摘要:
The invention relates to a moulding composition, comprising a) 50 to 99.9% by weight of a matrix composed of a thermoplastic polymer and b) from 0.1 to 50% by weight of a matting agent in the form of a (meth)acrylate copolymer dispersed in the matrix, characterized in that the matting agent is a (meth)acrylate copolymer which has been prepared from the following monomers, b1) from 50 to 95% by weight of methyl methacrylate b2) from 5 to 50% by weight of C1-C6-alkyl acrylates b3) from 0.01 to less than 0.5% by weight of a crosslinking monomer and/or graft-linking agent having two or more ethylenically unsaturated radicals capable of free-radical polymerization, b4) from 0 to 20% by weight of one or more other, non-crosslinking ethylenically unsaturated monomers capable of free-radical polymerization, where the entirety of the constituents b1) and b2) and, where appropriate, b3) and/or b4) gives 100% by weight, and the glass transition temperature Tmg of the matting agent is at least 20° C.
摘要:
The invention relates to a moulding composition, comprising a) 50 to 99.9% by weight of a matrix composed of a thermoplastic polymer and b) from 0.1 to 50% by weight of a matting agent in the form of a (meth)acrylate copolymer dispersed in the matrix, characterized in that the matting agent is a (meth)acrylate copolymer which has been prepared from the following monomers, b1) from 50 to 95% by weight of methyl methacrylate b2) from 5 to 50% by weight of C1-C6-alkyl acrylates b3) from 0.01 to less than 0.5% by weight of a crosslinking monomer and/or graft-linking agent having two or more ethylenically unsaturated radicals capable of free-radical polymerization, b4) from 0 to 20% by weight of one or more other, non-crosslinking ethylenically unsaturated monomers capable of free-radical polymerization, where the entirety of the constituents b1) and b2) and, where appropriate, b3) and/or b4) gives 100% by weight, and the glass transition temperature Tmg of the matting agent is at least 20° C.
摘要:
The present invention relates to a core-shell particle which has a core, a first shell and, where appropriate, a second shell, where: i) the core encompasses, based on its total weight, at least 75.0% by weight of (meth)acrylate repeat units; ii) the first shell has a glass transition temperature below 30° C.; iii) the second shell present where appropriate encompassed, based on its total weight, at lest 75.0% by weight of (meth)acrylate repeat units; iv) the first shell encompasses, based on its total weight, the following constituents; E) from 92.0 to 98.0% by weight of (meth)acrylate repeat units and F) from 2.0 to 8.0% by weight of styrenic repeat units of the general formula (I) where the radicals R1 to R6 are defined according to the Description and the percentages by weight of E) and F) give a total of 100.0% by weight, v) the radius of the core-shell particle inclusive of any second shell present, measured by the Coulter method, is in the range from above 160.0 to 240.0 nm. The present invention further relates to a process for preparing core-shell particles, to a moulding composition comprising core-shell particles, and to the use thereof.
摘要:
The present invention relates to a core-shell particle which has a core, a first shell and, where appropriate, a second shell, where: i) the core encompasses, based on its total weight, at least 75.0% by weight of (meth)acrylate repeat units; ii) the first shell has a glass transition temperature below 30° C.; iii) the second shell present where appropriate encompassed, based on its total weight, at lest 75.0% by weight of (meth)acrylate repeat units; iv) the first shell encompasses, based on its total weight, the following constituents; E) from 92.0 to 98.0% by weight of (meth)acrylate repeat units and F) from 2.0 to 8.0% by weight of styrenic repeat units of the general formula (I) where the radicals R1 to R6 are defined according to the Description and the percentages by weight of E) and F) give a total of 100.0% by weight, v) the radius of the core-shell particle inclusive of any second shell present, measured by the Coulter method, is in the range from above 160.0 to 240.0 nm; a process for preparing core-shell particles, to a moulding composition comprising core-shell particles, and to the use thereof.
摘要:
The printed sheets are scanned, by image elements, immediately behind the last printing mechanism, with one or several measuring heads. Suitable dimensions of an image element range from approximately 1.times.1 mm.sup.2 to 10.times.10 mm.sup.2. In each image element the reflectance is measured in four spectral ranges (infrared for black, red for cyan, green for magenta and blue for yellow). The measured reflectance values are converted by means of Neugebauer equations into surface coverages in a demasking step and inputted to a computer for evaluation. With the same measuring device, both the reference values associated with OK sheets, and the actual values associated with continuous printing, are measured. The computer compares the measured data, weights them with respect to such factors as surface coverage, foreign color component and the environment of a respective image element, and produces a regulating signal to control the ink feed elements. The color coordinates (X,Y,Z) may be determined from the surface coverage values of the four colors in a parallel computer program. Image elements which are important for the visual appearance of an image are given a high weight. A quality measure may be determined from the weighted comparison of reference and actual values to change the visual appearance. With this process it is possible to control the ink feed elements of a multicolor printing press by direct on-line measurement of the printed image, without using color measuring strips.