet condition; (b) embossing the wet-conditioned raw crepe paper; and (c) drying the embossed wet-conditioned raw crepe paper.
摘要翻译: 本发明的目的是提供一种压花皱纹纸,其可以明显地形成为细小的浮雕形状,并且蓬松感觉优异,因此对于脂肪的吸收性优异。 作为实现该目的的手段,根据本发明的压纹皱纹纸的制造方法是一种压纹皱纹纸的制造方法,其特征在于,包括对原料绉纸进行压花的工序,其中, 重量为6〜28g / m 2的原料作为起皱纸使用; 并且压花步骤包括以下步骤:(a)以原料重量为基准,以0.1至100重量%的量向原料起皱纸供应水,从而使生皱纹纸处于潮湿状态; (b)将湿绉原料绉纹纸压花; 和(c)干燥压花的湿条纹生绉纸。
-
公开(公告)号:US07967951B2
公开(公告)日:2011-06-28
申请号:US12853607
申请日:2010-08-10
申请人: Shinji Suzuki , Yukio Hayashi , Noriyasu Ike , Hiromu Matsumoto , Eri Tamura , Yasunori Endo , Jun Morisawa , Maya Sasaki , Kenji Taniguchi
发明人: Shinji Suzuki , Yukio Hayashi , Noriyasu Ike , Hiromu Matsumoto , Eri Tamura , Yasunori Endo , Jun Morisawa , Maya Sasaki , Kenji Taniguchi
CPC分类号: B31F1/07 , B31F1/122 , B31F1/36 , B31F2201/0756 , B31F2201/0761 , B31F2201/0784 , Y10T156/1023 , Y10T156/1039 , Y10T428/1303 , Y10T428/24455 , Y10T428/24463 , Y10T428/24479 , Y10T428/24612 , Y10T428/24628 , Y10T428/27
摘要: An object of the present invention is to provide an embossed crepe paper which can clearly be formed into fine embossed shapes, and is excellent in the fluffy feel and therefore excellent in such as absorbency for fats. As a means of achieving this object, the method for manufacturing an embossed crepe paper, according to the present invention, is a method for manufacturing an embossed crepe paper comprising a step of embossing a raw crepe paper, wherein: a raw paper having a basis weight of 6 to 28 g/m2 is used as the raw crepe paper; and the embossing step includes the steps of: (a) supplying the raw crepe paper with water in an amount of 0.1 to 100 weight % based on the basis weight to thereby put the raw crepe paper in a wet condition; (b) embossing the wet-conditioned raw crepe paper; and (c) drying the embossed wet-conditioned raw crepe paper.
摘要翻译: 本发明的目的是提供一种压花皱纹纸,其可以明显地形成为细小的浮雕形状,并且蓬松感觉优异,因此对于脂肪的吸收性优异。 作为实现该目的的手段,根据本发明的压纹皱纹纸的制造方法是一种压纹皱纹纸的制造方法,其特征在于,包括对原料绉纸进行压花的工序,其中, 重量为6〜28g / m2用作生绉纸; 并且压花步骤包括以下步骤:(a)以原料重量为基准,以0.1至100重量%的量向原料起皱纸供应水,从而使生皱纹纸处于潮湿状态; (b)将湿绉原料绉纹纸压花; 和(c)干燥压花的湿条纹生绉纸。
-
公开(公告)号:US20080075760A1
公开(公告)日:2008-03-27
申请号:US11679624
申请日:2007-02-27
申请人: Shinji Suzuki , Noriyasu Ike , Kiyotsugu Sawamura , Hiromu Matsumoto , Eri Tamura , Jun Morisawa , Hiroto Takiguchi , Masaaki Ariyoshi , Kenji Taniguchi , Hideaki Yoshida , Hitoshi Tsuruta , Masaaki Sasaoka , Akihiro Sasaki
发明人: Shinji Suzuki , Noriyasu Ike , Kiyotsugu Sawamura , Hiromu Matsumoto , Eri Tamura , Jun Morisawa , Hiroto Takiguchi , Masaaki Ariyoshi , Kenji Taniguchi , Hideaki Yoshida , Hitoshi Tsuruta , Masaaki Sasaoka , Akihiro Sasaki
CPC分类号: A61K8/0208 , A61K8/345 , A61Q19/00 , A61Q19/007 , D04H1/425 , D04H1/4258 , D04H1/4291 , D04H1/435 , D04H1/4382 , D04H1/492 , Y10T442/2525
摘要: The moisturized nonwoven fabric of the invention contains 1% or more of a water-soluble component to a weight of a pre-moisturized nonwoven fabric and an increase ratio of an equilibrium moisture regain (equilibrium water content) is 0.5% or more as compared with an equilibrium moisture regain of the moisturized nonwoven fabric after the water-soluble component is removed. Therefore, this moisturized nonwoven fabric is excellent in use feel such as skin touch and wiping property and functionalities such as water absorption property and water retention property. Further, this moisturized nonwoven fabric is excellent in functionalities such as moisturizing liquid transferring capability and skin moisturizing effect.
摘要翻译: 本发明的保湿无纺布含有1质量%以上的水溶性成分与预保湿无纺布的重量相比,平衡回潮率(平衡含水量)的增加比例为0.5%以上,与 除去水溶性成分后的保湿无纺布的平衡回潮。 因此,该保湿无纺布的使用感如皮肤触感和擦拭性以及吸水性和保水性等功能性优异。 此外,该保湿无纺布的功能性优异,例如保湿液输送能力和皮肤保湿效果。
-
公开(公告)号:US5273288A
公开(公告)日:1993-12-28
申请号:US760773
申请日:1991-09-17
申请人: Tooru Teshima , Hiromu Matsumoto
发明人: Tooru Teshima , Hiromu Matsumoto
CPC分类号: A63F13/33 , A63F13/12 , A63F13/214 , A63F2300/1068
摘要: A communication terminal connected to a telephone line for playing a game with an opponent through a telephone line, includes a display board for displaying the game, a touch panel provided on the display board to detect a coordinate to be displayed, a touch signal detection circuit for generating a position signal corresponding to the coordinate, and a display board drive circuit for displaying the position signal on the display board. A PB signal transmission circuit is provided for transmitting the PB signal indicating the position signal to the telephone line. A PB signal detection circuit receives a PB signal from the opponent and converts that PB signal to a respective position signal.
-
公开(公告)号:USD507533S1
公开(公告)日:2005-07-19
申请号:US29185101
申请日:2003-06-23
-
-
-
-
-