Olefin polymerisation titanium catalyst
    1.
    发明申请
    Olefin polymerisation titanium catalyst 失效
    烯烃聚合钛催化剂

    公开(公告)号:US20050113537A1

    公开(公告)日:2005-05-26

    申请号:US10502219

    申请日:2002-01-25

    摘要: An olefin polymerisation titanium catalyst. It comprises a titanium compounds and an organoaluminium compound cocatalyst supported on a soluble polysulfone comprising free reactive sulfone groups. The molar ratio of titanium to aluminium is 1-10:200 and the weight ratio of titanium to polysulfone is 0.01-0.1:0.3-2.5. The process for preparing the catalyst comprises preparing a supported titanium compound by contacting a solution of a polysulfone in a halogenated or polar solvent with a titanium compound or a solution thereof in a halogenated or polar solvent in an inert atmosphere at a temperature between 10° C. and the boiling point of the solvent such that the weight ratio of titanium to polysulfone is 0.01-0.1:0.3-2.5. The supported titanium compound is mixed with an organoaluminium cocatalyst such that the molar ratio of titanium to aluminium is 1-10:200.

    摘要翻译: 烯烃聚合钛催化剂。 它包括负载在包含游离反应性砜基团的可溶性聚砜上的钛化合物和有机铝化合物助催化剂。 钛与铝的摩尔比为1-10:200,钛与聚砜的重量比为0.01-0.1:0.3〜2.5。 制备催化剂的方法包括通过使卤化或极性溶剂中的聚砜溶液与卤化或极性溶剂中的钛化合物或其溶液在惰性气氛中在10℃ 和溶剂的沸点,使得钛与聚砜的重量比为0.01-0.1:0.3-2.5。 将负载的钛化合物与有机铝助催化剂混合,使得钛与铝的摩尔比为1-10:200。