    摘要: A data analysis device includes an input unit that receives a measured value of an optoelectronic signal from a photoelectron spectroscopic device measuring the optoelectronic signal generated from a sample by photoelectron spectroscopy and an analysis unit that analyzes the depth profile of the sample by minimizing a sum of square deviations between a theoretical value of the optoelectronic signal and the measured value of the optoelectronic signal using the theoretical value of the optoelectronic signal when the sample is modeled into a multilayer body including a plurality of layers. The analysis unit calculates a relative concentration so as to satisfy a maximum smoothness condition that the relative concentration of the chemical species of the sample smoothly changes in the plurality of layers of the multilayer body in minimizing the sum of square deviations.

    OPTICAL FIBER
    4.
    发明申请
    OPTICAL FIBER 有权
    光纤

    公开(公告)号:US20160147010A1

    公开(公告)日:2016-05-26

    申请号:US14943190

    申请日:2015-11-17

    IPC分类号: G02B6/02

    摘要: An optical fiber containing an alkali metal and capable of reducing Rayleigh scattering loss is provided. An optical fiber has a core and a cladding made of silica glass and enclosing the core. The cladding contains fluorine and has a refractive index lower than the refractive index of the core. The core contains first group dopants selected from the group of Na element, K element, or a compound thereof at an average concentration of 0.2 ppm or more and 10 ppm or less. The core also contains second group dopants for reducing the viscosity of silica glass and having a diffusion coefficient of 1×10−12 cm2/s or more and smaller than the diffusion coefficient of the first group dopants, by an average concentration of 0.2 ppm or more at a temperature of 2000° C. to 2300° C.

    摘要翻译: 提供含有碱金属并能够降低瑞利散射损失的光纤。 光纤具有由石英玻璃制成的芯和包层,并且包围芯。 包层含氟,折射率低于芯的折射率。 核心包含平均浓度为0.2ppm以上且10ppm以下的选自Na元素,K元素或其化合物的第一族掺杂剂。 该芯还含有第二组掺杂剂,用于降低石英玻璃的粘度,并且扩散系数为1×10-12cm2 / s以上且小于第一组掺杂剂的扩散系数,平均浓度为0.2ppm或 更高温度在2000°C至2300°C