公开(公告)号:US09988698B2
公开(公告)日:2018-06-05
申请号:US14566769
申请日:2014-12-11
发明人: Glenn Glennon , Eric Bono
IPC分类号: C22C19/03 , B32B15/04 , B32B37/10 , B32B37/06 , B32B15/01 , B05D7/24 , B05D3/02 , B05D7/14 , B23K20/02 , C23C28/02 , C23C26/00 , C23C30/00 , C22C19/00 , C23C24/08
CPC分类号: C22C19/03 , B23K20/023 , B32B15/01 , C22C19/00 , C22C19/007 , C23C24/087 , C23C26/00 , C23C28/02 , C23C28/021 , C23C30/00 , C23C30/005 , Y10T428/12451 , Y10T428/12472 , Y10T428/12806 , Y10T428/12944 , Y10T428/12993
摘要: Disclosed herein is a method comprising disposing on a base article a nickel-titanium alloy; where the nickel is in an amount of about 58 to about 62 weight percent and titanium in an amount of about 38 to about 42 wt %, based on the total weight of the nickel-titanium alloy; and applying a pressure of 12 to 20 kilopounds per square inch at a temperature of 1400 to 2100° F. for a period of 1 to 8 hours to form a nickel-titanium alloy coating on the base article. Disclosed is an article comprising a base article; and a nickel-titanium alloy; where the nickel-titanium alloy is disposed on the base article; where the nickel is in an amount of about 58 to about 62 weight percent and titanium in an amount of about 38 to about 42 wt %, based on the total weight of the nickel-titanium alloy.