摘要: A urethane prepolymer composition useful as sealant is disclosed. The composition comprises a reaction product of an organic polyisocyanate and a polyether polyol mixture at an NCO/OH equivalent ratio from 1.6 to 2.5. The polyether polyol mixture contains (a) from 75 to 95 % by weight of the mixture of a polyoxyalkylenediol having an average MW from 400 to 1,000 and an oxyethlene unit content greater than 50 % by weight, and (b) the balance of the mixture of a polyoxyalkylenetriol having an average MW from 5,000 to 10,000 and an oxyethylene unit content greater than 50 % by weight. An equivalent composition is produced by reacting the polyoxyalkylenediol and polyoxyalkylenetriol with the organic polyisocyanate separately and mixing together after the reaction.
摘要翻译: 公开了可用作密封剂的氨基甲酸酯预聚物组合物。 组合物包含有机多异氰酸酯与聚醚多元醇混合物的反应产物,其NCO / OH当量比为1.6至2.5。 聚醚多元醇混合物含有(a)75至95重量%的平均MW为400至1,000,氧乙烯单元含量大于50重量%的聚氧化烯二醇的混合物,和(b)混合物的余量 的平均MW为5,000至10,000并且氧化乙烯单元含量大于50重量%的聚氧亚烷基三醇。 通过使聚氧亚烷基二醇和聚氧亚烷基三醇与有机多异氰酸酯分别反应并在反应之后混合在一起制备等效的组合物。
-
公开(公告)号:US4582891A
公开(公告)日:1986-04-15
申请号:US699058
申请日:1985-02-06
IPC分类号: C09D5/08 , C08G18/08 , C08G18/36 , C09D175/00 , C09D175/04
CPC分类号: C08G18/36 , C08G18/0885 , C08G2150/90 , Y10S528/905
摘要: An anti-corrosive polyurethane coating composition which has excellent metal corrosion inhibiting property, water resistance, adhesion property to metals, impact resistance and other properties required for anti-corrosive paints, and can be coated thick with one coating operation, containing as an essential component a polyurethane resin having a density of crosslinking of 1.10 to 2.00 per 1,000 atomic weight of the resin and produced by reaction of (A) a polyol component having a hydroxyl value of 160 to 350 mgKOH/g and being composed of a castor oil polyol alone or a mixture of a castor oil polyol and a low molecular polyol having a functionality of at least 2, preferably at least 3, and (B) a polyisocyanate component in an NCO/active hydrogen ratio of 0.85-1.151 by equivalent.
摘要翻译: 具有优异的金属腐蚀抑制性,耐水性,对金属的粘附性,抗冲击性等抗腐蚀性涂料所需的耐腐蚀性的聚氨酯涂料组合物,可以用一次涂布操作进行涂布,作为必要成分 通过(A)羟基值为160〜350mgKOH / g的多元醇成分与单独的蓖麻油多元醇单体的反应而生成的交联密度为1.10〜2.00的聚氨酯树脂, 或蓖麻油多元醇和官能度至少为2,优选至少3的低分子多元醇的混合物,和(B)NCO /活性氢比为0.85-1.151的多异氰酸酯组分相当于。
-