Green pellet
    1.
    发明授权
    Green pellet 有权
    绿色颗粒

    公开(公告)号:US09273262B2

    公开(公告)日:2016-03-01

    申请号:US13701727

    申请日:2010-06-16

    CPC分类号: C10L5/32 C22B1/2406 C22B1/245

    摘要: Provided is a green pellet (10) which comprises: an inner core layer (11) containing an iron oxide-containing starting material, a carbonaceous material for reduction, and a slag-forming agent; and a coating layer (12) disposed so as to encapsulate the surface of the inner core layer (11), wherein the coating layer (12) is formed from a protective layer (12a), which is disposed so as to encapsulate the surface of the inner core layer (11) and which contains an inorganic compound (includes an alkali metal oxide) having a melting point that is 750°C. or greater but less than 1100°C., and a combustion layer (12b ), which is disposed so as to encapsulate the surface of the protective layer (12a) and which contains the carbonaceous material.

    摘要翻译: 本发明提供一种绿色颗粒(10),其包括:含有含氧化铁原料的内芯层(11),还原用碳质材料和成渣剂; 以及设置成封装所述内芯层(11)的表面的涂层(12),其中所述涂层(12)由保护层(12a)形成,所述保护层(12a)被设置为将所述内芯层 内芯层(11),其含有熔点为750℃的无机化合物(包括碱金属氧化物)。 或更大但小于1100℃,以及燃烧层(12b),其被设置为封装保护层(12a)的表面并且含有碳质材料。

    GREEN PELLET
    2.
    发明申请
    GREEN PELLET 有权
    绿色小丸

    公开(公告)号:US20130111809A1

    公开(公告)日:2013-05-09

    申请号:US13701727

    申请日:2010-06-16

    IPC分类号: C10L5/32

    CPC分类号: C10L5/32 C22B1/2406 C22B1/245

    摘要: Provided is a green pellet (10) which comprises: an inner core layer (11) containing an iron oxide-containing starting material, a carbonaceous material for reduction, and a slag-forming agent; and a coating layer (12) disposed so as to encapsulate the surface of the inner core layer (11), wherein the coating layer (12) is formed from a protective layer (12a), which is disposed so as to encapsulate the surface of the inner core layer (11) and which contains an inorganic compound (includes an alkali metal oxide) having a melting point that is 750° C. or greater but less than 1100° C., and a combustion layer (12b), which is disposed so as to encapsulate the surface of the protective layer (12a) and which contains the carbonaceous material.

    摘要翻译: 本发明提供一种绿色颗粒(10),其包括:含有含氧化铁原料的内芯层(11),还原用碳质材料和成渣剂; 以及设置成封装所述内芯层(11)的表面的涂层(12),其中所述涂层(12)由保护层(12a)形成,所述保护层(12a)被设置为将所述内芯层 内芯层(11),其含有熔点为750℃以上且小于1100℃的无机化合物(包括碱金属氧化物)和燃烧层(12b),其中, 被设置为封装保护层(12a)的表面并且包含碳质材料。

    Impeller manufacturing method
    3.
    发明授权
    Impeller manufacturing method 有权
    叶轮制造方法

    公开(公告)号:US08590150B2

    公开(公告)日:2013-11-26

    申请号:US13805021

    申请日:2011-10-25

    IPC分类号: B21D51/16

    摘要: The present invention relates to a method of joining a hub 11 and a shroud 12 of an impeller 10, either one of which has blades 13 integrally formed thereon, by welding. During the welding, in an upright state in which the hub 11 is placed to face a mount surface, the hub 11 and the shroud 12 are placed on top of each other to form an assembled body 10. Welding is performed on the assembled body 10 covered with a heat insulating jacket 30(a to g), the jacket 30 covering the assembled body 10 except an open region (OP) and an inflow port 14IN required for welding. When welding of one open region OP is completed, a new open region OP is formed by moving the heat insulating jacket 30 with respect to the assembled body, and then the next welding is performed.

    摘要翻译: 本发明涉及一种将叶轮10的轮毂11和护罩12连接起来的方法,叶轮10中的任一个具有通过焊接一体形成的叶片13。 在焊接期间,在轮毂11被放置成面向安装表面的直立状态下,轮毂11和护罩12被放置在彼此的顶部以形成组装体10.在组装体10上进行焊接 覆盖有隔热护套30(a至g),除了开放区域(OP)和焊接所需的流入端口14IN之外,护套30覆盖组装体10。 当一个开放区域OP的焊接完成时,通过相对于组装体移动隔热套30而形成新的开放区域OP,然后进行下一次焊接。

    IMPELLER MANUFACTURING METHOD
    4.
    发明申请
    IMPELLER MANUFACTURING METHOD 有权
    叶轮制造方法

    公开(公告)号:US20130140349A1

    公开(公告)日:2013-06-06

    申请号:US13805021

    申请日:2011-10-25

    IPC分类号: B23K31/02

    摘要: The present invention relates to a method of joining a hub 11 and a shroud 12 of an impeller 10, either one of which has blades 13 integrally formed thereon, by welding. During the welding, in an upright state in which the hub 11 is placed to face a mount surface, the hub 11 and the shroud 12 are placed on top of each other to form an assembled body 10. Welding is performed on the assembled body 10 covered with a heat insulating jacket 30(a to g), the jacket 30 covering the assembled body 10 except an open region (OP) and an inflow port 14IN required for welding. When welding of one open region OP is completed, a new open region OP is formed by moving the heat insulating jacket 30 with respect to the assembled body, and then the next welding is performed.

    摘要翻译: 本发明涉及一种将叶轮10的轮毂11和护罩12连接起来的方法,叶轮10中的任一个具有通过焊接一体形成的叶片13。 在焊接期间,在轮毂11被放置成面向安装表面的直立状态下,轮毂11和护罩12被放置在彼此的顶部以形成组装体10.在组装体10上进行焊接 覆盖有隔热护套30(a至g),除了开放区域(OP)和焊接所需的流入端口14IN之外,护套30覆盖组装体10。 当一个开放区域OP的焊接完成时,通过相对于组装体移动隔热套30而形成新的开放区域OP,然后进行下一次焊接。