METHOD FOR PRODUCTION OF BEAD POLYMERS WITH AN AVERAGE PARTICLE SIZE IN THE RANGE OF 1 MICROMETER TO 40 MICROMETERS AND MOULDED MASSES AND MOULDED BODIES COMPRISING BEAD POLYMERS
    2.
    发明申请
    METHOD FOR PRODUCTION OF BEAD POLYMERS WITH AN AVERAGE PARTICLE SIZE IN THE RANGE OF 1 MICROMETER TO 40 MICROMETERS AND MOULDED MASSES AND MOULDED BODIES COMPRISING BEAD POLYMERS 审中-公开
    用于生产具有平均颗粒大小的珠粒聚合物的方法在1微米至40微米和模塑质量和包含珠粒聚合物的成型体的范围内

    公开(公告)号:US20090043044A2

    公开(公告)日:2009-02-12

    申请号:US11913325

    申请日:2007-11-01

    IPC分类号: C08K3/10

    摘要: Process for preparation of bead polymers whose average particle size is in the range from 1 μm to 40 μm, by dispersing and polymerizing a polymerizable composition in an aqueous phase, where the dispersion stabilized by an aluminium compound is prepared at a shear rate ≧103 s−1. A polymerizable composition is used here which, in each case based on its total weight, comprises a) more than 50.0% by weight of at least one compound of the formula (I),  where the radicals 1R to 6R have definitions according to the Description, b) from 0.1% by weight to 10.0% by weight of at least one crosslinking agent and c) less than 49.9% by weight of at least one compound of the formula (II)  where the radicals R and 7R to 9R have definitions according to the Description The bead polymers prepared according to the inventive process are particularly suitable for production of mouldings with light-scattering properties.

    摘要翻译: 通过将可聚合组合物分散和聚合在水相中制备其平均粒度在1〜40μm范围内的珠粒聚合物的方法,其中通过铝化合物稳定的分散体以剪切速率> = 103 s-1。 在这里使用可聚合组合物,其在每种情况下基于其总重量包含a)超过50.0重量%的至少一种式(I)化合物,其中基团1R至6R具有根据说明书的定义 ,b)0.1重量%至10.0重量%的至少一种交联剂和c)小于49.9重量%的至少一种式(II)化合物,其中基团R和7R至9R具有如下定义: 根据本发明方法制备的珠粒聚合物特别适用于生产具有光散射性质的模制品。