公开(公告)号:US12090549B2
公开(公告)日:2024-09-17
申请号:US17794300
申请日:2020-12-15
Applicant: Toho Titanium Co., Ltd.
Inventor: Yosuke Inoue , Syogo Tsumagari , Yasuhiko Goto
CPC classification number: B22F1/16 , B22F1/142 , B22F1/145 , B22F3/1007 , B22F3/11 , B22F5/006 , C22C14/00 , B22F2201/03 , B22F2201/10 , B22F2201/20 , B22F2301/205 , B22F2302/25 , B22F2304/10 , B22F2999/00 , B22F1/145 , B22F2201/03 , B22F1/16
Abstract: A method for manufacturing a porous metal body according to the present invention includes: a surface oxidizing step of heating a titanium-containing powder in an atmosphere containing oxygen at a temperature of 250° C. or more for 30 minutes or more to provide a surface-oxidized powder; and a sintering step of depositing the surface-oxidized powder in a dry process, and sintering the surface-oxidized powder by heating it in a reduced pressure atmosphere or an inert atmosphere at a temperature of 950° C. or more.
-
公开(公告)号:US20230084462A1
公开(公告)日:2023-03-16
申请号:US17794300
申请日:2020-12-15
Applicant: Toho Titanium Co., Ltd.
Inventor: Yosuke Inoue , Syogo Tsumagari , Yasuhiko Goto
Abstract: A method for manufacturing a porous metal body according to the present invention includes: a surface oxidizing step of heating a titanium-containing powder in an atmosphere containing oxygen at a temperature of 250° C. or more for 30 minutes or more to provide a surface-oxidized powder; and a sintering step of depositing the surface-oxidized powder in a dry process, and sintering the surface-oxidized powder by heating it in a reduced pressure atmosphere or an inert atmosphere at a temperature of 950° C. or more.
-
公开(公告)号:US11502305B2
公开(公告)日:2022-11-15
申请号:US16960230
申请日:2018-03-19
Applicant: TOHO TITANIUM CO., LTD.
Inventor: Masashi Hayakawa , Syogo Tsumagari
Abstract: To provide a titanium-based porous body that has high void fraction to ensure gas permeability and water permeability for practical use as an electrode and a filter, has a large specific surface area to ensure conductivity and sufficient reaction sites with a reaction solution or a reaction gas, thus showing excellent reaction efficiency, and contains less contaminants because of no organic substance used. A titanium-based porous body having a specific void fraction and a high specific surface area is obtained by filling an irregular-shaped titanium powder having an average particle size of 10 to 50 μm in a dry system without using any binder or the like into a thickness of 4.0×10−1 to 1.6 mm, and sintering the irregular-shaped titanium powder at 800 to 1100° C.
-
-