摘要:
Disclosed is a method for producing a norbornene monomer composition, a norbornene polymer produced using the norbornene monomer composition, an optical film including the norbornene polymer, and a method for producing the norbornene polymer. The method includes reacting a reaction solution that contains cyclopentadiene, dicyclopentadiene, or a mixture of cyclopentadiene and dicyclopentadiene, an acetate compound, and a solvent so that a content of an exo isomer is 50 mol % or more. Variables such as a reaction temperature, a reaction time, a molar ratio between reactants, and addition of a solvent are controlled so that the exo isomer is contained in content of 50 mol % or more. Accordingly, it is possible to industrially produce an acetate norbornene addition polymer by using the acetate norbornene monomer composition containing the exo isomer in content of 50 mol % or more.
摘要:
The present invention relates to a norbornene based addition polymer, and more particularly to an addition polymer of norbornene based monomers containing an ester group. The present invention provides a norbornene-ester based addition polymer having a molecular weight (Mn) larger than 20,000 and comprising a norbornene-ester based monomer comprising more than 50 mol % of exo norbornene-ester monomer as a repeating unit, a method for preparing the same, and an optically anisotropic film comprising the same. The norbornene-ester based addition polymer of the present invention is transparent, has a low dielectric constant, has good thermal stability and strength, leaves no unwanted materials when attached to metals or other polymers, and has good adhesivity, so that it can be used for optical films, retardation films, plastic substrate materials, transparent polymers such as POF or PCB, insulating materials, or insulating electronic devices such as PCB or insulating materials.
摘要:
The present invention relates to a norbornene based addition polymer, and more particularly to an addition polymer of norbornene based monomers containing an ester group. The present invention provides a norbornene-ester based addition polymer having a molecular weight (Mn) larger than 20,000 and comprising a norbornene-ester based monomer comprising more than 50 mol % of exo norbornene-ester monomer as a repeating unit, a method for preparing the same, and an optically anisotropic film comprising the same. The norbornene-ester based addition polymer of the present invention is transparent, has a low dielectric constant, has good thermal stability and strength, leaves no unwanted materials when attached to metals or other polymers, and has good adhesivity, so that it can be used for optical films, retardation films, plastic substrate materials, transparent polymers such as POF or PCB, insulating materials, or insulating electronic devices such as PCB or insulating materials.
摘要:
The present invention provides a negative C-plate type optical anisotropic film having negative birefringence along the thickness direction. In particular, the present invention provides n film comprising cycloolefin addition polymer, which is prepared by addition polymerizing norbornene-based monomers, a method for preparing the same, and a liquid crystal display comprising the same. The film of the present invention can be used for optical compensation films of a variety of LCD (liquid crystal display) modes because the refractive index alone the thickness direction can be controlled by the kind and amount of functional groups introduced to the cycloolefin addition polymer.
摘要:
Disclosed is a method for preparing a cycloolefin polymer containing polar functional groups, comprising the steps of: a) preparing a catalyst mixture including i) a precatalyst; ii) a first cocatalyst; and iii) a second cocatalyst; and b) subjecting a monomer solution comprising a norbornene-based compound containing a polar functional group to an addition polymerization reaction in the presence of an organic solvent and the catalyst mixture, wherein the product yield of the prepared polymer is 50% by weight or more based on the total weight of the monomer.
摘要:
Disclosed is a method for preparing a cycloolefin polymer containing polar functional groups, comprising: preparing a catalyst mixture including i) a precatalyst, containing a Group 10 transition metal having a ligand containing oxygen ions bonded to the metal; ii) a first cocatalyst which is an organic compound containing a Group 15 element; and iii) a second cocatalyst which is capable of providing an anion and weakly coordinating to the metal of the precatalyst; and subjecting a monomer solution comprising a norbornene-based compound containing a polar functional group to an addition polymerization reaction in the presence of an organic solvent and the catalyst mixture, at a temperature of 80-200° C., the total amount of the organic solvent being 50-800% by weight based on the total weight of the monomer contained in the monomer solution, and the product yield of the polymer being 50% by weight or more based on the total weight of the monomer.
摘要:
Disclosed is a method for preparing a cycloolefin polymer containing polar functional groups, comprising the steps of: a) preparing a catalyst mixture including i) a precatalyst; ii) a first cocatalyst; and iii) a second cocatalyst; and b) subjecting a monomer solution comprising a norbornene-based compound containing a polar functional group to an addition polymerization reaction in the presence of an organic solvent and the catalyst mixture, wherein the product yield of the prepared polymer is 50% by weight or more based on the total weight of the monomer.
摘要:
Disclosed is a method for preparing a cycloolefin polymer containing polar functional groups, comprising: preparing a catalyst mixture including i) a precatalyst, containing a Group 10 transition metal having a ligand containing oxygen ions bonded to the metal; ii) a first cocatalyst which is an organic compound containing a Group 15 element; and iii) a second cocatalyst which is capable of providing an anion and weakly coordinating to the metal of the precatalyst; and subjecting a monomer solution comprising a norbornene-based compound containing a polar functional group to an addition polymerization reaction in the presence of an organic solvent and the catalyst mixture, at a temperature of 80-200° C., the total amount of the organic solvent being 50-800% by weight based on the total weight of the monomer contained in the monomer solution, and the product yield of the polymer being 50% by weight or more based on the total weight of the monomer.
摘要:
Disclosed is a method for preparing a cycloolefin polymer containing polar functional groups, comprising: preparing a catalyst mixture including i) a precatalyst, containing a Group 10 transition metal having a ligand containing oxygen ions bonded to the metal; ii) a first cocatalyst which is an organic compound containing a Group 15 element; and iii) a second cocatalyst which is capable of providing an anion and weakly coordinating to the metal of the precatalyst; and subjecting a monomer solution comprising a norbornene-based compound containing a polar functional group to an addition polymerization reaction in the presence of an organic solvent and the catalyst mixture, at a temperature of 80-200° C., the total amount of the organic solvent being 50-800% by weight based on the total weight of the monomer contained in the monomer solution, and the product yield of the polymer being 50% by weight or more based on the total weight of the monomer.
摘要:
Disclosed is a method for preparing a cycloolefin polymer containing polar functional groups, comprising: preparing a catalyst mixture including i) a precatalyst, containing a Group 10 transition metal having a ligand containing oxygen ions bonded to the metal; ii) a first cocatalyst which is an organic compound containing a Group 15 element; and iii) a second cocatalyst which is capable of providing an anion and weakly coordinating to the metal of the precatalyst; and subjecting a monomer solution comprising a norbornene-based compound containing a polar functional group to an addition polymerization reaction in the presence of an organic solvent and the catalyst mixture, at a temperature of 80-200° C., the total amount of the organic solvent being 50-800% by weight based on the total weight of the monomer contained in the monomer solution, and the product yield of the polymer being 50% by weight or more based on the total weight of the monomer.