Polyketone fiber and process for producing the same
    1.
    发明申请
    Polyketone fiber and process for producing the same 有权
    聚酮纤维及其制造方法

    公开(公告)号:US20060128933A1

    公开(公告)日:2006-06-15

    申请号:US10525452

    申请日:2003-08-27

    IPC分类号: C08G16/00

    CPC分类号: D01F6/30 B60C9/0042

    摘要: Polyketone fibers comprising, on the basis of the entire repeating units, 95% by mole of a repeating unit of the formula (1) shown below, and showing a minimum value (Amin(F)) of a UV absorbance of 0.5 or less in a wavelength region of 210 to 240 nm. —CH2CH2—CO—  (1)

    摘要翻译: 基于整个重复单元,包含以下所示的式(1)的重复单元为95摩尔%,表示最小值(A min min(F))的聚酮纤维 在210〜240nm的波长范围内的紫外吸光度为0.5以下。 <?in-line-formula description =“In-line Formulas”end =“lead”?> CH 2 2 CH 2 2 -CO-(1)<βin -line-formula description =“内联公式”end =“tail”?>

    Polyketone fiber and process for producing the same
    3.
    发明授权
    Polyketone fiber and process for producing the same 有权
    聚酮纤维及其制造方法

    公开(公告)号:US06818728B2

    公开(公告)日:2004-11-16

    申请号:US10082219

    申请日:2002-02-26

    IPC分类号: C08G216

    摘要: Disclosed are polyketone fibers which contain a ketone unit represented by —CH2CH2—CO— as a main repeating unit, and have an intrinsic viscosity of not less than 0.5 dl/g, a crystal orientation of not less than 90%, a density of not less than 1.300 g/cm3, an elastic modulus of not less than 200 cN/dtex, and a heat shrinkage of −1 to 3%. The polyketone fibers are high in strength and elastic modulus, and excellent in fatigue resistance, processability, heat resistance, dimensional stability, and, besides, adhesion, and, therefore, can be applied to the fields which require high fatigue resistance, such as tire cords, belts, hoses, ropes, etc.

    摘要翻译: 公开了含有由-CH 2 CH 2 -CO-表示的酮单元作为主要重复单元的聚酮纤维,其特性粘度不小于0.5dl / g,晶体取向不小于90%,密度不为 小于1.300g / cm 3,弹性模量不小于200cN / dtex,热收缩率为-1〜3%。 聚酮纤维的强度和弹性模量高,耐疲劳性,加工性,耐热性,尺寸稳定性优异,另外,粘合性也可以适用于需要高耐疲劳性的领域,如轮胎 绳,皮带,软管,绳索等

    Polyketone solution
    4.
    发明授权
    Polyketone solution 有权
    聚酮溶液

    公开(公告)号:US07223829B2

    公开(公告)日:2007-05-29

    申请号:US11300299

    申请日:2005-12-15

    IPC分类号: C08G2/06 C08G2/16

    摘要: A solution of a polyketone as a copolymer of carbon monoxide and one or more olefins, wherein 90 wt % or more of said copolymer comprises carbon monoxide units and olefin units, and a solvent is an aqueous solution of at least one member selected from the group consisting of zinc salts, calcium salts, thiocyanates and iron salts.

    摘要翻译: 作为一氧化碳和一种或多种烯烃的共聚物的聚酮溶液,其中所述共聚物的90重量%或更多含有一氧化碳单元和烯烃单元,并且溶剂是选自以下的至少一种的水溶液: 由锌盐,钙盐,硫氰酸盐和铁盐组成。

    Polyketone fiber and process for producing the same
    5.
    发明授权
    Polyketone fiber and process for producing the same 有权
    聚酮纤维及其制造方法

    公开(公告)号:US06881478B2

    公开(公告)日:2005-04-19

    申请号:US10929428

    申请日:2004-08-31

    IPC分类号: D01F6/30 D01F6/00

    摘要: Disclosed are polyketone fibers which contain a ketone unit represented by —CH2CH2—CO— as a main repeating unit, and have an intrinsic viscosity of not less than 0.5 dl/g, a crystal orientation of not less than 90%, a density of not less than 1.300 g/cm3, an elastic modulus of not less than 200 cN/dtex, and a heat shrinkage of −1 to 3%. The polyketone fibers are high in strength and elastic modulus, and excellent in fatigue resistance, processability, heat resistance, dimensional stability, and, besides, adhesion, and, therefore, can be applied to the fields which require high fatigue resistance, such as tire cords, belts, hoses, ropes, etc.

    摘要翻译: 公开了含有以-CH 2 CH 2 CO 2 - 作为主要重复单元表示的酮单元的聚酮纤维,其特性粘度不小于0.5dl / g,晶体取向不小于90%,密度不小于1.300g / cm 3,弹性模量不小于200cN / dtex,热收缩率为 - 1〜3%。 聚酮纤维的强度和弹性模量高,耐疲劳性,加工性,耐热性,尺寸稳定性优异,另外,粘合性也可以适用于需要高耐疲劳性的领域,如轮胎 绳,皮带,软管,绳索等

    Polyketone fiber and process for producing the same
    7.
    发明申请
    Polyketone fiber and process for producing the same 有权
    聚酮纤维及其制造方法

    公开(公告)号:US20050031864A1

    公开(公告)日:2005-02-10

    申请号:US10929428

    申请日:2004-08-31

    IPC分类号: D01F6/30 D02G3/00

    摘要: Disclosed are polyketone fibers which contain a ketone unit represented by —CH2CH2—CO— as a main repeating unit, and have an intrinsic viscosity of not less than 0.5 dl/g, a crystal orientation of not less than 90%, a density of not less than 1.300 g/cm3, an elastic modulus of not less than 200 cN/dtex, and a heat shrinkage of −1 to 3%. The polyketone fibers are high in strength and elastic modulus, and excellent in fatigue resistance, processability, heat resistance, dimensional stability, and, besides, adhesion, and, therefore, can be applied to the fields which require high fatigue resistance, such as tire cords, belts, hoses, ropes, etc.

    摘要翻译: 公开了含有由-CH 2 CH 2 -CO-表示的酮单元作为主要重复单元的聚酮纤维,其特性粘度不小于0.5dl / g,晶体取向不小于90%,密度不为 小于1.300g / cm 3,弹性模量不小于200cN / dtex,热收缩率为-1〜3%。 聚酮纤维的强度和弹性模量高,耐疲劳性,加工性,耐热性,尺寸稳定性优异,另外,粘合性也可以适用于需要高耐疲劳性的领域,如轮胎 绳,皮带,软管,绳索等

    Polyketone solution
    8.
    发明授权
    Polyketone solution 有权
    聚酮溶液

    公开(公告)号:US07015303B1

    公开(公告)日:2006-03-21

    申请号:US09744884

    申请日:1999-08-05

    IPC分类号: C08G2/16 C08G18/08 C08K5/17

    摘要: A solution of a polyketone as a copolymer of carbon monoxide and one or more olefins, wherein 90 wt % or more of said copolymer comprises carbon monoxide units and olefin units, and a solvent is an aqueous solution of at least one member selected from the group consisting of zinc salts, calcium salts, thiocyanates and iron salts.

    摘要翻译: 作为一氧化碳和一种或多种烯烃的共聚物的聚酮溶液,其中所述共聚物的90重量%或更多含有一氧化碳单元和烯烃单元,并且溶剂是选自以下的至少一种的水溶液: 由锌盐,钙盐,硫氰酸盐和铁盐组成。